journal article·2026-07

Exceptional long-duration ablation resistance at 2200 °C of damage-tolerant C/SiC-Cu3Si-Cu interpenetrating composites

Bin Liang, Yue Wu, Shengyang Pang, Rida Zhao, Chenglong Hu, Jian Li, Meng Yan, Sufang Tang, Bohui Sun

Corrosion Science· Volume 267
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Microstructure and ablation behavior of C/C-SiC-ZrC-Cu composites prepared by reactive melt infiltration
2. Structure evolution and ablative mechanism of C/C-ZrC-ZrxCuy composites with low porosity fabricated by pressure assisted reactive melt infiltration10.1016/j.corsci.2022.110801 ↗
3. Fabrication of 3D-SiC/aluminum alloy interpenetrating composites by DIW and pressureless infiltration10.1016/j.ceramint.2021.05.147 ↗
4. Microstructure and ablation behaviour of a Cf/SiC-Al composite prepared by infiltrating Al alloy into Cf/SiC10.1016/j.jallcom.2021.162430 ↗
5. Construction of C/SiC-Cu3Si-Cu interpenetrating composites for long-duration thermal protection at 2500 °C by cooperative active-passive cooling10.1016/j.compositesb.2023.111015 ↗
6. Low-temperature preparation of C/C-W-Cu composites with enhanced particle impact and ablation resistance10.1016/j.jallcom.2024.177605 ↗
7. Preparation of 3D C/SiC-Cu composites via precursor pyrolysis and property investigation10.4028/www.scientific.net/KEM.368-372.1031 ↗
8. Microstructure, mechanical and ablation properties of transpiration cooling applied to C/C-SiC composite for novel anti-ablation material10.1007/s10443-022-10058-9 ↗
9. Microstructure and ablation behaviour of a carbon/carbon-ZrC-Cu composite prepared by adding Ti to Zr/Cu powder mixture10.1016/j.corsci.2019.108175 ↗
10. Microstructural development of a C/C-ZrC-Cu composite prepared by reactive melt infiltration with Zr/Cu powder mixture10.1016/j.matchar.2018.01.034 ↗
11. Effect of Cu on the ablation properties of Cf/ZrC composites fabricated by infiltrating Cf/C preforms with Zr-Cu alloys10.1016/j.ceramint.2015.01.036 ↗
12. Tuning ceramic content, mechanical and ablative properties of C/C-ZrC-ZrxCuy composites via using various C/C skeletons10.1016/j.ceramint.2022.12.069 ↗
13. Ablative property and mechanism of SiC-CuxSiy modified C/C-ZrC composites prepared by a rapid method10.1016/j.jeurceramsoc.2023.04.011 ↗
14. Fabrication of C/SiC composites by siliconizing carbon fiber reinforced nanoporous carbon matrix preforms and their properties10.1016/j.jeurceramsoc.2022.10.028 ↗
15. Fracture mechanical and ablation behaviors of C/SiC-Cu3Si-Cu interpenetrating composites and their dependence on metal addition and interface thickness10.1016/j.compositesb.2024.111632 ↗
16. Reactive melt infiltration fabrication of C/C-SiC composite: Wetting and infiltration10.1016/j.ceramint.2016.08.007 ↗
17. Fundamental mechanisms with reactive infiltration of silicon melt into carbon capillaries
18. Damage mechanism analysis to the carbon fiber and fiber-ceramic interface tailoring of Cf/ZrC-SiC using PyC coating10.1016/j.ceramint.2018.07.065 ↗
19. An application of Raman spectroscopy on the measurement of residual stress in porous silicon10.1016/j.optlaseng.2004.09.005 ↗
20. Measurement of residual stress in silicon carbide fibers of tubular composites using Raman spectroscopy10.1016/j.actamat.2021.117164 ↗
21. Measurement of interfacial residual stress in SiC fiber reinforced Ni-Cr-Al alloy composites by Raman spectroscopy10.1016/j.jmst.2018.09.023 ↗
22. Thermophysical properties of carbon/carbon composites and physical mechanism of thermal expansion and thermal conductivity10.1016/j.carbon.2004.06.024 ↗
23. Comparative ablation behaviors of C/SiC-ZrC and C/SiC-HfC composites prepared by ceramization of carbon aerogel preforms10.1016/j.corsci.2023.111623 ↗
24. Efficient fabrication of light Cf/SiHfBOC composites with excellent thermal shock resistance and ultra-high-temperature ablation up to 1800 °C10.26599/JAC.2023.9220808 ↗
25. Universal scaling of the stress-strain curve in amorphous solids10.1103/PhysRevE.96.033002 ↗
26. High damage-tolerance bio-inspired ZL205A/SiC composites with a lamellar-interpenetrated structure10.1016/j.msea.2017.09.114 ↗
27. Mechanical properties and damage tolerance of bulk Yb3Al5O12 ceramic10.1016/j.jmst.2015.01.002 ↗
28. Measurement of residual stress in silicon carbide fibers of tubular composites using Raman spectroscopy10.1016/j.actamat.2021.117164 ↗
29. Rare earth monosilicates as oxidation resistant interphase for SiCf/SiC CMC: Investigation of SiCf/Yb2SiO5 model composites10.1007/s40145-021-0560-4 ↗
30. Measurement of interfacial residual stress in SiC fiber reinforced Ni-Cr-Al alloy composites by Raman spectroscopy10.1016/j.jmst.2018.09.023 ↗
31. Pre-oxidation temperature optimization of ultra-high temperature ceramic components: Flexural strength testing and residual stress analysis10.1016/j.ceramint.2014.12.079 ↗
32. Effects of residual stress on the flexural strength and microstructure of Al2O3-ZrO2 composites fabricated by different methods10.1186/s40712-025-00216-9 ↗
33. Optimization of interfacial bonding to enhance fracture toughness of ceramic matrix reinforced with metallic ribbon10.1007/BF01184592 ↗
34. Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800 °C10.1016/j.corsci.2016.03.026 ↗
35. High temperature solar thermochemical process for production of stored energy and oxygen based on CuO/Cu2O redox reactions10.1016/j.solener.2017.05.025 ↗
36. Oxidation Mechanism of Cu2O to CuO at 600-1050 °C10.1007/s11085-004-7808-6 ↗
37. High-temperature thermochemical heat storage via the CuO/Cu2O redox cycle: From material synthesis to packed-bed reactor engineering and cyclic operation10.1021/acs.energyfuels.0c02572 ↗
38. Preparation and properties of 2D C/ZrB2-SiC ultra high temperature ceramic composites10.1016/j.msea.2009.07.005 ↗
39. Ablation behavior of nose-shaped HfB2-SiC modified carbon/carbon composites exposed to oxyacetylene torch10.1016/j.corsci.2019.02.015 ↗
40. Zirconium phosphate ceramic composites: High-temperature resistant materials for thermal protection and insulation up to 2500 °C10.1016/j.exm.2025.09.001 ↗