journal article·2026-06

Enhancing the corrosion resistance of SAC305 via alternating-voltage-driven oxide film dissolution and regrowth

Yixing Lu, Yujie Fang, Guo Yu, Jinming Zhang, Xinzhe Yuan, Zhishang Huang, Yifei Zhang, Weiwei Wu, Yiming Jiang, Jin Li, Yangting Sun

Corrosion Science· Volume 265
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Anodic Oxide Films and Nanostructures

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. The polarization characteristics of Pb-free Sn–8.5Zn–XAg–0.1Al–0.05Ga alloy in 3.5% NaCl solution10.1016/j.corsci.2007.02.005 ↗
2. Corrosion behavior of Sn-3.0Ag-0.5Cu lead-free solder joints10.1016/j.microrel.2017.04.017 ↗
3. Corrosion characterization of Sn-Zn solder: a review10.1108/SSMT-05-2018-0013 ↗
4. Electrochemical composite deposition of Sn–Ag–Cu alloys10.1016/j.mseb.2009.09.012 ↗
5. Corrosion behavior of Sn–3.0Ag–0.5Cu solder under high-temperature and high-humidity condition10.1007/s10854-014-1714-8 ↗
6. Electrochemical corrosion of SAC alloys: a review10.3390/met10101276 ↗
7. Surface failure analysis of a field-exposed copper-clad plate in a marine environment with industrial pollution10.1016/j.apsusc.2016.12.118 ↗
8. Surface failure mechanism of PCB-ENIG in typical outdoor atmospheric environments10.1016/j.materresbull.2017.03.017 ↗
9. R. Ambat, A Review of Corrosion and Environmental Effects on Electronics, (n.d.).
10. The impact of temperature and humidity conditions on surface insulation resistance values for various fluxes10.1108/09540919910254921 ↗
11. Formation of Ag dendrites: selective oxidation of Ag3Sn and its electrochemical migration in halogen-containing media10.1016/j.corsci.2025.113087 ↗
12. Screening corrosion-resistant genetic elements of Sn-0.7Cu solders by high-throughput calculations10.1016/j.corsci.2025.112726 ↗
13. Effect of Bi doping on the mechanical properties, solder joint microstructure, and corrosion resistance of SAC305-0.1Ni-2.0Sb solder alloys10.1016/j.matchar.2025.115442 ↗
14. Role of bismuth in the mechanical and corrosion properties of Cu/Sn-3.0Ag-0.5Cu/Cu solder lap joints10.1007/s10854-024-11942-9 ↗
15. Effect of Nd addition on the corrosion behavior of SAC305 solder alloy10.1016/j.corsci.2023.111264 ↗
16. Electrochemical behaviour of lead-free Sn-0.7Cu-xIn solders alloys in 3.5 wt% NaCl solution10.1007/s10854-021-06824-3 ↗
17. Influence of Ni, Bi, and Sb additives on the microstructure and the corrosion behavior of Sn-Ag-Cu solder alloys10.1007/s10854-020-04095-y ↗
18. Influence of cobalt content on microstructure and corrosion performance of extruded Sn-9Zn solder alloys10.1007/s11771-020-4325-y ↗
19. Corrosion problems of SAC-SiC composite solder alloys10.1016/j.corsci.2023.111488 ↗
20. Effect of Cr addition on microstructure, mechanical properties and corrosion properties of Sn-58Bi-0.075GNSs solder alloy
21. Effect of doping Si3N4 nanoparticles on the properties and microstructure of Sn1.0Ag0.5Cu solder
22. Corrosion characterizations of Sn-9Zn-xS in acidic and alkaline solutions10.1007/s10854-024-12109-2 ↗
23. Effects of phosphorus addition on the properties of Sn-9Zn lead-free solder alloy10.1007/s12613-013-0766-8 ↗
24. Effect of Ni-coated carbon nanotubes on the corrosion behavior of Sn-Ag-Cu solder10.1007/s11664-013-2763-0 ↗
25. Effects of Cu@Sn@Ag core-shell particles on microstructure, corrosion and mechanical properties of SAC305 solder joint
26. Corrosion properties of Cu/Sn–3.0Ag–0.5Cu/Cu solder butt joints fabricated by conventional reflow and microwave hybrid heating10.1016/j.corsci.2022.110641 ↗
27. Corrosion properties of Sn–9Zn/Cu solder joint reflowed by microwave hybrid heating10.1016/j.jmrt.2025.08.085 ↗
28. Aging induced structural and electrochemical corrosion behaviour of Sn-1.0Ag-0.5Cu and Sn-3.8Ag-0.7Cu solder alloys10.1016/j.jallcom.2018.01.292 ↗
29. Microstructure, corrosion and mechanical properties of Sn-3.0Ag-0.5Cu solder alloy aged at 150 °C10.1007/s10854-025-14858-0 ↗
30. Effects of In and aging treatment on the microstructure, mechanical properties and electrochemical corrosion behavior of Sn 2Cu solder alloy10.1016/j.matchar.2024.113740 ↗
31. Influence of CrFeCoNiCu high-entropy alloy and ultrasonic stirring on the thermal, electrochemical and mechanical properties of Zn-30Sn high-temperature solder alloy10.1016/j.matchar.2023.112977 ↗
32. Investigation of microstructure, corrosion and mechanical properties of iron and holmium modified Sn-3.0Ag0.5Cu solder alloy with ultrasonic treatment10.1016/j.matchar.2024.114141 ↗
33. The effect of permanent magnet stirring on the corrosion resistance of Sn-2.0Ag-0.5Cu-2Zn solder alloys in NaCl solution10.1016/j.matchemphys.2023.127774 ↗
34. Effect of alternating voltage treatment on the corrosion resistance of pure magnesium10.1016/j.corsci.2009.05.002 ↗
35. A novel anti-corrosion strategy for ultra-high purity 316 L stainless steel in the semiconductor industry: leveraging alternating voltage passivation and nitric acid passivation10.1016/j.corsci.2025.113153 ↗
36. Effect of alternating voltage passivation on the corrosion resistance of duplex stainless steel10.1007/s10800-008-9718-9 ↗
37. Effect of alternating voltage treatment on corrosion resistance of AZ91D magnesium alloy10.1002/maco.201005999 ↗
38. Enhanced corrosion resistance of AZ31 magnesium alloy by pulse anodization10.1149/2.067308jes ↗
39. Effect of passivation behavior of SAC305 alloy on the structure and defects of surface oxide film
40. Understanding the corrosion protection effect by surface oxide film to underlying Sn solder substrate under thermal exposure condition10.1016/j.corsci.2024.111930 ↗
41. Corrosion behavior of NiTi alloys fabricated by laser powder bed fusion in relation to the formed passive films in Hank’s solution10.1016/j.jmrt.2024.12.182 ↗
42. Distinctive transpassivation behavior and characteristics of passive films of laser powder bed fusion produced and annealed Ti–6Al–4V in Hank’s solution10.1016/j.jmrt.2025.06.201 ↗
43. Metastable pitting corrosion behavior and characteristics of passive film of laser powder bed fusion produced Ti–6Al–4V in NaCl solutions with different concentrations10.1016/j.corsci.2023.111017 ↗
44. In-situ EIS study on the initial corrosion evolution behavior of SAC305 solder alloy covered with NaCl solution10.1016/j.jallcom.2020.156953 ↗
45. Electrochemical corrosion behaviour of SnAgCu (SAC) eutectic alloy in a chloride containing environment
46. Enhancement on the high-temperature joint reliability and corrosion resistance of Sn–0.3Ag–0.7Cu low-Ag solder contributed by Al2O3 Nanoparticles (0.12 wt%)10.1007/s10854-018-0092-z ↗
47. Diffusion impedance of electroactive materials, electrolytic solutions and porous electrodes: Warburg impedance and beyond10.1016/j.electacta.2018.05.136 ↗
48. Analysis of Warburg’s impedance and its equivalent electric circuits10.1039/C7CP04032F ↗
49. Transmission line models for evaluation of impedance response of insertion battery electrodes and cells10.1016/j.powera.2021.100047 ↗
50. Electrochemical impedance spectroscopy for the measurement of the corrosion rate of magnesium alloys: brief review and challenges10.3390/met10060775 ↗
51. Effect of bias voltage on the acceleration of anodic dissolution of SAC305 alloy10.1016/j.jallcom.2025.180866 ↗
52. Native oxide film powered corrosion protection of underlying Pb-free Sn solder substrate10.1016/j.corsci.2023.111359 ↗
53. A perspective on effect by Ag addition to corrosion evolution of Pb-free Sn solder10.1016/j.matlet.2021.129935 ↗
54. Metal oxide nanocomposites: a perspective from strain, defect, and interface
55. Understanding localized corrosion10.1016/S1369-7021(08)70206-2 ↗
56. High-temperature aging time-induced composition and thickness evolution in the native oxides film on Sn solder substrate
57. Corrosion evolution of high-temperature formed oxide film on pure Sn solder substrate10.1016/S1003-6326(22)66073-4 ↗
58. Raman studies of the intermediate tin-oxide phase
59. Vibrational and defect states in SnOx nanoparticles10.1063/1.2203408 ↗
60. IR and Raman spectroelectrochemical studies of corrosion films on tin10.1016/S0013-4686(00)00660-5 ↗
61. Synthesis, characterization and in situ Raman detection of Sn 3 O 2 (OH) 2−x Cl x phases as intermediates in tin corrosion10.1016/j.corsci.2015.05.052 ↗
62. The complete Raman spectrum of nanometric SnO2 particles10.1063/1.1385573 ↗
63. Study on the electrochemical corrosion behavior and solderability of SnAgCuNi solder alloy10.1016/j.jmrt.2025.04.119 ↗
64. B.N. Stirrup, N.A. Hampson, The Active Dissolution of Tin in Concentrated Alkaline Solution, (n.d.). https://doi.org/10.1016/S0022-0728(76)80064-2.10.1016/S0022-0728(76)80064-2 ↗
65. Electrochemical reactions of tin in aqueous electrolytic solutions10.1016/0376-4583(77)90011-5 ↗
66. B.N. Stirrup, N.A. Hampson, Anodic passivation of tin in sodium hydroxide solutions, (n.d.). https://doi.org/10.1016/S0022-0728(76)80063-0.10.1016/S0022-0728(76)80063-0 ↗
67. Selective corrosion of ?-Sn and intermetallic compounds in an Ag-Sn alloy at different potentials in NaCl and Na2SO4 solutions10.1016/j.corsci.2022.110958 ↗
68. Anodic behaviour of tin in potassium hydroxide solution10.1179/000705968798326523 ↗
69. Electrochemical behaviour of tin in alkali solutions containing halides10.1016/j.matchemphys.2011.12.063 ↗
70. On the anodic passivity of tin in alkaline solutions10.1016/0013-4686(64)85039-8 ↗
71. Comprehensive enhancement of pitting corrosion resistance in 2205 duplex stainless steel: mechanisms via defect-rich surface regulation10.1016/j.corsci.2025.113477 ↗
72. Susceptibility of rare-earth-magnesium alloys to micro-galvanic corrosion10.1016/j.corsci.2010.08.006 ↗
73. SKPFM measured Volta potential correlated with strain localisation in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel10.1016/j.corsci.2015.06.035 ↗
74. High-resolution Kelvin probe microscopy in corrosion science: scanning Kelvin probe force microscopy (SKPFM) versus classical scanning Kelvin probe (SKP)10.1016/j.electacta.2007.03.016 ↗
75. Effects of surface micro–galvanic corrosion and corrosive film on the corrosion resistance of AZ91–xNd alloys10.1016/j.apsusc.2020.147761 ↗
76. A strategy to overcome the negative effect of Mg treatment on localized corrosion and enhance the performance of high-nitrogen martensitic stainless steel by Mg&Ce composite treatment10.1016/j.corsci.2025.112852 ↗