journal article·2026-05

Deciphering the role of manganese-alloying on hydrogen embrittlement susceptibility of martensitic steel

Saeed Jamal, Yangwei Wang, Mirza Muhammad Abu Bakar Baig, Saba Shoaib, Lintao Gui, Jian Wang, Fatima Shehzadi, Tahir Mehmood Bhatti, Yan Zhao

Corrosion Science· Volume 263
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (82)

Show source-provided references
1. Lightweighting in the automotive industry as a measure for energy efficiency: Review of the main materials and methods10.1016/j.heliyon.2024.e29728 ↗
2. Bake-partitioning in a press-hardening steel10.1016/j.scriptamat.2018.10.053 ↗
3. A review of hydrogen embrittlement of martensitic advanced high-strength steels
4. New developments of formability evaluation methods for hot stamping10.1088/1757-899X/1270/1/012116 ↗
5. Phase transformation and carbon profile at the interface between Al-Si coating and steel substrate in a press-hardened steel10.1016/j.mtla.2021.101268 ↗
6. Origin of deformation twins and their influence on hydrogen embrittlement in cold-rolled austenitic stainless steel10.1016/j.ijhydene.2021.04.045 ↗
7. Study of temperature effect on hydrogen embrittlement in X70 pipeline steel10.1016/j.corsci.2024.111939 ↗
8. Hydrogen embrittlement property of a 1700-MPa-class ultrahigh-strength tempered martensitic steel10.1088/1468-6996/11/2/025005 ↗
9. Recent progress in medium-Mn steels made with new designing strategies, a review10.1016/j.jmst.2017.06.017 ↗
10. Effect of Ti variation on microstructure evolution and mechanical properties of low carbon medium Mn heavy plate steel10.1016/j.matchar.2019.04.004 ↗
11. Medium Mn transformation-induced plasticity steels: Recent progress and challenges10.1016/j.scriptamat.2016.07.013 ↗
12. Impact of intercritical annealing temperatures on the stability of retained austenite and hydrogen embrittlement resistance of 34MnB5Nb press-hardened steel10.1016/j.ijhydene.2025.04.466 ↗
13. The Effects of Process Temperatures on the Microstructure and Tensile Properties of Warm-Stamped Nb-Bearing Medium-Mn Steel10.1007/s11661-019-05570-w ↗
14. Evaluations of tensile properties as a function of austenitizing temperature and springback by V-bending testing in medium-Mn steels10.1016/j.msea.2020.139534 ↗
15. Impact of precipitates on the hydrogen embrittlement behavior of a V-alloyed medium-manganese austenitic stainless steel10.1016/j.jmrt.2020.09.085 ↗
16. Hydrogen Embrittlement of Medium Mn Steels10.3390/met11020358 ↗
17. The possibility of enhanced hydrogen embrittlement resistance of medium-Mn steels by addition of micro-alloying elements10.1016/j.matchar.2020.110386 ↗
18. Effect of intercritical annealing time on hydrogen embrittlement of warm-rolled medium Mn steel10.1016/j.msea.2018.04.100 ↗
19. Current Challenges and Opportunities Toward Understanding Hydrogen Embrittlement Mechanisms in Advanced High-Strength Steels: A Review10.1007/s40195-021-01233-1 ↗
20. Effect of reverted austenite fraction on hydrogen embrittlement of TRIP-aided medium Mn steel (0.1C-5Mn)10.1016/j.engfailanal.2019.01.018 ↗
21. Enhancing Hydrogen Embrittlement Resistance of Lath Martensite by Introducing Nano-Films of Interlath Austenite10.1007/s11661-015-3009-y ↗
22. Effect of grain size on the susceptibility of martensitic steel to hydrogen-related failure10.1080/09500830500482316 ↗
23. Study of hydrogen-induced delayed fracture in high-Mn TWIP/TRIP steels during in situ electrochemical hydrogen-charging: Role of microstructure and strain rate in crack initiation and propagation10.1016/j.corsci.2019.108191 ↗
24. Microstructure effect on hydrogen-induced cracking in TM210 maraging steel10.1016/j.msea.2013.07.097 ↗
25. Statistical study on the effects of heterogeneous deformation and grain boundary character on hydrogen-induced crack initiation and propagation in twining-induced plasticity steels10.1016/j.corsci.2021.109796 ↗
26. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
27. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
28. In-situ observation of hydrogen induced crack initiation in a nickel-based superalloy10.1016/j.scriptamat.2017.07.006 ↗
29. Impact of chemical inhomogeneities on local material properties and hydrogen environment embrittlement in AISI 304L steels10.1016/j.ijhydene.2018.01.062 ↗
30. Effect of manganese content on the hydrogen embrittlement of twinning-induced plasticity (TWIP) steels under hydrogen charging and hydrogen environment10.1016/j.msea.2022.144289 ↗
31. A fractographic study of gaseous hydrogen embrittlement and liquid-metal embrittlement in a tempered-martensitic steel10.1016/0001-6160(84)90204-9 ↗
32. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
33. Mechanical and microstructural analysis on hydrogen-related fracture in a martensitic steel10.1016/j.ijhydene.2019.09.097 ↗
34. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
35. Hydrogen embrittlement of steels
36. Deformation-induced defects controlling fracture toughness of steel revealed by tritium desorption behaviors10.1016/S1359-6454(99)00392-4 ↗
37. Hydrogen embrittlement of ferritic steels: Observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
38. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
39. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(99)00094-6 ↗
40. Characteristics and mechanisms of hydrogen-induced quasi-cleavage fracture of lath martensitic steel10.1016/j.actamat.2021.116635 ↗
41. Factors Distinguishing Hydrogen-Assisted Intergranular and Intergranular-Like Fractures in a Tempered Lath Martensitic Steel10.1007/s11661-022-06608-2 ↗
42. Multiscale thermodynamic analysis on fracture toughness loss induced by solute segregation in steel10.1080/14786435.2014.906757 ↗
43. Hydrogen trapping and embrittlement of titanium- and vanadium carbide-containing steels after high-temperature hydrogen charging10.1007/s10853-024-09611-7 ↗
44. Recent progress of molybdenum carbide based electrocatalysts for electrocatalytic hydrogen evolution reaction10.1039/D3NR02511J ↗
45. On the Methodology of Thermal Desorption Spectroscopy to Evaluate Hydrogen Embrittlement10.4028/www.scientific.net/MSF.706-709.2354 ↗
46. Mitigating hydrogen embrittlement via film-like retained austenite in 2 GPa direct-quenched and partitioned martensitic steels10.1016/j.msea.2024.146872 ↗
47. Influence of microstructure on hydrogen embrittlement in hot-rolled medium Mn steels10.1016/j.msea.2020.139147 ↗
48. Study of the electrochemical permeation of hydrogen in iron10.1016/j.corsci.2008.10.024 ↗
49. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
50. Determination of dislocation density by electron backscatter diffraction and X-ray line profile analysis in ferrous lath martensite10.1016/j.matchar.2015.11.014 ↗
51. Dislocation Density within Lath Martensite in Fe-C and Fe-Ni Alloys10.2355/isijinternational.43.1475 ↗
52. Identification of prior β grains of additive manufactured Ti-6Al-4V alloy using electron backscatter diffraction10.1016/j.matlet.2022.132758 ↗
53. Effect of thermomechanical processing on the grain boundary character distribution of phosphorus bronze10.1016/j.matchar.2024.114401 ↗
54. A Two-Step Thermomechanical Process for Improving High-Angle Grain Boundary Proportion and Achieving Delamination Toughening in Hot-Rolled Steel with a Limited Slab-to-Plate Ratio10.1002/srin.202200085 ↗
55. Grain boundary energy effect on grain boundary segregation in an equiatomic high-entropy alloy
56. Antagonist effects of grain boundaries between the trapping process and the fast diffusion path in nickel bicrystals10.1038/s41598-021-94107-6 ↗
57. Quantitative hydrogen trap states on high-angle grain boundaries and at dislocations in iron10.1016/j.scriptamat.2023.115339 ↗
58. Interrelationship between hydrogen and α′-martensite of SUS 304 austenitic stainless steel revealed by tensile tests10.1016/j.msea.2021.142169 ↗
59. Effect of Metal Carbides on Hydrogen Embrittlement: A Density Functional Theory Study10.3390/hydrogen5010009 ↗
60. Difference in hydrogen trapping behaviors between epsilon carbide and cementite in steels10.1016/j.matchar.2024.114557 ↗
61. On the propensity of lath martensite intervariant boundaries to hydrogen absorption using molecular statics simulation10.1016/j.mtla.2022.101539 ↗
62. Effect of Hydrogen Content on the Microstructure, Mechanical Properties, and Fracture Mechanism of Low-Carbon Lath Martensite Steel10.3390/met14121340 ↗
63. Engineering metal-carbide hydrogen traps in steels10.1038/s41467-024-45017-4 ↗
64. New insights into hydrogen trapping and embrittlement in high strength aluminum alloys10.1016/j.corsci.2023.111453 ↗
65. On the Change in Hydrogen Diffusion and Trapping Behaviour of Pearlitic Rail Steel at Different Stages of Production
66. Precipitation processes in steels
67. Switching nanoprecipitates to resist hydrogen embrittlement in high-strength aluminum alloys10.1038/s41467-022-34628-4 ↗
68. Effects of titanium content on hydrogen embrittlement susceptibility of hot-stamped boron steels10.1016/j.jallcom.2017.12.004 ↗
69. Hydrogen embrittlement and hydrogen diffusion behavior in interstitial nitrogen-alloyed austenitic steel10.1016/j.ijhydene.2021.07.084 ↗
70. Effect of hydrogen trapping on hydrogen permeation in a 2205 duplex stainless steel: Role of austenite–ferrite interface10.1016/j.corsci.2022.110332 ↗
71. Hydrogen trapping, desorption and clustering in heterophase interfaces of W-ZrC alloy10.1016/j.actamat.2022.118469 ↗
72. The Thermodynamics of Liquid Dilute Iron Alloys10.1179/msc.1974.8.1.298 ↗
73. Impact of Mn on the solution enthalpy of hydrogen in austenitic Fe-Mn alloys: A first-principles study10.1002/jcc.23742 ↗
74. Effects of solid solution and grain-boundary segregation of Mo on hydrogen embrittlement in 32MnB5 hot-stamping steels10.1016/j.actamat.2021.116661 ↗
75. Achieving ultrahigh strength by tuning the hierarchical structure of low-carbon martensitic steel10.1016/j.msea.2023.145370 ↗
76. A model for the microstructure behaviour and strength evolution in lath martensite10.1016/j.actamat.2015.07.018 ↗
77. Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
78. A study on structural characteristics and metallurgical mechanism of carbides for 440 martensitic stainless steel with different melt refining processes
79. Quantitative investigation on deep hydrogen trapping in tempered martensitic steel10.1016/j.jallcom.2020.157218 ↗
80. Revealing grain refinement and hydrogen trapping mechanism for anti-hydrogen susceptibility of Nb-alloyed 34MnB5 press hardened steel10.1016/j.ijhydene.2024.10.244 ↗
81. The role of titanium and vanadium based precipitates on hydrogen induced degradation of ferritic materials10.1016/j.matchar.2018.06.030 ↗
82. Modeling the Hydrogen Redistribution at the Grain Boundary of Misoriented Bicrystals in Austenite Stainless Steel