Optimization of geometry parameters for ceramic cutting tools in intermittent turning of hardened steel
Source abstract
Abstract
Abstract For the purpose of improving the ceramic cutting tool lives in intermittent hard turning, investigations on optimization of tool geometry parameters were conducted in the present study. The initial damage of the ceramic cutting tool was determined based on damage mechanics. The initial damage was more sensitive to the changes of porosity when it was relatively low. The stress distribution of the tool body was obtained using finite element simulation. The initial damage of the cutting tool and the tool stress were integrated on the basis of the concept of damage equivalent stress. The evolutions of the maximum value of damage equivalent stress on the tool body were acquired for different cutting length ratios and different combinations of tool geometry parameters. The highest value of damage equivalent stress in one cutting cycle was proposed as a new indicator for optimization of tool geometry parameters. The contribution order of tool geometry parameters for the indicator was corner radius, cutting edge angle and rake angle. This order stayed the same at different cutting length ratios. The optimization method for ceramic tool geometry parameters was proposed and it was validated through intermittent turning tests.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced machining processes and optimization · Advanced Surface Polishing Techniques · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Machinability of hardened steel using alumina based ceramic cutting tools10.1016/S0263-4368(03)00004-0 ↗
2. Cutting performance and life prediction of an Al2O3/TiC micro–nano-composite ceramic tool when machining austenitic stainless steel10.1016/j.ceramint.2015.02.012 ↗
3. Machining parameters optimization for alumina based ceramic cutting tools using genetic algorithm10.1080/10910340601009358 ↗
4. Wear resistance of Al2O3/TiB2 ceramic cutting tools in sliding wear tests and in machining processes10.1016/S0924-0136(97)00176-3 ↗
5. Design optimization of cutting parameters when turning hardened AISI 4140 steel (63 HRC) with Al2O3+TiCN mixed ceramic tool10.1016/j.matdes.2006.02.006 ↗
6. Development of Al2O3–SiC composite tool for machining application10.1016/j.ceramint.2003.11.011 ↗
7. Machinability evaluation in hard turning of cold work tool steel (D2) with ceramic tools using statistical techniques10.1016/j.matdes.2006.01.011 ↗
8. Preparation of in-situ growth TaC whiskers toughening Al2O3 ceramic matrix composite10.1016/j.ijrmhm.2012.08.003 ↗
9. Preparation and characterization of Al2O3/TiC micro–nano-composite ceramic tool materials10.1016/j.ceramint.2012.10.277 ↗
10. Cutting performance and failure mechanisms of an Al2O3/WC/TiC micro–nano-composite ceramic tool10.1016/j.ijrmhm.2009.11.007 ↗
11. Damage mechanics analysis of failure mechanisms for ceramic cutting tools in intermittent turning10.1016/j.euromechsol.2012.06.002 ↗
12. Predictability of tool failure modes in turning with complex grooved tools using the equivalent toolface (ET) model10.1016/S0043-1648(00)00447-6 ↗
13. Optimization of tool geometry parameters for turning operations based on the response surface methodology10.1016/j.measurement.2010.11.018 ↗
14. Optimization of cutting insert geometry using DEFORM-3D: numerical simulation and experimental validation10.2507/IJSIMM11(2)1.200 ↗
15. Effect of tool geometry in turning AISI 1045 steel: experimental investigation and FEM analysis10.1007/s13369-014-1054-2 ↗
16. Selection of optimum tool geometry and cutting conditions using a surface roughness prediction model for end milling10.1007/s00170-004-2110-y ↗
17. Simulation-based solid carbide end mill design and geometry optimization10.1007/s00170-014-5638-5 ↗
18. Lemaitre · 2005
19. Damage mechanics: accomplishments, trends and needs10.1016/S0020-7683(99)00081-5 ↗
20. Process simulation using finite element method—prediction of cutting forces, tool stresses and temperatures in high-speed flat end milling10.1016/S0890-6955(99)00080-2 ↗
21. Finite element modeling the influence of edge roundness on the stress and temperature fields induced by high-speed machining10.1007/s00170-006-0720-2 ↗
22. Chip temperature and its effects on chip morphology, cutting forces, and surface roughness in high-speed face milling of hardened steel10.1007/s00170-014-6635-4 ↗
23. Lemaitre · 1992
24. Optimisation for hot turning operations with multiple performance characteristics10.1007/s00170-003-1672-4 ↗
25. Machining and ecological effects of a new developed cutting fluid in combination with different cooling techniques on turning operation10.1016/j.jclepro.2015.01.055 ↗
26. Cutting performance and wear mechanisms of Sialon–Si3N4 graded nano-composite ceramic cutting tools10.1007/s00170-011-3379-2 ↗
27. Finite element method simulation of machining of AISI 1045 steel with a round edge cutting tool
28. The failure of brittle solids containing small cracks under compressive stress states10.1016/0001-6160(86)90086-6 ↗
29. A model for non-linear rock deformation under compression due to sub-critical growth10.1016/0148-9062(91)91121-7 ↗
30. Brittle failure in compression: splitting, faulting, and brittle–ductile transition10.1098/rsta.1986.0101 ↗
31. Micromechanical modelling of the mechanical properties of a granite under dynamic uniaxial compressive loads10.1016/S1365-1609(00)00025-3 ↗
32. Dynamic failure of brittle materials under uniaxial compression
33. A micromechanical model for high strain rate behavior of ceramics10.1016/0020-7683(94)00286-6 ↗
34. Effect of grain size on brittle and semibrittle strength: implications for micromechanical modelling of failure in compression10.1029/JB095iB07p10907 ↗
35. Analysis of PCBN tool failure mechanisms in face milling of hardened steel using damage equivalent stress10.1007/s00170-015-7175-2 ↗
36. The exit failure in interrupted cutting