journal article·2018-05

Influence of composition and crystal structure on the fracture toughness of NbCo2 Laves phase studied by micro-cantilever bending tests

W. Luo, C. Kirchlechner, X. Fang, S. Brinckmann, G. Dehm, F. Stein

Materials & Design· Volume 145
Publisher page

Abstract

Abstract Cubic and hexagonal NbCo2 Laves phases are known to have composition dependent hardness and yield strength. However, it is unknown whether this dependence is also reflected in their fracture toughness values. In order to elucidate the fracture behavior, single-crystalline micro-cantilevers of the cubic and hexagonal NbCo2 Laves phases having different compositions were fabricated in the diffusion layers grown by the diffusion couple technique. Micro-cantilever bending tests were performed to study the composition- and crystal-structure-dependence of the fracture toughness. To exclude the influence of micro-cantilever geometry, pentagonal and rectangular beams were tested and found to result in the same fracture toughness value. The present results reveal that neither a change of the crystal structure nor a change in chemical composition has a significant influence on the fracture toughness of NbCo2 Laves phase.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Laves-phase superalloys?10.1002/pssa.2211310215 ↗
2. Physical metallurgy and mechanical properties of transition-metal Laves phase alloys10.1016/S0966-9795(00)00109-6 ↗
3. Laves phases for high temperatures—part II stability and mechanical properties10.1016/S0966-9795(02)00025-0 ↗
4. Precipitation around welds in the nickel-base superalloy, Inconel 71810.1016/0001-6160(85)90231-7 ↗
5. Precipitation behavior of Laves phase and its effect on toughness of 9Cr-2Mo ferritic-martensitic steel10.1016/S0022-3115(86)80083-6 ↗
6. Mechanical properties of austenitic heat-resistant Fe-20Cr-30Ni-2Nb steel at ambient temperature10.1016/j.msea.2016.03.038 ↗
7. Novel concept of austenitic heat resistant steels strengthened by intermetallics10.4028/www.scientific.net/MSF.539-543.3012 ↗
8. Polytypic transformations in Laves phases10.1016/j.intermet.2004.02.017 ↗
9. Point defects in binary Laves phase alloys10.1016/S1359-6454(99)00090-7 ↗
10. Defect structures and room-temperature mechanical properties of C15 Laves phases in Zr-Nb-Cr and Zr-Hf-Cr alloy systems10.1007/s11661-004-0184-7 ↗
11. Composition dependence of the hardness of Laves phases in the Fe-Nb and Co-Nb systems10.1557/proc-1128-u08-05 ↗
12. Compositional dependence of the compressive yield strength of Fe-Nb(-Al) and Co-Nb Laves phases10.1557/opl.2011.459 ↗
13. Factors affecting the room-temperature mechanical properties of TiCr2-base Laves phase alloys10.1016/S0921-5093(97)00526-1 ↗
14. Microstructures and mechanical properties of NbCr2 and ZrCr2 Laves phase alloys prepared by powder metallurgy10.1023/A:1021807519728 ↗
15. HfCo2 Laves phase intermetallics—part II: elastic and mechanical properties as a function of composition10.1016/S0966-9795(01)00067-X ↗
16. Experimental reinvestigation of the Co–Nb phase diagram10.1016/j.intermet.2008.02.017 ↗
17. Synthesis of defect-free single-phase bars of high-melting Laves phases through modified cold crucible levitation melting10.1016/j.msea.2010.08.066 ↗
18. Phase stability and mechanical behavior of NbCr2-based Laves phases10.1016/S0966-9795(99)00010-2 ↗
19. Comments on “Measurement of the microstructural fracture toughness of cortical bone using indentation fracture”10.1016/j.jbiomech.2008.01.022 ↗
20. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
21. Fracture toughness testing for advanced technical ceramics: internationally agreed good practice10.1179/174367606X84422 ↗
22. Measuring fracture toughness of coatings using focused-ion-beam-machined microbeams10.1557/JMR.2005.0048 ↗
23. A comparative micro-cantilever study of the mechanical behavior of silicon based passivation films10.1016/j.tsf.2009.07.143 ↗
24. Can microscale fracture tests provide reliable fracture toughness values? A case study in silicon10.1557/jmr.2015.2 ↗
25. Micro-scale fracture experiments on zirconium hydrides and phase boundaries10.1016/j.jnucmat.2016.03.026 ↗
26. Lubliner · 2014
27. Overview on micro- and nanomechanical testing: new insights in interface plasticity and fracture at small length scales10.1016/j.actamat.2017.06.019 ↗
28. Microcantilever investigation of fracture toughness and subcritical crack growth on the scale of the microstructure in Al2O310.1016/j.jeurceramsoc.2015.08.023 ↗
29. Temperature dependent fracture initiation in microscale silicon10.1016/j.scriptamat.2016.11.016 ↗
30. Characterization of the fracture toughness of micro-sized tungsten single crystal notched specimens10.1080/14786435.2012.658449 ↗
31. In situ micro-cantilever tests to study fracture properties of NiAl single crystals10.1016/j.actamat.2011.10.060 ↗
32. A method to estimate the influence of the notch-root radius on the fracture toughness measurement of ceramics10.1016/j.jeurceramsoc.2005.02.016 ↗
33. Small-scale fracture toughness of ceramic thin films: the effects of specimen geometry, ion beam notching and high temperature on chromium nitride toughness evaluation10.1080/14786435.2016.1223891 ↗
34. Structure and stability of Laves phases. Part I. Critical assessment of factors controlling Laves phase stability10.1016/j.intermet.2004.02.010 ↗