Application of pure oxygen for the passivation of mild steel in high temperature and pressure Bayer liquor under conditions of disturbed flow

Gareth Kear, Klaus Bremhorst

Corrosion Science· Volume 50· Issue 7
Publisher page

Abstract

The passivation characteristics of sulfuric acid cleaned mild steel in spent Bayer liquor (pH 14.4 and 160 degrees C) are examined using a high pressure nickel flow loop. An entrained atmosphere of 99.90% v/v oxygen gas is incorporated as an experimental variable along with Reynolds number (141,700 and 50,950) and intensity of fluid now disturbance. State of passivation has been defined using criteria derived from transient polaristion resistance measurements an large-scale polarisation, linear sweep voltammetry. In the majority of cases, oxygenation introduces instantaneous passivation of the mild steel on contact with the Bayer liquor. In comparison to de-oxygenated and aerated electrolytes, this rapid rate of passivation can lead to LIP to an order of magnitude reduction in the quantity of charge associated with metal dissolution over 20 h. Although relative rates of corrosion when passive are low and largely independent of the level of flow disturbance, dissolution rates when passive are somewhat larger at the higher Reynolds number. (c) 2008 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Meyer · Wear · 1994 · 176 · 16310.1016/0043-1648(94)90144-9 ↗
2. Meyer · Mater. Perf. · 1994 · 33 · 57
3. Meyer · Wear · 1995 · 189 · 10710.1016/0043-1648(95)06673-X ↗
4. S. Giddey, C.S. Zheng Ya Lu, D.F.A. Koch, Corrosion of mild steel in turbulent caustic solution, in: Proceedings of 13th International Corrosion Congress, Australasian Corrosion Association, Melbourne, Australia, 1996.
5. Giddey · Corros. Sci. · 1998 · 40 · 83910.1016/S0010-938X(97)00162-5 ↗
6. S. Giddey, B. Cherry, F. Lawson, M. Forsyth, D.F.A. Koch, High temperature, high pressure equipment for the study of erosion corrosion of metals in corrosive liquors – application to the electrochemical behaviour of AISI 1020 steel in Bayer liquor, in: Proceedings of Corrosion and Prevention’97, Australian Corrosion Association, Melbourne, Australia, 1997.
7. Lu · J. Appl. Electrochem. · 2001 · 31 · 137310.1023/A:1013824010279 ↗
8. Rihan · Corros. Sci. · 2006 · 48 · 263310.1016/j.corsci.2005.09.018 ↗
9. Rihan · Corros. Sci. · 2006 · 48 · 266010.1016/j.corsci.2005.09.019 ↗
10. Kear · Corrosion · 2008 · 64 · 28910.5006/1.3278473 ↗
11. Rocchini · Corros. Sci. · 1994 · 36 · 204310.1016/0010-938X(94)90007-8 ↗
12. Battino · J. Phys. Chem. Ref. Data · 1983 · 12 · 16310.1063/1.555680 ↗
13. J.T. Malito, M.L. Roberson, Removal of high molecular weight organic compounds from Bayer process caustic liquor, United States Patent: 4,663,133, 1987.
14. Pletcher · 1991
15. AS/NZS 3679.1, Structural steel – hot-rolled bars and sections, Standards Australia/Standards New Zealand, Homebush, Australia/Wellington, New Zealand, 1996.
16. G. Kear, K. Bremhorst, S. Coles, S.-H. Huáng, Corros. Sci., in press, doi: 10.1016/j.corsci.2008.04.001.10.1016/j.corsci.2008.04.001 ↗
17. Nesic · Corrosion · 2000 · 56 · 100510.5006/1.3294377 ↗
18. ASTM G61, Standard test method for conducting cyclic potentiodynamic polarization measurements for localized corrosion susceptibility of iron-, nickel-, or cobalt-based alloys, ASTM International, West Conshohocken, USA, 2003.
19. Pourbaix · 1966
20. Tafel · Z. Phys. Chem. · 1905 · 50 · 64110.1515/zpch-1905-5043 ↗
21. Craig · 1991