Impact of transient chemistry on the corrosion potential of a steam turbine disc steel
Source abstract
Abstract
Abstract The adoption of two-shifting in coal-fired power generation (switching from on-load to off-load conditions on a daily basis and off-load for the weekend) results in regular cycling of the solution chemistry of the condensed steam on the turbine discs. A first stage investigation has been made of the effect of such chemistry cycling on the corrosion potential of the disc steel. The corrosion potential is typically about +0.05 V (SCE) in off-load chemistry (aerated pure water) and below −0.6 V (SCE) in on-load chemistry (deaerated solution containing chloride or chloride and sulphate anions). The critical observation was the sluggish response of the corrosion potential upon restoration of deaerated on-load conditions with the implication of a likely increase in pit and stress corrosion crack development.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Zhou · Corros. Eng. Sci. Tech. · 2003 · 38 · 9710.1179/147842203767789177 ↗
2. S. Zhou, A, Turnbull, Environment assisted cracking of steam turbine disc and blade steels – description of test procedure and preliminary results, NPL Report MATC (A) 41, 2001.
3. Turnbull · Corros. Sci. · 2004 · 46 · 19310.1016/S0010-938X(03)00118-5 ↗
4. Corrosion of steam turbine blading and discs in the phase transition zone, Electric Power Research Institute, Palo Alto, CA, TR-111340, November 1998.
5. G.J. Bignold, G.P. Quirk, Corrosion 2002, Paper No. 02333, NACE, Houston, 2002.
6. Zhou · Corrosion · 2006 · 62 · 50810.5006/1.3279909 ↗
7. Ritter · Power Plant Chem. · 2004 · 6 · 748
8. Liu · Corros. Sci. · 1994 · 36 · 201710.1016/0010-938X(94)90005-1 ↗
9. H.S. Isaacs, The pitting of iron in dilute chloride and sulphate solution, in advances in Localised Corrosion, in: H.S. Isaacs, U. Bertocci, J. Kruger, S. Smialowska (Eds.), NACE, Houston, Orlando 1987, 1990, pp. 221–226.
10. Schmuki · J. Electrochem. Soc. · 1996 · 143 · 57410.1149/1.1836483 ↗
11. Virtanen · J. Electrochem. Soc. · 1997 · 144 · 19810.1149/1.1837385 ↗
12. A. Turnbull, Current understanding of environment induced cracking of steam turbine steels, Paper No. 07RTS5, in: CORROSION/07, NACE Int. Houston, TX, 2007.10.5006/1.3278482 ↗