Growth behavior and barrier mechanism of corrosion product layer from calcium-magnesium-aluminosilicate on Yb2Si2O7-Yb2SiO5 composite environmental barrier coatings at 1300 ℃

Shuang Yu, Shuqi Wang, Yaming Wang, Zhiyun Ye, Qiang Zhao, Yang Li, Dawei Ren, Guoliang Chen, Yongchun Zou, Jiahu Ouyang, Dechang Jia, Yu Zhou

Corrosion Science· Volume 255
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. The application of ceramic-matrix composites to the automotive ceramic gas turbine10.1016/S0266-3538(99)00016-0 ↗
2. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
3. High-temperature oxidation of silicon carbide and silicon nitride10.2320/matertrans1989.38.821 ↗
4. SiC and Si3N4 recession due to SiO2 scale volatility under combustor conditions10.1111/j.1151-2916.1999.tb02005.x ↗
5. Oxidation behavior of a multilayered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
6. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
7. SiC recession caused by SiO2 scale volatility under combustion conditions: II10.1111/j.1151-2916.1999.tb02005.x ↗
8. Current status of environmental barrier coatings for Si-based ceramics
9. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
10. Stability and CMAS resistance of ytterbium-silicate/hafnate EBCs/TBC for SiC composites10.1111/jace.13262 ↗
11. Silicate deposit degradation of engineered coatings in gas turbines: progress toward models and materials solutions10.1146/annurev-matsci-010917-105000 ↗
12. Jr., Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
13. Calcium-magnesium-alumino-silicate interaction with yttrium monosilicate environmental barrier coatings10.1111/j.1551-2916.2010.03916.x ↗
14. Calcium-magnesium-aluminosilicate (CMAS) reactions and degradation mechanisms of advanced environmental barrier coatings10.1016/j.surfcoat.2013.08.036 ↗
15. Chemical and mechanical consequences of environmental barrier coating exposure to calcium-magnesium- aluminosilicate10.1111/j.1551-2916.2011.04448.x ↗
16. CMAS degradation of environmental barrier coatings10.1016/j.surfcoat.2007.06.045 ↗
17. D.M. Zhu, Aerospace ceramic materials: thermal, environmental barrier coatings and SiC/SiC ceramic matrix composites for turbine engine applications, (2018) 1-30..
18. Development and property evaluation of selected Si-HfO2 and rare earth-silicon based bond coats and environmental barrier coating systems for SiC/SiC ceramic matrix composites
19. Micromechanical analysis and theoretical predictions towards thermal shock resistance of Si-HfO2 environmental barrier coatings10.1016/j.compositesb.2021.109334 ↗
20. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N410.1016/j.jeurceramsoc.2004.12.013 ↗
21. Environmental barrier coatings for SiCf/SiC
22. Stresses in ytterbium silicate multilayer environmental barrier coatings
23. Residual stresses and phase transformations in ytterbium silicate environmental barrier coatings
24. Microstructure and thermal properties of atmospheric plasma-sprayed Yb2Si2O7 coating10.1007/s11666-016-0482-9 ↗
25. R. Vassen, Yb2Si2O7 environmental barrier coatings deposited by various thermal spray techniques: a preliminary comparative study10.1007/s11666-017-0574-1 ↗
26. Mixed phase ytterbium silicate environmental-barrier coating materials for improved calcium-magnesium-alumino-silicate resistance10.1557/jmr.2020.151 ↗
27. Thermal shock resistance of tri-layer Yb2SiO5/Yb2Si2O7/Si coating for SiC and SiC-matrix composites10.1111/jace.15713 ↗
28. Phase and microstructure evolution in plasma sprayed Yb2Si2O7 coatings10.1016/j.jeurceramsoc.2018.11.018 ↗
29. Characterization of Yb2Si2O7-Yb2SiO5 composite environmental barrier coatings resultant from in situ plasma spray processing10.1016/j.ceramint.2020.05.228 ↗
30. Resistance of pure and mixed rare earth silicates against calcium-magnesium-aluminosilicate (CMAS): A comparative study10.1111/jace.17328 ↗
31. Phase composition evolution and oxidation behavior of atmospheric plasma spraying Si and Si-HfO2 bond coats at 1300 ℃10.1016/j.corsci.2023.111439 ↗
32. Effect of the surface microstructure ablated by femtosecond laser on the bonding strength of EBCs for SiC/SiC composites10.1016/j.optcom.2018.04.055 ↗
33. Molten silicate reactions with plasma sprayed ytterbium silicate coatings10.1016/j.surfcoat.2015.12.053 ↗
34. Yb2Si2O7 environmental barrier coatings deposited by various thermal spray techniques: a preliminary comparative study10.1007/s11666-017-0574-1 ↗
35. Structure, composition, and defect control during plasma spray deposition of ytterbium silicate coatings10.1007/s10853-015-9358-5 ↗
36. Molten silicate reactions with plasma sprayed ytterbium silicate coatings10.1016/j.surfcoat.2015.12.053 ↗
37. General trend on the phase stability and corrosion resistance of rare earth monosilicates to molten calcium magnesium aluminosilicate at 1300 ℃10.1016/j.corsci.2018.12.032 ↗
38. Study of calcium–magnesium–aluminum–silicate (CMAS) glass and glass-ceramic sealant for solid oxide fuel cells10.1016/j.jpowsour.2012.12.055 ↗
39. Properties of CMAS glass from desert sand10.1016/j.ceramint.2014.11.072 ↗
40. Corrosion of RE2Si2O7 (RE=Y, Yb, and Lu) environmental barrier coating materials by molten calcium-magnesium-alumino-silicate glass at high temperatures10.1016/j.jeurceramsoc.2019.05.036 ↗
41. Tunable corrosion resistance of rare-earth monosilicate to molten calcia-magnesia-aluminosilicate glass by RE-doping strategy10.1016/j.corsci.2022.110319 ↗
42. Mass spectrometric measurements of the silica activity in the Yb2O3-SiO2 system and implications to assess the degradation of silicate-based coatings in combustion environments10.1016/j.jeurceramsoc.2015.07.019 ↗
43. Effects of cation substitution and temperature on the interaction between thermal barrier oxides and molten CMAS10.1016/j.jeurceramsoc.2014.09.006 ↗
44. Improvement of a bulk optical basicity table for oxidic systems10.1006/jssc.1997.7722 ↗
45. Ionic-covalent character of metal and nonmetal oxides10.1021/jp063846j ↗
46. 2ZrO2·Y2O3 thermal barrier coatings resistant to degradation by molten CMAS: Part I10.1111/jace.13210 ↗
47. Electronic polarizability and optical basicity of lanthanide oxides10.1016/j.physb.2006.11.015 ↗
48. G. Guti´errez, Gibbs’ phase rule revisited10.1007/BF02070248 ↗
49. Model of interface-coupled dissolution-precipitation mechanism of pseudomorphic replacement reaction in aqueous solutions based on the system of cerussite PbCO3-pyromorphite Pb5(PO4)3Cl10.1016/j.gca.2020.08.015 ↗
50. Interaction of yttrium disilicate environmental barrier coatings with calcium-magnesium-iron alumino-silicate melts10.1016/j.actamat.2017.12.004 ↗
51. Viscosity of nitrogen containing Y2O3-Al2O3-SiO2 melts and hardness of glasses
52. Garnet stability in the Al-Ca-Mg-Si-Y-O system with implications for reactions between TBCs, EBCs, and silicate deposits10.1111/jace.17176 ↗
53. Thermodynamics of reaction between gas-turbine ceramic coatings and ingested CMAS corrodents10.1111/jace.16113 ↗
54. Calcium-magnesium aluminosilicate (CMAS) interactions with ytterbium silicate environmental barrier coating material at elevated temperatures10.1016/j.ceramint.2020.03.249 ↗
55. Mechanical and thermal properties of calcium-magnesium aluminosilicate (CMAS)10.1016/j.jeurceramsoc.2015.03.032 ↗
56. Thermochemical interactions between CMAS and Ca2Y8(SiO4)6O2 apatite environmental barrier coating material10.1016/j.jeurceramsoc.2019.08.040 ↗
57. Viscosity of CaO-MgO-Al2O3-SiO2 (CMAS) melts: experimental measurements and comparison to model calculations10.1016/j.jnoncrysol.2022.121508 ↗