The corrosion behavior of a sputtered micrograin film on Fe-5Cr-5Si alloy in H 2 -CO 2 -H 2 S mixture at 700 °C
Source abstract
Abstract
Abstract The corrosion behaviors of as-cast Fe-5Cr-5Si alloy with and without sputtered Fe-5Cr-5Si film in H 2 -CO 2 -H 2 S mixture at 700 °C are studied. The corrosion scale forming on the as-cast alloy is non-protective and mainly composed of FeS outer layer and FeS + FeCr 2 O 4 + Fe 2 SiO 4 inner layer. However, a continuous Cr 2 O 3 + SiO 2 layer which possesses favorable protectiveness forms at the coating/alloy interface for the coated alloy, even though FeS layer and FeS + FeCr 2 O 4 + Fe 2 SiO 4 mixed layer also form. The formation mechanism of the Cr 2 O 3 + SiO 2 layer on the coated alloy is discussed thoroughly.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal Alloys Wear and Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Sulfidation and Mixed Gas Corrosion of Alloys
2. Mechanisms of the simultaneous sulfidation and oxidation of Fe-Mn alloys10.1016/0010-938X(96)00117-5 ↗
3. Corrosion of binary Fe-Si alloys in reducing oxidizing and sulfidizing-oxidizing atmospheres at 700°C10.1007/s11085-013-9459-y ↗
4. The corrosion of Fe-15wt% Y and Fe-30wt% Y in sulfidizing-oxidizing atmospheres at 600–800°C10.1016/S0010-938X(98)00170-X ↗
5. The oxidation-sulfidation of Ni-Nb alloys at 600–800°C in H2-H2S-CO2 mixtures10.1016/0010-938X(94)00128-S ↗
6. The corrosion of Co-15wt.% Y at 600–800 degrees C in sulfidizing-oxidizing atmospheres10.1023/A:1018887110251 ↗
7. The oxidation-sulfidation of Fe-Nb alloys at 600–800°C in H2-H2S-CO210.1016/0010-938X(94)90025-6 ↗
8. Enabling theory
9. Sulfidation behavior of Fe-25Cr-20Ni-Si in H2/H2O/H2S/Ar at 700°C10.5006/1.3585310 ↗
10. Sulfidation–oxidation behavior of FeCrAl and TiCrAl and the third-element effect10.1007/s11085-010-9194-6 ↗
11. Enhanced sulphidation/oxidation resistance of Ti-45Al-8Nb alloy by nanostructured CrAlYN/CrN coatings at 750°C10.1002/maco.201106417 ↗
12. Tortorelli · 1996 · 175
13. Thermal oxidation kinetics and oxide scale adhesion of Fe–15Cr alloys as a function of their silicon content10.1016/j.actamat.2006.04.023 ↗
14. Scaling behavior of two Fe-xCr-5Si alloys under high and low oxygen pressures at 700°C10.1016/j.corsci.2015.08.034 ↗
15. Sulfidation kinetics of iron and ferritic iron-cobalt alloys10.1149/1.2132792 ↗
16. High temperature sulfidation behavior of low Al iron-aluminum compositions10.1016/S1359-6462(98)00108-0 ↗
17. Self-diffusion of iron and sulfur in ferrous sulfide10.1007/BF00603390 ↗
18. Diffusion-limited sulfidation of wustite10.1007/BF02825678 ↗
19. The diffusion of Fe3+ in amorphous SiO2 and the protective properties of SiO2 layers10.1016/0010-938X(81)90063-9 ↗
20. The oxidation resistance of a sputtered: microcrystalline TiAl-intermetallic-compound film10.1007/BF01046890 ↗
21. Oxidation kinetics of sputtered Ni-5Cr-5Al nanocrystalline coating at 900°C and 1000°C10.1016/S0965-9773(99)00351-7 ↗
22. Influence of grain size on the oxidation resistance of 2 4 1 Cr-1Mo steel10.1007/BF00665627 ↗
23. Surface composition of magnetron sputtered Pt-Co thin film catalyst for proton exchange membrane fuel cells10.1016/j.apsusc.2016.01.004 ↗
24. Influence of annealing on structural morphological, compositional and surface properties of magnetron sputtered nickel–titanium thin films10.1016/j.apsusc.2013.05.159 ↗
25. On the structure and surface chemical composition of indium–tin oxide films prepared by long-throw magnetron sputtering10.1016/j.tsf.2008.10.146 ↗
26. Sulfidation of iron at high temperatures and diffusion kinetics in ferrous sulfide10.1007/BF00606194 ↗
27. Determination of diffusion-coefficient of oxygen in alpha-iron from internal oxidation measurements in Fe-Si alloys10.1007/BF00547959 ↗
28. Diffusion and solubility of sulphur in iron and silicon