Abstract

Abstract The corrosion behaviour of AA 1370 in different metallurgical states was studied in chloride-containing sulphate solutions. The microstructures of a rod, a deformed strand and an annealed strand constitutive of wires were examined using scanning electron microscopy, transmission electron microscopy and electron backscattered diffraction. Results offered evidence for the ultra-fine grain size, high density of interfaces and high level of misorientation of the interfaces as relevant explanations for the low corrosion resistance of the deformed strand compared to the rod and the annealed strand.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Intermetallic phase selection in 1xxx Al alloys10.1016/S0079-6425(98)00003-6 ↗
2. An assessment of the entire Al-Fe system including D03 ordering10.1016/j.actamat.2009.02.046 ↗
3. Effect of iron-containing intermetallic particles on the corrosion behaviour of aluminum10.1016/j.corsci.2006.01.005 ↗
4. Scanning Microsensors for measurement of local pH distributions at the microscale10.1149/1.1837020 ↗
5. The dissolution of FeAl3 Intermetallic compound and deposition on aluminum in AlCl3 solution10.1016/0010-938X(90)90060-I ↗
6. Electrochemical corrosion parameters of as-cast Al-Fe alloys in a NaCl solution10.1016/j.corsci.2010.05.011 ↗
7. Influence of severe plastic deformations on secondary phase precipitation in a 6082 Al-Mg-Si alloy10.1007/s11661-005-0226-9 ↗
8. Microstructure of two-phase Al 1.7 at% Cu alloy deformed by equal channel angular pressing10.1016/S1359-6454(00)00308-6 ↗
9. Microstructures in the 6060 aluminium alloy after various severe plastic deformation treatments10.1016/j.matchar.2011.01.009 ↗
10. Impact of ultrafine-grained microstructure on the corrosion of aluminium alloy AA202410.1016/j.corsci.2011.12.016 ↗
11. Recovery and recrystallization in commercial purity aluminum cold rolled to an ultrahigh strain10.1016/j.actamat.2013.05.024 ↗
12. Microstructure and local crystallography of cold rolled aluminum10.1016/0956-7151(94)00473-U ↗
13. The development of microstructure and the influence of processing route during equal channel angular drawing of pure aluminium10.1016/S0921-5093(98)01129-0 ↗
14. Effect of grain size on corrosion of high purity aluminium10.1016/j.electacta.2010.09.023 ↗
15. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
16. Effect of friction stir processing on electrical conductivity and corrosion resistance of AA6063-T6 Al alloy10.1243/09544062JMES847 ↗
17. The role of macrostructural morphology and grain size on the corrosion resistance of Zn and Al castings10.1016/j.msea.2005.02.094 ↗
18. Influence of grain size on mechanical and corrosion properties of magnesium alloy for medical implants10.1002/mawe.200900434 ↗
19. Grain Boundary Character distribution and intergranular corrosion behavior in high purity aluminium10.1016/S1359-6462(00)00682-5 ↗
20. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
21. Transition between low and high angle grain boundaries10.1016/j.actamat.2005.03.005 ↗
22. Effect of heat-treatment on filiform corrosion of aluminum alloy AA300510.1016/S0010-938X(01)00014-2 ↗
23. Effect of heat-treament on electrochemical behaviour of aluminum alloy AA300510.1016/S0010-938X(01)00024-5 ↗
24. Filiform corrosion of aluminum sheet III. Microstructure of reactive surfaces10.1016/S0010-938X(98)00094-8 ↗
25. Influence of the altered surface layer on the corrosion of AA508310.1149/2.0321506jes ↗
26. Surface morphological changes of aluminum alloys in alkaline solution: effect of second phase material10.1016/S0010-938X(98)00188-7 ↗
27. Stress corrosion cracking susceptibility of ultra-fine grain copper produced by equal-channel angular pressing10.1016/S0921-5093(01)01332-6 ↗
28. Rolling textures in F.C.C. and B.C.C metals10.1016/0001-6160(64)90204-4 ↗
29. Preferred orientation in extruded aluminum alloy rod10.1016/0036-9748(83)90169-2 ↗
30. Effect of deformation path change on plastic response and texture evolution for 1050 Al pre-deformed by ECAP and subsequently plane strain compressed10.1016/j.msea.2010.01.003 ↗
31. Microstructure evolution and strengthening mechanisms of cold-drawn commercially pure aluminum wire10.1016/j.msea.2015.04.102 ↗
32. Mechanical properties, microstructure and texture of single pass equal channel angular pressed 1050, 5083, 6082 and 7010 aluminum alloys with different dies10.1016/j.matdes.2011.03.006 ↗
33. Deformation microstructures10.1016/0956-716X(92)90125-X ↗
34. Continuous recrystallisation of lamellar deformation structures produced by severe deformation10.1016/j.actamat.2004.03.019 ↗
35. Severe plastic deformation of commercial purity aluminum by rotary swaging: microstructure evolution and mechanical properties10.1016/j.msea.2012.12.046 ↗
36. Microstructure and strength of commercial purity aluminium10.1016/S1359-6454(02)00174-X ↗
37. Effect of the number of ECAP pass time on the electrochemical properties of 1050 Al alloys10.1016/j.msea.2003.08.056 ↗
38. Effect of grain boundary structure on sensitization and corrosion of stainless steel10.1007/BF02668561 ↗
39. A study of the relation between grain boundary type and sensitisation in partially-sensitised AISI 304 stainless stell using Electron Back-Scattering patterns10.1016/0036-9748(89)90480-8 ↗