Effect of water vapor content on the corrosion mechanism of HR3C in simulated oxy-coal combustion environment
Source abstract
Abstract
The corrosion performance of the HR3C steels covered with salt deposition (Na 2SO 4:K 2SO 4 = 1:1) was investigated under various water vapor content at 700 °C. Results show that the HR3C alloy undergoes severe pitting and sulfidation in a dry corrosive atmosphere (0.5SO 2-4O 2-CO 2 ) and the corrosion products are peculiarly prone to peel off. In comparison, the corrosion behavior is gradually mitigated with increasing water vapor content. In highly humid corrosive gas (0.5SO 2-4O 2-20H 2O-CO 2 ), the corrosion degree is remarkably faint and the dominant corrosion mode is oxidation. The mechanism responsible for the transition of corrosion mode as water vapor content varied is discussed in detail.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Energetic Materials and Combustion · Industrial Gas Emission Control
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Clean coal technology development in China10.1016/j.enpol.2009.06.003 ↗
2. High-efficiency coal-fired power plants development and perspectives10.1016/j.energy.2005.05.025 ↗
3. Techno-economic study of CO2 capture from an existing coal-fired power plant: MEA scrubbing vs. O2/CO2 recycle combustion10.1016/S0196-8904(03)00040-2 ↗
4. M. Lucquiaud, 10 - CO2 capture-ready ultra-supercritical coal power plants, in: D. Zhang (Ed.) Ultra-Supercritical Coal Power Plants, Woodhead Publishing, 2013, pp. 244-271.10.1533/9780857097514.2.244 ↗
5. Oxy-fuel combustion of pulverized coal in an industrial boiler with a tangentially fired furnace
6. Ash and deposit formation from oxy-coal combustion in a 100kW test furnace10.1016/j.ijggc.2011.04.003 ↗
7. Mercury and SO3 emissions in oxy-fuel combustion10.1016/j.egypro.2014.11.041 ↗
8. A. Di Gianfrancesco, 19 - Worldwide overview and trend for clean and efficient use of coal, in: A. Di Gianfrancesco (Ed.) Materials for Ultra-Supercritical and Advanced Ultra-Supercritical Power Plants, Woodhead Publishing, 2017, pp. 643-687.10.1016/B978-0-08-100552-1.00019-1 ↗
9. Effect of SO2 in flue gas on coal ash hot corrosion of Inconel 740 alloy - A high temperature electrochemical sensor study10.1016/j.corsci.2013.07.012 ↗
10. Fireside corrosion behaviors of super304H and HR3C in coal ash/gas environment with different SO2 contents at 650 °C10.1007/s11665-017-3051-6 ↗
11. Rates of fireside corrosion of superheater and reheater tubes: making sense of available data10.1179/1878641314Y.0000000030 ↗
12. Corrosion behaviour of Fe-Cr-(Mn, Si) ferritic alloys in wet and dry CO2-SO2 atmospheres at 650 °C10.1007/s11085-017-9826-1 ↗
13. J.M. Wheeldon, J.P. Shingledecker, 4 - Materials for boilers operating under supercritical steam conditions, in: D. Zhang (Ed.) Ultra-Supercritical Coal Power Plants, Woodhead Publishing, 2013, pp. 81-103.10.1533/9780857097514.1.81 ↗
14. Atomic origins of water-vapour-promoted alloy oxidation10.1038/s41563-018-0078-5 ↗
15. Review of flue gas acid dew-point and related low temperature corrosion10.1016/j.joei.2020.02.004 ↗
16. Prediction of sulfuric acid dew point temperature on heat transfer fin surface10.1016/j.applthermaleng.2015.12.078 ↗
17. In situ study of dew point corrosion by electrochemical measurement10.1016/j.corsci.2013.03.001 ↗
18. Experimental study on the removal of SO3 from coal-fired flue gas by alkaline sorbent10.1016/j.fuel.2019.116306 ↗
19. Effects of solid NaCl deposit and water vapor on corrosion resistance of K452 superalloy and aluminized coating10.1016/j.corcom.2022.07.004 ↗
20. Effect of water vapor content on corrosion performance of aluminide coatings on TP347H in a simulated biomass combustion environment10.1016/j.jmrt.2022.07.170 ↗
21. The effects of water vapour on the hot corrosion of gas turbine blade materials at 700 °C10.1080/09603409.2022.2056299 ↗
22. Oxy-fuel and air atmosphere combustions of Chinese medicine residues: performances, mechanisms, flue gas emission, and ash properties10.1016/j.renene.2021.10.010 ↗
23. Effect of pre-oxidation on hot corrosion resistance of HR3C stainless steel in sulfate salt with or without Fe2O310.1016/j.corsci.2021.109789 ↗
24. Investigation on the hot corrosion behavior of a single crystal Ni-based superalloy in molten Na2SO4 + K2SO4 salts improved by different preoxidation treatments10.1016/j.corsci.2023.111377 ↗
25. High-temperature oxidation and hot corrosion of Ni-based single crystal superalloy in the incubation stage10.1016/j.corsci.2023.111026 ↗
26. Structural characteristics and wear, oxidation, hot corrosion behaviors of HVOF sprayed Cr3C2-NiCr hardmetal coatings10.1016/j.surfcoat.2023.129319 ↗
27. Effect of oxygen doping on the corrosion behavior of nanocrystalline coating under the synergy of solid NaCl deposit and water vapor10.1016/j.jmst.2022.09.023 ↗
28. Hot corrosion behaviors of TP347H and HR3C stainless steel with KCl deposit in oxy-biomass combustion10.1016/j.jenvman.2020.110411 ↗
29. Oxidation of Sanicro 25 (42Fe22Cr25NiWCuNbN) in O2 and O2 + H2O Environments at 600–750 °C10.1007/s11085-015-9528-5 ↗
30. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
31. The effect of water vapor on the transition from internal to external oxidation of austenitic steels at 1,073 K10.1007/s11085-012-9350-2 ↗
32. Fuel ash corrosion of boiler and superheater tubes10.1023/A:1018585129341 ↗
33. D.J. Young, Chapter 8 - Corrosion by Sulphur, in: D.J. Young (Ed.) High Temperature Oxidation and Corrosion of Metals (Second Edition), Elsevier, 2016, pp. 393-430.10.1016/B978-0-08-100101-1.00008-X ↗
34. Synergistic dissolution of oxides in molten sodium sulfate10.1149/1.2086647 ↗
35. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
36. Mechanochemical-molten salt synthesis of α-Al2O3 platelets10.1016/j.ceramint.2015.03.095 ↗
37. Size control of α-Al2O3 platelets synthesized in molten Na2SO4 flux10.1111/j.1551-2916.2004.00533.x ↗
38. Growth habit of rutile and α-Al2O3 crystals10.1016/S0022-0248(99)00419-4 ↗
39. Corrosion behaviour of Fe-Cr-(Mn, Si) Ferritic alloys in wet and dry CO2–SO2 atmospheres at 650 °C10.1007/s11085-017-9826-1 ↗
40. Role of alloying elements and carbides in the chlorine-induced corrosion of steels and alloys10.1590/S1516-14392004000100013 ↗