journal article·2024-02

Heating/cooling-induced formation, dissociation and phase separation of CuFe2O4 during thermal oxidation of Sm2(Co, Fe, Cu, Zr)17 permanent magnet

Ravi Teja Mittireddi, Nisha Hiralal Makani, Ranjan Kumar Singh, Rupak Banerjee, Emila Panda

Corrosion Science· Volume 227
Publisher page

Abstract

This paper addresses the heating/cooling-induced formation, dissociation and phase separation during thermal oxidation of Sm 2(Co, Fe, Cu, Zr) 17 alloys at 298.15 K-973 K, using real-time and room-temperature measurements. Whereas, Fe 3O 4 forms at 673 K ≤ T ≤ 773 K, it transforms to CuFe 2O 4 at 823 K ≤ T ≤ 973 K because of the incorporation of Cu +2 into the octahedral Fe +2 lattice sites in Fe 3O 4. CuFe 2O 4 dissociates instantaneously upon cooling, and separates into layered structure of Cu-oxides at oxide-surface and Fe 3O 4 underneath. A detailed discussion on possible reaction pathways leading to these phenomena during the heating/cooling cycle is presented here.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties and Synthesis of Ferrites · Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. RETM5 and RE2TM17 permanent magnets development10.1063/1.341084 ↗
2. M. Marinescu, J.F. Liu and M.H. Walmer, Recent Progress in Sm-Co Type Permanent Magnets M. Marinescu, J. F. Liu and M. H. Walmer Electron Energy Corporation, Landisville, PA, USA, (2008) 1–8.
3. Metallurgical behavior of Sm(Co, Fe, Cu, Zr)z alloys10.1063/1.333575 ↗
4. Magnetic and structural properties of commercial Sm2(Co, Fe, Cu, Zr)17-based magnets10.1063/1.367565 ↗
5. A new class of permanent-magnetic materials for high temperature applications in TWTs
6. Prediction of the oxidation behaviour of Sm-Co-based magnets10.1016/j.jmmm.2004.11.408 ↗
7. Corrosion behavior of Sm-Co-based permanent magnets in oxidizing environments10.1109/TMAG.2004.829195 ↗
8. The oxidation morphology of SmCo alloys10.1016/j.jallcom.2009.07.115 ↗
9. The mechanism of high temperature oxidation of a SmCo-based magnetic alloy10.1016/j.corsci.2012.04.028 ↗
10. Decomposition behavior in the early-stage oxidation of Sm2Co17-type magnets10.1016/j.scriptamat.2021.113911 ↗
11. Atomic-scale oxidation of a Sm2Co17-type magnet10.1016/j.actamat.2021.117343 ↗
12. The oxidation morphology of SmCo alloys10.1016/j.jallcom.2009.07.115 ↗
13. Internal oxidation of Sm(CobalFe0.22Cu0.08Zr0.02)7.5 alloy at 700°C10.1016/j.corsci.2013.01.038 ↗
14. The effect of grain size on the internal oxidation of Sm2Co17-type permanent magnets10.1016/j.jmmm.2022.169219 ↗
15. Thermodynamic properties of minerals and related substances at 298.15K and 1 bar
16. Effect of dry thermal oxidation on the microstructure and magnetic properties of SmCo5 permanent magnet10.1016/j.corsci.2021.109647 ↗
17. Numerical values of the surface free energies of solid chemical elements10.1007/BF00620635 ↗
18. Activities in the spinel solid solution, phase equilibria and thermodynamic properties of ternary phases in the system Cu-Fe-O10.1007/BF02696932 ↗
19. Thermodynamic assessment of the Cu-Fe-O system10.1007/s11669-011-9951-5 ↗
20. Critical assessment and thermodynamic modeling of the Cu-Fe-O system
21. Effect of oxygen partial pressure on the phase stability of copper-iron delafossites at elevated temperatures10.3390/ma11101888 ↗
22. Preparation of a new Cu-substituted cobaltite spinel: CuCo2O410.1016/0025-5408(75)90058-6 ↗
23. Cationic distribution in copper-cobalt CuXCo3−XO4 spinels prepared by low-temperature decomposition of nitrates10.1016/0025-5408(83)90223-4 ↗
24. Phase equilibria in the cobalt oxide-copper oxide system10.1361/1054971023604161 ↗
25. Callister · 2012 · 751
26. CuO surfaces and CO2 activation: a dispersion-corrected DFT+U study10.1021/acs.jpcc.5b10431 ↗
27. The thermodynamic stability of amorphous oxide overgrowths on metals10.1016/j.actamat.2007.10.023 ↗
28. Surface oxidation and reduction of CuO-Cu2O studied using XPS and XAES10.1002/(SICI)1096-9918(199611)24:12<811::AID-SIA191>3.0.CO;2-Z ↗
29. Theoretical calculation of absolute radii of atoms and ions. Part 1. The atomic radii10.3390/i3020087 ↗
30. Interionic interactions in transition metals10.1103/PhysRevB.28.4363 ↗
31. High-throughput investigation of the formation of double spinels10.1039/D0TA09200B ↗
32. Microwave-assisted route for synthesis of nanosized metal oxides10.1016/j.stam.2007.07.001 ↗
33. Rietveld structure refinement of the cation distribution in ferrite fine particles studied by X-ray powder diffraction10.1016/j.jmmm.2004.11.053 ↗
34. The role of Fe and Cu additions on the structural, thermal and magnetic properties of amorphous Al-Ce-Fe-Cu alloys10.1016/j.jnoncrysol.2018.01.003 ↗
35. R.T. Mittireddi, A. Kumawat, R.K. Singh, E. Panda, Size-dependent thermal oxidation kinetics in Sm2(Co, Fe, Cu, Zr)17 alloy powder, (2023). [Manuscript submitted].10.1016/j.corsci.2024.111932 ↗
36. Atomic-scale oxidation of a Sm2Co17-type magnet10.1016/j.actamat.2021.117343 ↗