Abstract
Abstract The damage behaviour of the TiAl alloy Ti-43.5Al-4Nb-1Mo-0.1B was investigated by isothermal thermogravimetric-analysis (TGA) and strain controlled low-cycle-fatigue (LCF) experiments at high temperature. Aluminium depletion and the formation of a continuous brittle layer in the subsurface zone takes place in synthetic exhaust gas. Contrary, a continuous ductile γ-phase forms in the subsurface zone in air. Since a continuous TiN layer as diffusion barrier is not formed in the early stages of corrosion, strong hardening is observed in LCF test samples in exhaust gas and a strain amplitude of 0,6 %, leading to a significant reduction of the cycles to failure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Design, Processing, Microstructure, Properties, and Application of Advanced Intermetallic TiAl Alloys10.1002/adem.201200231 ↗
2. Intermetallic Titanium Aluminide – An Innovative Low-weight Material for High-temperature Applications
3. Microstructural design and mechanical properties of a cast and heattreated intermetallic multi-phase γ-TiAl based alloy10.1016/j.intermet.2013.09.010 ↗
4. Intermetallic titanium aluminides in aerospace application – processing, microstructure and properties10.1080/09603409.2016.1163792 ↗
5. Thermomechanical fatigue, Oxidation, and Creep: Part I. Damage Mechanisms10.1007/BF02663207 ↗
6. Bräunling · 2009
7. Merker · 2014
8. Oxidation behaviour of TiAl-X (X=Cr, V, Si, Mo or Nb) intermetallics at elevated temperature10.1016/0956-716X(95)00327-R ↗
9. Thermal barrier coatings on γ-TiAl protected by the halogen effect10.1016/j.surfcoat.2012.09.021 ↗
10. The effect of Microstructure on the oxidation behaviour of TiAl-based intermetallics10.1016/0010-938X(93)90276-M ↗
11. The influence of cooling rate during alloy casting on the oxidation behaviour of TiAl-based intermetallics10.1007/BF00365194 ↗
12. The isothermal and cyclic high temperature oxidation behaviour of Ti-48Al-2Mn-2Nb compared with Ti-48Al-2Cr-2Nb and Ti-48Al-2Cr10.1016/S0966-9795(98)00076-4 ↗
13. The high temperature oxidation behaviour of high and low alloyed TiAl-based intermetallics10.1016/S0966-9795(01)00137-6 ↗
14. Review of the effect of alloy composition on the growth rate of scales formed during oxidation of gamma titanium aluminide alloys10.1016/S0921-5093(02)00064-3 ↗
15. Fundamentals of TiAl oxidation – A critical review10.1002/maco.19950460503 ↗
16. Microstructural Study of Oxidized γ-TiAl10.1023/A:1018892422121 ↗
17. Mechanism of Isothermal Oxidation of the Intermetallic TiAl and of TiAl Alloys
18. Influence of moisture on the oxidation of γ-TiAl10.1002/maco.19970480107 ↗
19. Influence of gaseous species on the oxidation behaviour of TiAl at high temperatures
20. Oxidation behaviour of TiAl based alloys in a simulated combustion atmosphere10.1016/j.intermet.2003.07.004 ↗
21. Correlation of high temperature oxidation with tensile properties for Ti-48Al-2Cr-2Nb and Ti-48Al-2Cr-2Fe alloys10.1016/j.intermet.2004.09.016 ↗
22. The Effect of Niobium Ion Implantation on the Oxidation Behaviour of a γ-TiAl-Based Intermetallics10.1007/BF01046882 ↗
23. Alloy Modification of γTiAl for Improved Mechanical Properties10.1016/0956-716X(94)90487-1 ↗
24. Effects of Nb addition an oxidation behaviour of TiAl10.1016/0966-9795(95)94254-C ↗
25. Effect of niobium on the oxidation behaviour of TiAl10.1557/JMR.2007.0188 ↗
26. Effect of Nb on oxidation behaviour of high Nb containing TiAl alloys10.1016/j.intermet.2010.08.029 ↗
27. High-temperature fatigue behaviour of a near- γ titanium aluminide alloy under isothermal and thermo-mechanical conditions10.1016/S0921-5093(00)02013-X ↗
28. Thermomechanical fatigue behaviour of a third generation γ-TiAl intermetallic alloy10.1016/j.intermet.2008.11.013 ↗
29. Influence of water vapour on the creep and fatigue properties of TiAl10.1016/S0966-9795(01)00105-4 ↗
30. Influence of water vapour on the oxidation behaviour of titanium aluminides10.1016/S0966-9795(01)00104-2 ↗
31. Development of a TiAl turbocharger for passenger vehicles10.1016/S0921-5093(01)01584-2 ↗
32. AMG TITANIUM ALLOYS & COATINGS, material data sheet. http://www.gfe.com/produktbereiche/titanaluminide/produktuebersicht/, 12/2017 (Accessed 13 July 19).
33. Ermittlung von anwendungsnahen Materialkennwerten am Beispiel einer TiAl-Legierung
34. Hähner · 2006
35. Oxidation behaviour of a fluorinated beta-stabilized γ-TiAl alloy with thermal barrier coatings in H2O- and SO2-contaning atmospheres10.1016/j.corsci.2014.11.045 ↗
36. The effect of nitrogen on the oxidation of γ-TiAl10.1016/0956-716X(95)00312-J ↗
37. The effect of nitrogen on the oxidation of TiAl
38. Beneficial and detrimental effects of nitrogen on the oxidation behaviour of TiAl-based intermetallics10.1002/maco.19970480106 ↗
39. Young · 2008
40. In Situ Observation of Various Phase Transformation Paths in Nb-Rich TiAl Alloys during Quenching with Different Rates10.1002/adem.201000289 ↗
41. Villars · 1985
42. Formation of Z-Ti 50Al30O20 in the suboxide zones of gamma-TiAl-based alloys during oxidation at 1000 °C10.1016/S1359-6454(99)00169-X ↗
43. Appel · 2011
44. Effect of microstructural instabillity on the creep resistance of an advanced intermetallic γ-TiAl based alloy10.1016/j.intermet.2016.09.007 ↗
45. In situ X-ray tomography investigation of the crack formation in an intermetallic beta-stabilized TiAl-alloy during a stepwise tensile loading10.1016/j.ijfatigue.2019.02.035 ↗
46. Oxidation-induced embrittlement of TiAl alloys10.1016/j.intermet.2009.01.010 ↗