Abstract

Abstract A simple stress-corrosion cracking (SCC) specimen, suitable for slow strain rate testing and incorporating heat transfer, with an artificial crevice or deposits has been designed and tested. It appears that when the solute level is above a certain value it can concentrate. The kinetics of solute accumulation and the concentration that can be induced in the specimen have been determined. Build up of solute from the ppm level in the bulk environment to the level required to cause cracking can take hours, not days or years. The limiting concentration reached is controlled by thermodynamics, specifically the available superheat. A brief review of relevant literature suggests that this experimental approach to predicting SCC has significant advantages over a modelling or measurement approach. The specimen also lends itself to a monitoring role––a modern version of the Schroeder embrittlement detector.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Thermal and Kinetic Analysis · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Corrosion and heat transfer––a review
2. Effect of concentration velocity and temperature
3. N. Thompson, J. Payer, Corrosion under heat transfer conditions, MTI Publication no 17, Columbus, 1982
4. The use of austenitic steel at the new huls power station
5. The generation of corrosive conditions in sodium heated fast steam generators
6. Influence of thermal and hydraulic circumstances on corrosion
7. A. Baum, Thermal–chemical interactions in restricted regions of steam generators, in: R.W. Lyczkowski (Ed.), Heat Transfer, AlCh E257, vol. 83, Pittsburgh, 1987
8. Distributions of NaCl and NaOH between steam and water at dryout in an experimental once-through boiler10.1016/0009-2509(75)80013-3 ↗
9. Corrosion properties of Inconel 600 under sodium phosphate treated high temperature water and corrosion resistance under AVT conditions
10. A mathematical model for localised corrosion in steam generator crevices under heat transfer conditions
11. P.J. Millet, J.M. Fenton, A detailed model of localised concentration processes in porous deposits in steam generators, in: Proceedings of the 5th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems–Water Reactors, ANES La Grange Park, 1992, pp. 745–751
12. I. Takamatsu et al., in: Proceedings of the 5th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems–Water Reactors, ANES La Grange Park, 1992, pp. 752–756
13. Inferring local chemistry from thermal hydraulic and electrochemical monitoring
14. Predicting and monitoring the possibility of stress corrosion cracking
15. Schroeder · US Bur. Mines Bull. · 1941 · 443
16. Stress corrosion cracking of type 316 stainless steel in caustic solutions: crack velocities and leak before break considerations10.1016/0010-938X(92)90032-X ↗
17. Electrochemical study of the stress corrosion of type 316 steel and Sanicro 71 in sodium hydroxide solution
18. B. Poulson, Some SCC aspects of the construction of the AGR boilers, Paper 24 Presented at Conference on Environmental Sensitive Problems in Nuclear Installations Containing High Temperature Water, Munich, 198410.1016/0010-938X(84)90062-3 ↗
19. Corrosion of PWR steam generators
20. PWR steam generators10.1016/0301-9322(95)00016-Q ↗
21. Caustic SCC studies at 288 °C using the straining electrode technique: comparisons of alloy 600 alloy 800 and type 304 stainless steel10.5006/0010-9312-34.6.198 ↗
22. Two phase flow and heat transfer
23. Collier · 1972
24. Webb · 1994
25. An experimental study of transition and film boiling heat transfer in liquid-saturated porous bed10.1115/1.3246875 ↗
26. A. Ulke, Thermal hydraulics of steam generator sludge, in: S.B. Yilmaz (Ed.), Heat Transfer––Minneapolis 1991, AlChE 283, vol. 87, 198710.2172/10192899 ↗
27. Meeting summary
28. L. Tomlinson, A.M. Pritchard, The effects of heat flux on the corrosion of high pressure boilers, Paper Presented at Symposium on Corrosion in Heat Transfer Conditions, NPL, November 1982
29. Corrosion failure: one cause and a cure in an operational boiler
30. P. Cohen, Westinghouse Electric Corp, WARD D0093, 1975
31. G.M.W. Mann, Concentration of Solute During Intermittent Wetting of a Hot Surface, CEGB CERL Research Report RD/L/N/42/77, 1977
32. G.M.W. Mann, The concentration of solutes by boiling in porous deposits, CEGB CERL Research Report RD/L/N124/75, 1975
33. Transport processes in steam generator crevices––1. General corrosion model10.1016/S0010-938X(99)00039-6 ↗
34. Transport processes in steam generator crevices 2––a simplified method for estimating impurity accumulation rates10.1016/S0010-938X(99)00040-2 ↗
35. C.B. Ashmore, M.H. Hurdus, A.P. Mead, P.J.B. Silver, L. Tomlinson, D.J. Finnigan, Accelerated corrosion of steam generator tubes by solutes concentrated in defects by boiling, Paper 80 Presented at Corrosion, 87, NACE, San Francisco
36. 2000 F.N. Speller Award Lecture: SCC in PWRs interpretation modelling and remedies10.5006/1.3280580 ↗
37. Issues in modelling of environment assisted cracking environmentally assisted cracking: predictive methods for risk assessment and evaluation of materials equipment and structures
38. R. Garnsey, F. Houghton, Deposition and corrosion studies on the foster wheeler rig, CEGB CERL Report RD/L/R1847, 1974
39. Concentration processes under tubesheet sludge piles in nuclear steam generators
40. J.B. Lumsden et al., Hideout in prototypic tube/tube support plate heated crevices, in: Proceedings of 8th International Symposium on Environmental Degradation of Materials in Nuclear Systems–Water Reactors, ANES La Grange Park, 1997
41. Localised solute enrichment and SCC in an experimental single tube steam generator
42. Chemical concentration and corrosion in PWR steam generator tubesheet crevices
43. Integrated modelling and characterisation of local crack chemistry
44. R. Pascali, G. Buzzanca, G.M. Quaglia, Stress corrosion cracking of alloy 600 in PWR steam generator tubes, Paper 239, Corrosion 86, NACE, Houston, 1986
45. W.J. Singley, I.H. Welinsky, S.F. Whirl, H.A. Klein, Stress corrosion of stainless steel and boiler water treatment at Shippingport Atomic Power Station, in: Proceedings of American Power Conference, vol. XXI, 1957, pp. 748–769
46. J.N. Wanklyn, D. Jones, The corrosion of austenitic stainless steels under heat transfer in high temperature water, AERE Report MR 2770, Harwell, 1958
47. Identifying the environment responsible for SCC of austenitic stainless steel10.1179/000705978798318756 ↗
48. Developments in nuclear power plant chemistry
49. Technical note: on ambiguities in modelling electrochemical impedance spectra using circuit analogues10.5006/1.3585234 ↗
50. Graphs in statistical analysis10.2307/2682899 ↗
51. Powell · 1954
52. Transport processes in steam generator crevices: III––experimental results10.1016/S0010-938X(01)00029-4 ↗
53. Thermal-hydraulics and electrochemistry of a boiling solution in a porous sludge pile––a test methodology
54. Experimental evaluation of tube support plate crevice chemistry
55. Progress in understanding and mitigating corrosion on the secondary side in PWR steam generators
56. Relationship between boiling regimes and chemical concentration processes in tube support plate crevices
57. On line monitoring of boiling crevice chemistry evolution