journal article·2026-09

Stiffness mismatch-induced interfacial delamination governs fretting-corrosion degradation of Cr–Mo coated Zr alloy in simulated PWR water

Jie Yang, Chenyu Wang, Yahuan Zhao, Kun Zhang, Yiheng Wu, Shuo Ma, Kun Zhang, Shixin Gao, Xiaoqing Shang, Kai Chen, Xiaoqin Zeng, Zhao Shen

Corrosion Science· Volume 270
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Mechanical stress and fatigue analysis · Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (98)

Show source-provided references
1. Materials challenges in nuclear energy
2. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
3. Corrosion of zirconium alloys used for nuclear fuel cladding10.1146/annurev-matsci-070214-020951 ↗
4. Theoretical study on loss of coolant accident of a research reactor10.1016/j.nucengdes.2016.09.016 ↗
5. Ishikawa Cardiff · 2015
6. Gauntt · Fukushima Daiichi Accid. Study · 2012
7. Overview and outcomes of the OECD/NEA benchmark study of the accident at the Fukushima Daiichi NPS (BSAF) Phase 2 – Results of severe accident analyses for Unit 110.1016/j.nucengdes.2020.110849 ↗
8. Overview and outcomes of the OECD/NEA benchmark study of the accident at the Fukushima Daiichi NPS (BSAF), Phase 2 – Results of severe accident analyses for unit 310.1016/j.nucengdes.2021.111138 ↗
9. Nuclear fuel in a reactor accident10.1126/science.1211285 ↗
10. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
11. Metrics for the technical performance evaluation of light water reactor accident-tolerant fuel10.13182/NT15-149 ↗
12. Nuclear Energy Agency · 2018
13. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: Properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
14. Research progress in FeCrAl alloys for accident-tolerant fuel cladding
15. Surface wettability and pool boiling Critical Heat Flux of Accident Tolerant Fuel cladding-FeCrAl alloys10.1016/j.nucengdes.2018.08.024 ↗
16. Early studies on Cr-Coated Zircaloy-4 as enhanced accident tolerant nuclear fuel claddings for light water reactors10.1016/j.jnucmat.2019.02.018 ↗
17. A systematic study of the oxidation behavior of Cr coatings on Zry4 substrates in high temperature steam environment10.1016/j.corsci.2020.108826 ↗
18. High temperature steam oxidation of chromium-coated zirconium-based alloys: Kinetics and process10.1016/j.corsci.2020.108537 ↗
19. H.-G. Kim, I.-H. Kim, Y.-I. Jung, D.J. Park, J.-Y. Park, Y.-H. Koo, High-temperature oxidation behavior of Cr-coated Zirconium alloy, 2013.
20. High temperature steam-oxidation behavior of arc ion plated Cr coatings for accident tolerant fuel claddings10.1016/j.surfcoat.2015.09.022 ↗
21. Oxidation behavior of Cr-coated zirconium alloy cladding in high-temperature steam above 1200 °C10.1038/s41529-021-00155-8 ↗
22. Microstructural evolution of Cr-coated Zr-4 alloy prepared by multi-arc ion plating during high temperature oxidation10.1016/j.jnucmat.2022.153616 ↗
23. Atomic-scale interface structure of a Cr-coated Zircaloy-4 material10.1007/s10853-018-2333-1 ↗
24. Interdiffusion behavior between Cr and Zr and its effect on the microcracking behavior in the Cr-coated Zr-4 alloy10.1007/s41365-021-00977-w ↗
25. Microstructural characteristics of multilayers and interfaces of Cr-coated Zircaloy-4 cladding based on elemental diffusion under high-temperature steam oxidation10.1016/j.jnucmat.2024.155113 ↗
26. Transient experiments on oxidation and degradation of Cr-coated Zircaloy in steam up to 1600 ℃10.1016/j.corsci.2021.109805 ↗
27. Microstructure evolution and interdiffusion behaviour of Cr/Mo coated Zr-4 alloys at 1330 °C-1500 °C
28. Interfacial evolution in Cr/Mo-coated Zr alloys near the Mo-Zr eutectoid temperature10.1016/j.jnucmat.2024.155406 ↗
29. Influence of a Mo interlayer on the oxidation behavior of a Cr coating on a Zr alloy substrate10.1016/j.corsci.2023.111192 ↗
30. High-temperature steam oxidation of accident-tolerant Cr/Mo-coated Zr alloy at 1200–1400 °C
31. Effect of Mo interlayer on the diffusion behavior and mechanical property of Cr-coated Zr alloy cladding tubes
32. A review of fretting study on nuclear power equipment10.1016/j.triboint.2019.106095 ↗
33. Grid-to-rod fretting in nuclear power reactors: Driving mechanisms, research methodologies and mitigation measures10.1016/j.jnucmat.2023.154705 ↗
34. Investigating grid-to-rod fretting wear of nuclear fuel claddings using a unique autoclave fretting rig10.1016/j.wear.2018.06.011 ↗
35. IAEA · 2019
36. Effect of temperature on the fretting wear behavior of Cr-coated Zircaloy cladding in high-temperature pressurized water10.1016/j.jnucmat.2023.154516 ↗
37. Autoclave grid-to-rod fretting wear evaluation of a candidate cladding coating for accident-tolerant fuel10.1016/j.wear.2020.203578 ↗
38. Tribolayer evolution and subsurface microstructural transformation in Cr-coated Zr alloy claddings under fretting corrosion in simulated PWR primary water10.1016/j.corsci.2025.113419 ↗
39. Stress analysis and probabilistic assessment of multi-layer SiC-based accident tolerant nuclear fuel cladding10.1016/j.jnucmat.2015.08.001 ↗
40. Integrating a multi-layer deformation model in FRAPTRAN for accident Tolerant fuel analysis10.1016/j.anucene.2019.05.048 ↗
41. Multi-scale design and mechanical enhancement of SiCf/SiC composite cladding for accident-tolerant fuel10.1016/j.jmrt.2025.04.130 ↗
42. W.G. Luscher, K.J. Geelhood, Material Property Correlations: Comparisons between FRAPCON-3.4, FRAPTRAN 1.4, and MATPRO, United States, United States, 2010. https://doi.org/10.2172/1030897.10.2172/1030897 ↗
43. C.J. (Colin J. Smithells, W.F. Gale, T.C. Totemeier, Smithells Metals Reference Book (8th Edition), 8th ed. / edited by W.F. Gale, T.C. Totemeier., Oxford, Oxford, 2004.
44. Microstructures and properties of Mo2N+MoS2 coatings deposited by direct current magnetron sputtering10.1016/j.vacuum.2020.109406 ↗
45. Probabilistic prediction of fretting-wear damage of nuclear fuel rods
46. Y.K. Jang, J.K. Kang, J.H. Choi, Y.H. Kim, K.T. Kim KEPCO N.F.C. Taejon (Korea, Republic of), K.Z. Cho Chonnam N.U. Gwangju (Korea, Republic of), An experimental study on the vibrations and grid-to-rod fretting wear in PWR fuel, in: KNS, Taejon (Korea, Republic of), Korean Nuclear Society, Taejon (Korea, Republic of), 2003.
47. Grid-to-rod flow-induced impact study for PWR fuel in reactor10.1016/j.pnucene.2016.06.003 ↗
48. 〈a〉 Prismatic, 〈a〉 basal, and 〈c+a〉 slip strengths of commercially pure Zr by micro-cantilever tests10.1016/j.actamat.2015.06.020 ↗
49. A dislocation-based constitutive law for pure Zr including temperature effects10.1016/j.ijplas.2007.07.017 ↗
50. Single-Crystal Elastic Moduli and the hcp-bcc Transformation in Ti, Zr, and Hf10.1103/PhysRev.135.A482 ↗
51. A comparison of the elastic constants of chromium as determined from diffuse X-ray and ultrasonic techniques10.1063/1.1729792 ↗
52. Elastic constants of tantalum, tungsten, and molybdenum10.1103/PhysRev.130.1324 ↗
53. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
54. Investigating a tribological failure10.1016/0043-1648(90)90080-T ↗
55. On the nature of running-in10.1016/j.triboint.2005.07.020 ↗
56. Fretting wear damage of the corroded fuel cladding tubes for nuclear fuel rod against supporting grids
57. The impact fretting corrosion behavior and damage mechanism of Inconel 690TT under different impact forces in high temperature pressurized water10.1016/j.corsci.2024.112507 ↗
58. Characterization of zirconium hydrides in Zircaloy-4 cladding with respect to cooling rate10.1016/j.jnucmat.2015.07.006 ↗
59. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
60. High temperature corrosion((Book))
61. Autoclave grid-to-rod fretting corrosion behaviors of the Zr alloy fuel cladding with and without Cr coating through advanced characterization10.1016/j.corsci.2024.112379 ↗
62. Triboelectrochemical techniques and interpretation methods in tribocorrosion: A comparative evaluation10.1016/j.triboint.2007.11.003 ↗
63. Review on chromium coated zirconium alloy accident tolerant fuel cladding10.1016/j.jallcom.2021.162450 ↗
64. Diffusivity and permeability of hydrogen in molybdenum10.1016/0022-3697(82)90104-4 ↗
65. Bowden · 2001
66. Cracking and spalling of the oxide layer developed in high-burnup Zircaloy-4 cladding under normal operating conditions in a PWR10.1016/j.jnucmat.2018.10.003 ↗
67. Transformations and cracks in zirconia films leading to breakaway oxidation of Zircaloy10.1016/j.actamat.2013.02.052 ↗
68. Evolution of fretting wear behavior of zirconium alloy cladding tube under gross slip regime in simulated primary water of pressurized water reactor10.1016/j.jmst.2024.09.022 ↗
69. MATPRO-Version 11: a handbook of materials properties for use in the analysis of light water reactor fuel rod behavior
70. Stress analysis of elastic-plastic contact damage in ceramic coatings on metal substrates10.1111/j.1151-2916.1996.tb09024.x ↗
71. Hard coatings on soft metallic substrates
72. Mechanical property and cracking mechanism of Cr-coated Zr alloy under tensile and compressive loading
73. Fracture modes in brittle coatings with large interlayer modulus mismatch10.1557/JMR.1999.0514 ↗
74. An overview of interface-dominated deformation mechanisms in metallic multilayers10.1016/j.cossms.2010.09.002 ↗
75. Mechanical properties of thin films10.1007/BF02666659 ↗
76. Length-scale-dependent deformation mechanisms in incoherent metallic multilayered composites10.1016/j.actamat.2005.06.025 ↗
77. Brewer · 2009 · 251
78. Stress in thin films and coatings: current status, challenges, and prospects10.1116/1.5011790 ↗
79. On the significance of the H/ E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
80. Mixed mode cracking in layered materials10.1016/S0065-2156(08)70164-9 ↗
81. An energy description of hard coating wear mechanisms10.1016/S0257-8972(00)01161-0 ↗
82. The significance and use of the friction coefficient10.1016/S0301-679X(01)00050-0 ↗
83. Application of an energy wear approach to quantify fretting contact durability: Introduction of a wear energy capacity concept10.1016/j.triboint.2007.02.011 ↗
84. On the mechanisms of various fretting wear modes10.1016/j.triboint.2011.02.010 ↗
85. Instabilities and ductility of nanocrystalline and ultrafine-grained metals, Viewp. Set No 31 Mech. Prop. Fully Dense Nanocrystalline Met10.1016/S1359-6462(03)00396-8 ↗
86. Mechanical behavior of nanocrystalline metals and alloys11The Golden Jubilee Issue—Selected topics in Materials Science and Engineering: Past, Present and Future, edited by S. Suresh
87. Effect of the cycle number on fretting wear behavior of alloy 690TT tube in high-temperature pressurized water10.1016/j.jnucmat.2022.153828 ↗
88. Mechanistic understanding on the fatigue cracking in fretting corrosion of alloy 690TT under partial slip regime in 100 ℃ and 290 ℃ water10.1016/j.corsci.2023.111655 ↗
89. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
90. Intrinsic stress in sputter-deposited thin films10.1080/10408439208244586 ↗
91. C. Wang, Q. Zhao, Y. Zhou, D. Wang, L. Wang, M. Abdel Wahab, Fretting fatigue crack initiation and propagation behaviours of Ti6Al4V alloy coated by functionally graded material, (2024).10.1016/j.compstruct.2024.118285 ↗
92. Estimating life scatter in fretting fatigue crack initiation10.1080/10402004.2013.766829 ↗
93. Fretting corrosion behavior and microstructure evolution of hydrided zirconium alloy under gross slip regime in high temperature high pressure water environment10.1016/j.corsci.2024.112582 ↗
94. Study on the fretting corrosion behavior of zirconium alloy in simulated primary coolant condition10.1016/j.wear.2025.206057 ↗
95. Suppression of Dynamic Recovery via Localized Solute Pinning for Superior High Temperature Strength in a Lightweight Refractory Medium-Entropy Alloy10.1016/j.actamat.2026.122459 ↗
96. Y. Wang X. Chen X. Wang C. Tang Z. Shen X. Zeng Progress in failure mechanisms and modification strategies of nickel-based alloys for molten salt reactors Acta Metall. Sin. doi: 10.11900/0412.1961.2025.00407.
97. Sequential δ/γ Interfacial Degradation Induces a Sigmoidal Kinetic Transition in Stress Corrosion Cracking during Superlong-Term Thermal Aging of Duplex Stainless Steel10.1016/j.actamat.2026.122314 ↗
98. Microstructure-Dependent Volatilization of Haynes 230 Alloy in Ultrahigh Vacuum at High Temperatures10.1016/j.corsci.2026.113821 ↗