Subsurface microstructural changes of alloy 625 related to oxidation at 900 °C in lab air and humid air

B. Jacquard, S. Mathieu, G. Steciuk, S. Migot, D. Bonina, T. Perez, E. Epifano, D. Monceau, A. Vande Put

Corrosion Science· Volume 267

Abstract

Alloy 625 was oxidized at 900 °C in lab air and in air + 20%vol. H 2 O for 400 h to estimate the microstructural changes experienced by the alloy during exposure at high temperature. The specimen mass loss in air + 20%vol. H 2 O evolved linearly after a very short period of exposure due to the formation of volatile species from the protective Cr 2 O 3 layer. The chromium loss rate was in the order of 5.5 × 10 −7 mg.cm -2 .s -1 (evaluated by direct mass variation measurements) and 7.5 × 10 −7 mg.cm -2 .s -1 (evaluated from Cr-mass balance) in air + 20%vol. H 2 O in the present conditions. Pronounced chemical and microstructural changes were observed in the subsurface for samples exposed in air + 20%vol. H2O. The recession of the alloy interface due to chromium removal was insufficient to explain the pronounced accumulation of δ-Ni 3 (Nb,Mo) phase at the alloy-oxide interface, demonstrating the significant uphill diffusion of Nb. Chemical breakaway on the sample edges involved the oxidation of δ-Ni 3 (Nb,Mo) phase, forming powdery oxides.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. J.B. Singh, Alloy 625: Microstructure, Properties and Performance, 2022 - Springer.10.1007/978-981-19-1562-8 ↗
2. Oxidation behavior of superalloys in oxidizing and reducing environments10.1016/S0010-938X(00)00011-1 ↗
3. Oxidation of Ni-Cr alloy at intermediate oxygen pressures. I. Diffusion mechanisms through the oxide layer10.1016/j.corsci.2016.05.025 ↗
4. Corrosion resistance of 625 nickel superalloy exposed to isothermal and thermal cycling conditions in a chloride/carbonate salt10.1016/j.solener.2022.11.034 ↗
5. A history of superalloy metallurgy for superalloy metallurgists
6. A review on additive manufacturing processes of inconel 62510.1007/s11665-021-06427-3 ↗
7. Microstructures and mechanical behaviors of additive manufactured Inconel 625 alloys via selective laser melting and laser engineered net shaping10.1016/j.jallcom.2022.165572 ↗
8. A critical review on the microstructure and mechanical properties correlation of additively manufactured nickel-based superalloys10.1016/j.jallcom.2022.164530 ↗
9. Oxidation in water vapor of inconel 625 fabricated by additive manufacturing10.1007/s11085-023-10205-y ↗
10. A comparison of the high-temperature oxidation behaviour of conventional wrought and laser beam melted Inconel 62510.1016/j.corsci.2019.108347 ↗
11. High-temperature oxidation behavior of additively manufactured IN625: effect of microstructure and grain size10.1016/j.corsci.2022.110382 ↗
12. S. Floreen, G.E. Fuchs, W.J. Wang, The Metallurgy of 625, Superalloys 718, 625, 706 and Various Derivatives, Warrendale, E.A. Loria (Ed.),TMS, vol.625, (1994) 13-37.10.7449/1994/Superalloys_1994_13_37 ↗
13. Microstructural evolutions during thermal aging of Alloy 625: impact of temperature and forming process10.1007/s11661-014-2256-7 ↗
14. A comparison of the precipitation kinetics of γ’’ particles in virgin and re-solutioned Alloy 625
15. W.J. Quaddakers, Oxidation behaviour and microstructural stability of alloy 625 during long-term exposure in steam10.1007/s10853-014-8344-7 ↗
16. Intergranular oxidation of additively manufactured Ni-base alloy 625: The role of Si10.1016/j.corsci.2023.111234 ↗
17. Microstructural evolution of Inconel 625 during thermal aging
18. Put, Fluid dynamic simulation of CrO2(OH)2 volatilization and gas phase evolution during the oxidation of a chromia forming alloy10.1016/j.corsci.2022.110306 ↗
19. Oxidation Lifetime Modeling of 625 and 120 Foils After Long-term Exposure in Flowing Air+10% H2O at 700 and 800 °C10.1007/s11085-022-10124-4 ↗
20. Effect of Temperature and Water Content on the Oxidation Behaviour and Cr Evaporation of High‑Cr Alloys for SOFC Cathode Air Preheaters10.1007/s11085-023-10167-1 ↗
21. Inconel 625 oxidation in CO2: Kinetics and reaction mechanism10.1016/j.corsci.2023.111101 ↗
22. Sub-Scale Depletion and Enrichment Processes During High Temperature Oxidation of the Nickel Base Alloy 625 in the Temperature Range 900–1000 °C10.1007/s11085-010-9225-3 ↗
23. Utilization of Alumina Scale Formation by Ni-base Alloys for High Temperature Oxidation and Corrosion Resistance in Harsh Environments10.1007/s11085-024-10280-9 ↗
24. Mechanism of high temperature oxidation of Inconel 625 superalloy with various solution and ageing heat treatment processes10.1016/S1003-6326(24)66632-X ↗
25. Effect of Manganese Additions on the Reactive Evaporation of Chromium in Ni-Cr Alloys10.1016/j.scriptamat.2006.01.026 ↗
26. Chromia Evaporation in Advanced Ultra-Supercritical Steam Boilers and Turbines in Thermodynamics
27. Chromium volatilization rates from Cr2O3 scales into flowing Gases containing water vapor10.1007/s11085-006-9030-1 ↗
28. Calculation of reactive-evaporation Rates of Chromia10.1007/s11085-008-9091-4 ↗
29. Theoretical and experimental investigation of the thermochemistry of CrO2(OH)2 (g). The10.1021/jp0647380 ↗
30. Effect of gas flow rate on oxidation behaviour of alloy 625 in wet air in the temperature range 900-1000 °C10.1002/maco.201608831 ↗
31. Influence of water vapor and local gas velocity on the oxidation kinetics of In625 at 900 °C: experimental study and CFD gas phase simulation10.1007/s11085-024-10307-1 ↗
32. Coated interconnects development for high temperature water vapour electrolysis: Study in anode atmosphere10.1016/j.ijhydene.2013.10.026 ↗
33. Chromium deposition and poisoning of cathodes of solid oxide fuel cells – A review10.1016/j.ijhydene.2013.10.042 ↗
34. Experimental review of the performances of protective coatings for interconnects in solid oxide fuel cells10.1016/j.jpowsour.2023.232831 ↗
35. Beitrag zur theorie des anlaufvorgangs10.1515/zpch-1933-2105 ↗
36. Ellingham diagram: A new look at an old tool10.1016/j.corsci.2023.111113 ↗
37. D.J. Young, High temperature oxidation and corrosion of materials, Elsevier Corrosion Series (2008).
38. Uphill diffusion in single and multi-species systems10.1088/1751-8121/acef0b ↗
39. High temperature oxidation of IN 718 manufactured by laser beam melting and electron beam melting: Effect of surface topography10.1016/j.corsci.2018.07.005 ↗
40. Characterization and oxidation resistance of additive manufactured and forged IN718 Ni-based superalloys10.1016/j.corsci.2018.07.032 ↗
41. High-temperature oxidation performance of Inconel 625 superalloy fabricated by wire arc additive manufacturing10.1016/j.corsci.2022.110087 ↗
42. The role of Ta in the microstructure evolution and high-temperature oxidation behavior of Inconel 625 superalloy fabricated by directed energy deposition10.1016/j.matchar.2025.115409 ↗
43. 3D Electron Diffraction: The Nanocrystallography Revolution10.1021/acscentsci.9b00394 ↗
44. 3D electron diffraction techniques. Acta Crystallographica Section B: Structural Science
45. Specifics of the Data Processing of Precession Electron Diffraction Tomography Data and Their Implementation in the Program PETS2.010.1107/S2052520619007534 ↗
46. Accurate lattice parameters from 3D electron diffraction data. I. optical distortions10.1107/S2052252522007904 ↗
47. Optimal estimated standard uncertainties of reflection intensities for kinematical refinement from 3D electron diffraction data
48. SUPERFLIP - a computer program for the solution of crystal structures by charge flipping in arbitrary dimensions10.1107/S0021889807029238 ↗
49. The charge-flipping algorithm in crystallography10.1107/S2052519212051366 ↗
50. Jana2020, a new version of the crystallographic computing system
51. Structure refinement using precession electron diffraction tomography and dynamical diffraction: theory and implementation10.1107/S2053273315001266 ↗
52. Structure refinement using precession electron diffraction tomography and dynamical diffraction: tests on experimental data10.1107/S2052520615017023 ↗
53. Casino software. 〈https://casino.espaceweb.usherbrooke.ca/〉.
54. Isothermal oxidation of Inconel 625 superalloy at 800 and 1000 °C: Microstructure and oxide layer characterization
55. Microstructure and mechanical properties of Inconel 625 Superalloy10.1016/S0022-3115(00)00723-6 ↗
56. The crystal structure of the R phase, Mo-Co-Cr10.1107/S0365110X60001394 ↗
57. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
58. Depletion and voids formation in the substrate during high temperature oxidation of Ni-Cr alloys10.1007/s11085-012-9328-0 ↗
59. Oxidation of additively manufactured Ni-base alloy IN625: Mechanism of intergranular oxidation10.1016/j.corsci.2025.113218 ↗
60. Alloy chemistry of σ (β-U)-related phases. II. the characteristics of δ and other σ-related phases in some Mo-NiX systems
61. The oxidation of metals at high temperatures
62. Volatilization behavior of high-purity MoO3 in the range of 600 °C to 750 °C: influences of water-vapor concentration and reaction temperature10.1016/j.ijrmhm.2025.107264 ↗