journal article·2026-02

The role of pre-strain on hydrogen embrittlement of 20# steel exposed to medium-pressure gaseous hydrogen

Jianwei Du, Chan Yao, Hongliang Ming, Jianqiu Wang, Chen Wang, En-Hou Han

Corrosion Science· Volume 259
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (84)

Show source-provided references
1. W.C. Leight, J. Holloway, R. Merer, B. Somerday, D.E. White, 2006, Compressorless hydrogen transmission pipelines deliver large-scale stranded renewable energy at competitive cost.
2. A coupled diffusion and cohesive zone modelling approach for numerically assessing hydrogen embrittlement of steel structures10.1016/j.ijhydene.2017.02.211 ↗
3. Effect of hydrogen gas impurities on the hydrogen dissociation on iron surface10.1002/qua.24633 ↗
4. Hydrogen diffusion and trapping in metals
5. Perspectives on hydrogen uptake, diffusion and trapping10.1016/j.ijhydene.2015.06.147 ↗
6. A visible technology for display of hydrogen distribution in metals10.1016/S0925-8388(99)00371-0 ↗
7. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
8. Prediction of threshold stress intensity factor for hydrogen induced intergranular cracking of tubular steel10.1016/S0921-5093(99)00444-X ↗
9. J. Venezuela, Q. Liu, M. Zhang, Q. Zhou, A.J.C.S. Atrens, The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test, 99 (2015) 98-117.10.1016/j.corsci.2015.06.038 ↗
10. S.J.C.R. Lynch, Hydrogen embrittlement phenomena and mechanisms, 30 (2012) 105-123.10.1515/corrrev-2012-0502 ↗
11. M. Koyama, C.C. Tasan, E. Akiyama, K. Tsuzaki, D.J.A.M. Raabe, 2014, Hydrogen-assisted decohesion and localized plasticity in dual-phase steel, 70 174-187.10.1016/j.actamat.2014.01.048 ↗
12. Comparison of tensile properties of X60 pipeline steel tested in high pressure gaseous hydrogen using tubular and conventional specimen10.1016/j.ijhydene.2022.07.211 ↗
13. Effect of gaseous hydrogen charging on the tensile properties of standard and medium MnX70 pipeline steels10.1080/02670836.2015.1130331 ↗
14. Microstructure-dependent hydrogen diffusion and trapping in high-tensile steel
15. Effect of bainitic microstructure on the susceptibility of pipeline steels to hydrogen induced cracking10.1016/j.msea.2011.03.036 ↗
16. Competitive role of film-like austenite and transition carbides on hydrogen embrittlement resistance and impact toughness in bainite-containing quenched and partitioned steel10.1007/s42243-023-00939-z ↗
17. Effect of retained austenite stability and morphology on the hydrogen embrittlement susceptibility in quenching and partitioning treated steels10.1016/j.msea.2016.02.026 ↗
18. Effect of retained austenite on the hydrogen embrittlement of a medium carbon quenching and partitioning steel with refined microstructure10.1016/j.msea.2016.04.025 ↗
19. Quantification of hydrogen trapping in multiphase steels: Part II - Effect of austenite morphology10.1016/j.actamat.2020.07.039 ↗
20. Effect of microstructure on hydrogen embrittlement and hydrogen-induced cracking behaviour of a high-strength pipeline steel weldment10.1016/j.corsci.2023.111764 ↗
21. Effect of d-ferrite in welded ER308 and ER316 microstructure on hydrogen embrittlement10.1016/j.ijhydene.2023.01.025 ↗
22. Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments10.1016/j.corsci.2012.01.028 ↗
23. Study on hydrogen embrittlement susceptibility of X80 steel through in-situ gaseous hydrogen permeation and slow strain rate tensile tests10.1016/j.ijhydene.2022.09.228 ↗
24. Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: Effect of plastic pre-strain10.1016/j.ijhydene.2014.04.122 ↗
25. Li · Eff. prestrain Hydrog. embrittlement High. Strength Steels · 2014 · 616 · 116
26. Hydrogen embrittlement sensitivity of X100 pipeline steel under different pre-strain10.1016/j.ijhydene.2019.06.054 ↗
27. Hydrogen embrittlement in vintage grade 290 pipeline steel and its welded region via ex-situ and in-situ testing10.1016/j.engfailanal.2025.109410 ↗
28. Hydrogen-assisted fatigue crack growth: Pre-charging vs in-situ testing in gaseous environments
29. Atomistic study of hydrogen diffusion in presence of defects in bcc and fcc iron10.1016/j.commatsci.2023.112433 ↗
30. First-Principles Study on Hydrogen Diffusivity in BCC, FCC, and HCP Iron10.1007/s11661-018-4815-9 ↗
31. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
32. Investigation of hydrogen concentration and hydrogen damage on API X80 steel surface under cathodic overprotection10.1016/j.ijhydene.2017.10.116 ↗
33. Improving the hydrogen embrittlement resistance by straining the ferrite / cementite interfaces10.1016/j.actamat.2024.119850 ↗
34. Role of deformation on the hydrogen trapping in the pearlitic steel10.1016/j.scriptamat.2023.115859 ↗
35. Effect of cold deformation on the hydrogen permeation in a dual-phase advanced high-strength steel10.1016/j.electacta.2022.140619 ↗
36. Pre-strain effects on critical stress and hydrogen content for hydrogen-induced quasi-cleavage fracture in a TRIP-aided bainitic ferrite steel: Martensitic transformation, matrix damage, and strain aging10.1016/j.ijhydene.2020.07.036 ↗
37. Lee · Correl. prestrain Hydrog. embrittlement Behav. MediumMn Steel · 2025 · 206 · 62
38. Evaluation of hydrogen embrittlement by Internal high-pressure hydrogen environment in specimen
39. Influence of high pressure hydrogen environment on tensile and fatigue properties of stainless steels at low temperatures10.1063/1.4712078 ↗
40. Effect of high-pressure H2 gas on tensile and fatigue properties of stainless steel SUS316L by means of the internal high-pressure H2 gas method10.1016/j.prostr.2019.12.053 ↗
41. Hydrogen embrittlement of 20# seamless steel in medium and low pressure gaseous hydrogen10.1016/j.matlet.2022.133734 ↗
42. Effect of Cold Deformation on the Hydrogen Permeation Behavior of X65 Pipeline Steel10.3390/coatings13020280 ↗
43. Slow strain rate tensile and fatigue properties of Cr-Mo and carbon steels in a 115 MPa hydrogen gas atmosphere10.1016/j.ijhydene.2015.02.098 ↗
44. Hydrogen diffusivity and tensile-ductility loss of solution-treated austenitic stainless steels with external and internal hydrogen10.1016/j.ijhydene.2017.04.055 ↗
45. Effect of highly pressurized hydrogen gas charging on the hydrogen embrittlement of API X70 steel10.1007/s12540-014-4010-5 ↗
46. Hydrogen embrittlement behavior at different strain rates in low-carbon martensitic steel
47. In situ observations of silver-decoration evolution under hydrogen permeation: Effects of grain boundary misorientation on hydrogen flux in pure iron10.1016/j.scriptamat.2016.10.027 ↗
48. Experimental study on slow tensile, fatigue, and impact on X42 steel and #20 carburizing steel10.1016/j.ijpvp.2024.105139 ↗
49. W.J. Hui, Y. Li, Y.J. Zhang, C. Zhou, H.J.To.M. Dong, H. Treatment, 2012, Effect of prestraining on hydrogen absorption and delayed fracture behavior of a medium-carbon TRIP steel, 33 (2012) 42-46.
50. Hydrogen embrittlement of ferrite-pearlite OCTG steels under electrochemical and gaseous hydrogen environment10.1016/j.jmrt.2025.07.076 ↗
51. In-situ EBSD study of deformation behaviour of 600 MPa grade dual phase steel during uniaxial tensile tests10.1016/j.msea.2019.05.083 ↗
52. Quantitative phase analysis of martensite-bainite steel using EBSD and its microstructure, tensile and high-cycle fatigue behaviors
53. Effects of temperature and load on fretting fatigue induced geometrically necessary dislocation distribution in titanium alloy
54. Microstructure and texture evolution during annealing a cryogenic-SPD processed Al-alloy with a nanoscale lamellar HAGB grain structure10.1016/j.actamat.2009.04.010 ↗
55. Investigating the influence mechanism of hydrogen partial pressure on fracture toughness and fatigue life by in-situ hydrogen permeation10.1016/j.ijhydene.2021.03.183 ↗
56. Pre-strain and hydrogen charging effect on the plastic and fracture behavior of quenching and partitioning (Q&P) steel10.1016/j.actamat.2023.119524 ↗
57. Effect of cold deformation on the hydrogen permeation behavior of X65 pipeline steel
58. Observation of local hydrogen on nickel surfaces10.1007/BF02663321 ↗
59. Detection of hydrogen permeation on the microscopic scale in nickel10.1016/S0036-9748(88)80176-5 ↗
60. A.R. Cottis, 2010, Shreir\"s Corrosion || Hydrogen Embrittlement, (2010) 902-922.10.1016/B978-044452787-5.00200-6 ↗
61. Hydrogen detrapping from grain-boundaries and dislocations in high-purity iron10.1016/0956-7151(92)90436-I ↗
62. Hydrogen induced cracking susceptibility in different layers of a hot rolled X70 pipeline steel10.1016/j.ijhydene.2013.08.046 ↗
63. Deep trapping states for hydrogen in deformed iron10.1016/0001-6160(80)90038-3 ↗
64. Hydrogen induced cracking of pipeline and pressure vessel steels: a review10.1016/j.engfracmech.2018.06.018 ↗
65. Hydrogen-induced degradation of high-strength steel pipeline welds: a critical review
66. Effect of stress and strain on hydrogen permeation process in X80 pipeline steel10.1016/j.corsci.2025.112934 ↗
67. Hydrogen effects in prestrained transformation induced plasticity steel10.1007/s11661-011-1075-3 ↗
68. Hydrogen embrittlement of X80 pipeline steel in H2S environment: effect of hydrogen charging time, hydrogen-trapped state and hydrogen charging-releasing-recharging cycles10.1007/s12613-019-1870-1 ↗
69. Slow strain rate technique for studying hydrogen induced cracking in 34CrMo4 high strength steel, Int. J. Hydrog
70. Enhanced hydrogen embrittlement of low-carbon steel to natural gas/hydrogen mixtures10.1016/j.scriptamat.2020.08.011 ↗
71. Hydrogen embrittlement mechanisms in advanced high strength steel10.1016/j.actamat.2021.117488 ↗
72. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
73. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
74. Hydrogen Embrittlement of Steels
75. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
76. Determination of the critical hydrogen concentration for delayed fracture of high strength steel by constant load test and numerical calculation10.1016/j.corsci.2005.07.010 ↗
77. In-situ measurement of hydrogen entry and hydrogen embrittlement of steel by atmospheric corrosion10.1016/j.corsci.2023.111212 ↗
78. Effect of ferrite on the hydrogen embrittlement in quenched-partitioned-tempered low carbon steel10.1016/j.msea.2017.12.032 ↗
79. Origin of tearing topography surface in hydrogen-charged pearlitic steel10.1016/j.actamat.2023.119116 ↗
80. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
81. Influence of hydrogen-enhanced plasticity and decohesion mechanisms of hydrogen embrittlement on the fracture resistance of steel10.1016/j.engfailanal.2021.105312 ↗
82. Effect of bainitic microstructure on hydrogen trapping in a low carbon micro-alloyed pipeline steel10.1016/j.ijhydene.2024.06.006 ↗
83. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
84. Investigation of quasi-cleavage in a hydrogen charged maraging stainless steel10.1016/j.corsci.2023.111163 ↗