Comparative study of the hydrogen-assisted cracking behavior in AISI 420 martensitic stainless steel under different heat treatments
Source abstract
Abstract
This study compares the hydrogen-assisted cracking behavior of AISI 420 martensitic stainless steel subjected to different heat treatments and clarifies the effect of key microstructural factors, including carbides, ferrite, and residual stress. The sample treated with the quenching-ferrite/martensite duplex tempering- tempering (QDT) process exhibits the highest resistance to hydrogen embrittlement (HE), mainly attributed to its minimal microscopic residual stress and the largest amount of fine Cr₂₃C₆ carbides. Secondary cracks preferentially propagate along banded ferrite/martensite boundaries but are deflected by small ferrite particles. For the quenched sample, the fracture exhibits the intergranular cracking morphology and the dominant HE mechanism is the hydrogen-enhanced decohesion (HEDE) mechanism. For the QDT sample, the HE mechanism under the pre-charging condition is the hydrogen-enhanced plasticity (HELP) mechanism, while it transitions to the HELP mediated HEDE mechanism under the in-situ charging condition.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (79)
Show source-provided references
1. Failure Study of 420 martensitic stainless steel needle holder with Cr Coating10.1007/s11668-024-02077-4 ↗
2. Case Studies of Steel Component Failures in Aerospace Applications
3. Surgical tool failure analyses10.1007/s11668-013-9763-5 ↗
4. Failure analysis of a high-pressure component10.1007/s11668-009-9246-x ↗
5. Experimental and modelling study of the effect of tempering on the susceptibility to environment-assisted cracking of AISI 420 martensitic stainless steel10.1016/j.corsci.2018.12.010 ↗
6. Influence of hydrogen on mechanical properties and fracture of tempered 13wt% Cr martensitic stainless steel10.1016/j.msea.2017.05.086 ↗
7. The effect of precipitations (NbC and carbide) in Fe–C–Mn-xNb steels on hydrogen embrittlement characteristics10.1016/j.msea.2020.139598 ↗
8. Influence of residual stresses on the hydrogen embrittlement of high-strength cold-drawn eutectoid pearlitic steel wires10.1016/j.prostr.2024.04.030 ↗
9. Balancing strength and toughness by QLT process in a low-Ni heavy steel plate with GPa grade10.1016/j.msea.2024.146748 ↗
10. Influence of heat treatments on the susceptibility of 9%Ni low carbon steel to sulfide stress corrosion cracking10.1016/j.engfailanal.2020.104554 ↗
11. The role of reverted transformation in hydrogen embrittlement of a Cu-containing low carbon high strength steel10.1016/j.jmrt.2023.07.071 ↗
12. The influence of precipitated austenite on hydrogen embrittlement in 5.5Ni steel10.1007/BF02665314 ↗
13. Effects of the microstructure and reversed austenite on the hydrogen embrittlement susceptibility of Ni-Cr-Mo-V/Nb high-strength steel10.1016/j.corsci.2023.111164 ↗
14. Effect of microstructure on the hydrogen embrittlement, diffusion, and uptake of dual-phase low alloy steels with varying ferrite-martensite ratios10.1016/j.ijhydene.2023.07.061 ↗
15. The role of delta ferrite in hydrogen embrittlement fracture of 17-4 PH stainless steel10.1016/j.ijhydene.2022.07.257 ↗
16. The role of retained austenite in hydrogen embrittlement of supermartensitic stainless steel10.1016/j.engfailanal.2013.07.025 ↗
17. Control of the concentrated-precipitation behaviour of Cr23C6 and its effect on the microstructure and properties of S600E sorbitic stainless steel10.1016/j.jmrt.2024.11.085 ↗
18. Influence of Thermomechanical Treatment on Delayed Fracture Property of Mo-Bearing Medium-Carbon Steel10.2355/isijinternational.ISIJINT-2021-407 ↗
19. Mechanism and prediction of hydrogen embrittlement based on complex phase structure of chromium alloy steel10.1016/j.msea.2021.141546 ↗
20. Comparison of crack initiation sites and main factors causing hydrogen embrittlement of tempered martensitic steels with different carbide precipitation states10.2355/isijinternational.ISIJINT-2023-026 ↗
21. Influence of tempering treatments on mechanical properties and hydrogen embrittlement of 13 wt% Cr martensitic stainless steel10.1016/j.ijpvp.2019.103969 ↗
22. Effect of Residual Stress and Strain-Induced α′-Martensite on Delayed Cracking of Metastable Austenitic Stainless Steels10.1007/s11661-013-2090-3 ↗
23. Effects of residual stress and plastic strain on hydrogen embrittlement of a stretch-formed TRIP-aided martensitic steel sheet10.1016/j.corsci.2020.108957 ↗
24. Determination of macroscopic and microscopic residual stresses in friction stir welded metal matrix composites via neutron diffraction10.1016/j.actamat.2015.01.006 ↗
25. Effects of hydrogen on the evolution of 4130 steel microstructure as a result of tensile loading10.1016/j.ijhydene.2024.07.051 ↗
26. Computational investigation into XRD peak broadening effects with discrete dislocation dynamics in additively manufactured 316L stainless steel10.1016/j.jmps.2024.105970 ↗
27. Residual stress analysis in industrial parts: a comprehensive comparison of XRD methods10.1007/s10853-023-09069-z ↗
28. Elastic constants and internal friction of martensitic steel, ferritic-pearlitic steel, and α-iron10.1016/j.msea.2006.11.147 ↗
29. Effect of the pre-strain on the elastic behavior of a dual-phase steel with different martensite contents10.4028/www.scientific.net/MSF.1016.1555 ↗
30. Elastic anisotropy of dual-phase steels with varying martensite content10.1016/j.ijsolstr.2018.02.028 ↗
31. Dislocation density measurements from x-ray diffraction of austenite and ferrite phases in superduplex UNS S39274
32. Huang · A Method Calc. Dislocation Density A TWIP Steel Based Neutron Diffr. Synchrotron XRay Diffr. · 2020 · 56 · 487
33. Hydrogen embrittlement and strain rate sensitivity of electrodeposited copper: part I – the effect of hydrogen content10.1038/s41529-024-00498-y ↗
34. Temperature mitigates the hydrogen embrittlement sensitivity of martensitic steels in slow strain rates10.1016/j.vacuum.2022.111187 ↗
35. The influence of steelmaking processes on the hydrogen embrittlement of a tempered martensitic steel10.1016/j.ijhydene.2024.06.251 ↗
36. Improving the hydrogen embrittlement resistance by straining the ferrite / cementite interfaces10.1016/j.actamat.2024.119850 ↗
37. The influence of the experimental methodology on evaluating the hydrogen embrittlement susceptibility of AISI 4340 steel manufactured by different routes10.1016/j.engfailanal.2024.108361 ↗
38. Qualification of the in-situ bending technique towards the evaluation of the hydrogen induced fracture mechanism of martensitic Fe–C steels10.1016/j.msea.2020.139754 ↗
39. Hydrogen-assisted cracking (HAC) of high-strength steels as a function of the hydrogen pre-charging time10.1016/j.engfracmech.2022.108246 ↗
40. Notch tensile behavior of 304L and 316L stainless steels under in-situ and ex-situ electrochemical hydrogen charging10.1016/j.jmrt.2025.05.132 ↗
41. Investigation of hydrogen embrittlement behavior in X65 pipeline steel under different hydrogen charging conditions10.1016/j.msea.2022.144262 ↗
42. Tecnology, Thermal analysis on hydrogen charged annealed and hardened AISI 420 stainless steel
43. Effect of strain rate on hydrogen embrittlement in low-carbon martensitic steel10.1016/j.ijhydene.2016.09.188 ↗
44. Research on hydrogen embrittlement behavior of L-PBF 18Ni(300) maraging steel by experiments and numerical simulations10.1016/j.actamat.2023.119141 ↗
45. Deformation and fracture mechanisms in fine- and ultrafine-grained ferrite/martensite dual-phase steels and the effect of aging10.1016/j.actamat.2010.10.002 ↗
46. Understanding ferrite deformation caused by austenite to martensite transformation in dual phase steels10.1016/j.scriptamat.2021.114032 ↗
47. Measurement and simulation of thermal-induced residual stresses within friction stir lapped Al/steel plate10.1016/j.jmatprotec.2022.117760 ↗
48. Elastic Properties of Fe–C and Fe–N Martensites10.2355/isijinternational.55.1512 ↗
49. Effects of hydrogen pressure and prior austenite grain size on the hydrogen embrittlement characteristics of a press-hardened martensitic steel10.1016/j.ijhydene.2021.05.005 ↗
50. Investigation on hydrogen embrittlement susceptibility in martensitic steels with 1000 MPa yield strength10.1016/j.jmrt.2021.11.130 ↗
51. Design of high-strength martensitic steels by novel mixed-metal nanoprecipitates for high toughness and suppressed hydrogen embrittlement10.1016/j.matdes.2023.112323 ↗
52. Failure analysis of pump shaft fracture of a high-pressure coke removal water pump10.1016/j.engfailanal.2025.109814 ↗
53. Comparative study on the effects of Cr, V, and Mo carbides for hydrogen-embrittlement resistance of tempered martensitic steel10.1038/s41598-019-41436-2 ↗
54. Criteria for slip transfer across grain and twin boundaries in pure Ni10.1016/j.mtla.2021.101303 ↗
55. On the origin of deformation mechanisms in a heterostructured aluminum alloy via slip trace and lattice rotation analyses10.1016/j.msea.2023.144723 ↗
56. Investigation of Micro-crack Initiation as a Trigger of Cleavage Fracture in Ferrite-pearlite Steels10.2355/isijinternational.ISIJINT-2016-396 ↗
57. Preparation of an overall intergranular fracture surface caused by hydrogen and identification of lattice defects present in the local area just below the surface of tempered martensitic steel10.1016/j.scriptamat.2022.115072 ↗
58. Quantitative investigation on deep hydrogen trapping in tempered martensitic steel10.1016/j.jallcom.2020.157218 ↗
59. Influence of Mo carbides and two-stage tempering methodology on the susceptibility of medium carbon martensitic steel to hydrogen embrittlement10.1016/j.engfailanal.2024.108562 ↗
60. Assessment of the potential of hydrogen plasma charging as compared to conventional electrochemical hydrogen charging on dual phase steel10.1016/j.msea.2019.03.097 ↗
61. Simultaneous improvement of hydrogen embrittlement resistance and tensile strength of quenching and partitioning steel through dense multiple interfaces10.1016/j.ijhydene.2024.01.270 ↗
62. First-Principles study of hydrogen solubility and embrittlement of Cr23C6 in nickel-based alloys10.1016/j.commatsci.2024.113304 ↗
63. Atomistic simulation study of the grain-size effect on hydrogen embrittlement of nanograined Fe10.1016/j.ijhydene.2019.11.131 ↗
64. Effects of grain size on hydrogen embrittlement in a Fe-22Mn-0.6C TWIP steel10.1016/j.ijhydene.2015.06.112 ↗
65. Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testing10.1016/j.corsci.2017.08.032 ↗
66. Effect of grain size on the hydrogen embrittlement sensitivity of a precipitation strengthened Fe–Ni based alloy10.1016/j.msea.2013.11.062 ↗
67. Effect of Austenite grain size on transformation behavior, microstructure and mechanical properties of 0.1C–5Mn Martensitic Steel10.2355/isijinternational.53.2218 ↗
68. Effect of grain size on mechanical properties of dual phase steels composed of ferrite and martensite10.1557/adv.2016.230 ↗
69. Grain refinement of dual phase steel maximizes deformation ability of martensite, leading to simultaneous enhancement of strength and ductility10.1016/j.actamat.2025.121061 ↗
70. Hydrogen embrittlement fracture mechanism of 430 ferritic stainless steel: The significant role of carbides and dislocations10.1016/j.msea.2021.142043 ↗
71. The role of size and volume fraction of carbides on hydrogen embrittlement and white etching areas formation in bearing steel under dynamic loading10.1016/j.ijfatigue.2023.107837 ↗
72. Role of interface between ferrite and martensite in hydrogen embrittlement behavior of ultra-high strength dual-phase steel sheets10.2355/isijinternational.ISIJINT-2019-013 ↗
73. Effect of ferrite on the hydrogen embrittlement in quenched-partitioned-tempered low carbon steel10.1016/j.msea.2017.12.032 ↗
74. Strong hydrogen trapping by tangled dislocations in cold-drawn pearlitic steels10.1016/j.actamat.2025.121231 ↗
75. Ferrite-enabled improvement of hydrogen embrittlement through strain partitioning in quenching and partitioning steels10.1016/j.msea.2024.147008 ↗
76. Investigation of hydrogen embrittlement in welded joints of the L360MH pipeline steel for hydrogen transportation10.1016/j.corsci.2025.112940 ↗
77. Effect of Electrochemical Hydrogen Charging on Hydrogen Embrittlement and Mechanical Properties of Quenched Tempered X100 Pipeline Steel10.1007/s11668-023-01841-2 ↗
78. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
79. Limitations of hydrogen detection after 150 years of research on hydrogen embrittlement10.1002/adem.202470048 ↗