Effect of deformation and high-temperature concentrated alkaline solution on intergranular oxidation behavior and cracking resistance of Alloy 690 plugs
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: High Temperature Alloys and Creep · Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (74)
Show source-provided references
1. Review of PWSCC and mitigation management strategies of alloy 600 materials of PWRs10.1016/j.jnucmat.2013.07.032 ↗
2. General corrosion and stress corrosion cracking of alloy 600 in light water reactor primary coolants10.1016/j.jnucmat.2019.04.023 ↗
3. Quantitatively evaluating the contribution of intergranular carbides, Cr-depleted zone, and grain boundary to intergranular stress corrosion cracking of alloy 600 in a simulated boiling water reactors environment with high oxygen concentrations10.1016/j.actamat.2024.119794 ↗
4. Assessing the influence of welding-induced mechanics on oxidation and stress corrosion cracking in an alloy 600-Alloy 152 m weldment under simulated PWR primary water10.1016/j.jnucmat.2024.155349 ↗
5. Effect of heat treatment on the stress corrosion cracking of alloy 69010.1016/S0921-5093(01)01747-6 ↗
6. Application of grain boundary engineering concepts to alleviate intergranular cracking in alloys 600 and 69010.1016/0921-5093(94)90925-3 ↗
7. Appling grain boundary engineering to alloy 690 tube for enhancing intergranular corrosion resistance10.1016/j.jnucmat.2011.06.017 ↗
8. SCC of alloy 690 and its weld metals in high temperature water[C]
9. Stress corrosion cracking of current structural materials in commercial nuclear power plants10.5006/0801 ↗
10. A review of stress corrosion cracking of austenitic stainless steels in PWR primary water10.1016/j.jnucmat.2023.154815 ↗
11. PWSCC in the tube expansion zone-an overview10.1016/0029-5493(93)90217-W ↗
12. Degradation of alloy 600 steam generator tubes in operating pressurized water reactor nuclear power plants10.5006/1.3277611 ↗
13. Insights into the stress corrosion cracking of solution annealed alloy 690 in simulated pressurized water reactor primary water under dynamic straining10.1016/j.actamat.2018.04.002 ↗
14. Insights into stress corrosion cracking in scratched area of alloy 690TT steam generator tubes10.1016/j.actamat.2023.119083 ↗
15. Effect of temperature on corrosion fatigue behavior of inconel alloy 690TT steam generator tube10.1016/j.corsci.2023.111741 ↗
16. Corrosion of steam generator pipelines analysed using mössbauer spectroscopy10.1016/j.nucengdes.2005.04.009 ↗
17. Fretting wear of alloy 690 tube mated with different materials in high temperature water10.1016/j.wear.2018.01.001 ↗
18. Degradation analysis strategy on alloy 690 SG tubings of a retired steam generator
19. Aging and life extension of major light water reactor components
20. Unraveling the local stress corrosion cracking behavior of alloy 690 plug in a high-temperature concentrated alkaline solution10.1016/j.corcom.2024.12.001 ↗
21. Caustic stress corrosion cracking of alloys 600 and 690 with NaOH concentrations10.1007/BF03027511 ↗
22. Kähkönen · 2009
23. Analysis of dislocation density in strain-hardened alloy 690 using scanning transmission electron microscopy and its effect on the PWSCC growth behavior
24. Three-dimensional study on the hydraulic characteristics under the steam generator (SG) tube plugging operations for AP100010.1016/j.pnucene.2018.10.016 ↗
25. Crack growth and cracking behavior of alloy 600/182 and alloy 690/152 welds in simulated PWR primary water
26. EPRI, materials reliability program: resistance to primary water stress corrosion cracking of Alloys 690, 52, and 152 in pressurized water reactors (MRP-111)[R] Report 1009801, Electric Power Research Institute (2004).
27. On the role of intergranular nanocavities in long-term stress corrosion cracking of alloy 69010.1016/j.actamat.2021.117453 ↗
28. ASEM. Code. Rules For In-service Inspection of Nuclear Power Plant Components. Paris: AFCEN; 1997 Edition + 1998, 2000 and 2005 addenda.
29. Susceptibility of alloy 690 to stress corrosion cracking in caustic aqueous solutions
30. Stress corrosion cracking of alloy 600 and alloy 690 in caustic solution
31. The correlation between the dislocation slip/grain boundary interaction mode and the resistance to SCC initiation of alloy 690 in simulated PWR primary water10.1016/j.corsci.2023.111096 ↗
32. Grain boundary character distribution in ordered FeAl10.1016/S1359-6462(97)00356-4 ↗
33. A study on the diffusion-induced grain boundary migration ahead of stress corrosion cracking crack tips through advanced characterization10.1016/j.corsci.2021.109328 ↗
34. A mechanistic study of SCC in alloy 600 through high-resolution characterization10.1016/j.corsci.2018.01.004 ↗
35. Quantification of SCC mechanisms in austenitic alloys under PWR primary water conditions
36. How oxidized grain boundaries fail10.1016/j.actamat.2013.05.012 ↗
37. Mechanistic understanding of the temperature dependence of crack growth rate in alloy 600 and 316 stainless steel through high-resolution characterization10.1016/j.actamat.2018.11.039 ↗
38. The intergranular oxidation behavior of low-angle grain boundary of alloy 600 in simulated pressurized water reactor primary water10.1016/j.actamat.2021.117533 ↗
39. The dependence of carbide morphology on grain boundary character in the highly twinned alloy 69010.1016/j.jnucmat.2010.01.008 ↗
40. The growth mechanism of grain boundary carbide in alloy 69010.1016/j.matchar.2013.04.005 ↗
41. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
42. Temperature-dependent, multi-mechanism crystal plasticity reveals the deformation and failure behaviour of multi-principal element alloys10.1016/j.jmps.2024.105549 ↗
43. Using local GND density to study SCC initiation10.1016/j.ultramic.2020.113054 ↗
44. Overcoming the drawbacks of plastic strain estimation based on KAM10.1016/j.ultramic.2017.08.013 ↗
45. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
46. The effect of grain boundary structure on the intergranular degradation behavior of solution annealed alloy 690 in high temperature, hydrogenated water10.1016/j.actamat.2019.10.041 ↗
47. The structure dependence of oxidation behavior of high-angle grain boundaries of alloy 600 in simulated pressurized water reactor primary water10.1016/j.corsci.2023.111162 ↗
48. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
49. The corrosion behaviour of alloy 690 tube in simulated PWR secondary water with the effect of solid diffusing hydrogen10.1016/j.jnucmat.2019.02.019 ↗
50. Magnetite deposition behavior on alloy 600 and alloy 690 tubes in simulated PWR secondary water10.3390/coatings12091231 ↗
51. Effect of surface hemispherical dent depth on the microstructure evolution and stress corrosion cracking of heat transfer tubes in steam generator10.1016/j.corsci.2024.111950 ↗
52. Experimental study on tube-to-tube reciprocating sliding wear behaviors of inconel 690 heat transfer tubes10.1016/j.nucengdes.2024.113002 ↗
53. The single effect of microstructure, residual strain and geometric structure on the stress corrosion cracking behavior of scratched alloy 690TT10.1016/j.corsci.2023.111709 ↗
54. Surface grain boundary engineering of alloy 600 for improved resistance to stress corrosion cracking10.1016/j.msea.2015.09.074 ↗
55. The role of secondary phases on SCC initiation of alloy 718 in simulated PWR primary water10.1016/j.corsci.2025.112930 ↗
56. Current developments of nanoscale insight into corrosion protection by passive oxide films10.1016/j.cossms.2018.05.004 ↗
57. Characterization of the crack initiation and propagation in alloy 600 with a cold-worked surface10.1016/j.corsci.2019.03.014 ↗
58. Computer calculated potential pH diagrams to 300 ℃(EPRI NP-3137), EPRI report. The Babcock & Wilcox Company, Allliance, Ohio, (1983).
59. Self-diffusion in austenitic Fe-Cr-Ni alloys10.1088/0305-4608/10/3/009 ↗
60. Effect of heat treatment applied potential on the caustic stress corrosion cracking of inconel 60010.5006/1.3583025 ↗
61. Effects of heat-treatment on the extent of chromium depletion and caustic corrosion resistance of alloy 69010.1016/j.corsci.2006.05.043 ↗
62. Insights into the stress corrosion cracking propagation behavior of alloy 690 and 316 l stainless steel in KOH versus LiOH oxygenated water10.1016/j.corsci.2023.111556 ↗
63. Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam10.1016/j.actamat.2022.117634 ↗
64. On the passivity of iron-chromium alloys: I. Reversible primary passivation and secondary film formation10.1149/1.2426646 ↗
65. Effect of surface scratch depth on microstructure change and stress corrosion cracking behavior of alloy 690TT steam generator tube10.1016/j.corsci.2021.109792 ↗
66. Effects of post-weld heat treatment on nanoscale microstructural degradation and primary water stress corrosion cracking resistance of submerged-arc-welded alloy 52M overlays10.1016/j.corsci.2025.113213 ↗
67. Nano-micrometer scale characterization of PWSCC crack tips in the transition zone of 52M overlay and the implication to intergranular cracking10.1016/j.jnucmat.2024.155400 ↗
68. High resolution characterization of Pb-SCC in alloy 800 exposed to 330 °C mildly caustic environments10.1016/j.corsci.2018.05.031 ↗
69. Effect of stress and surface finish on Pb-caustic SCC of alloy 690TT10.1016/j.corsci.2021.109462 ↗
70. De-alloying of type 316 stainless steel in hot, concentrated sodium hydroxide solution10.1016/j.corsci.2004.01.011 ↗
71. Multi-scale characterization of stress corrosion cracking of cold-worked stainless steels and the influence of cr content10.1016/j.actamat.2009.07.040 ↗
72. Dependence of stress corrosion cracking of alloy 690 on temperature, cold work, and carbide precipitation-role of diffusion of vacancies at crack tips10.5006/1.3563640 ↗
73. Linking grain boundary microstructure to stress corrosion cracking of cold-rolled alloy 690 in pressurized water reactor primary water10.5006/0808 ↗
74. Formulating stress corrosion cracking growth rates by combination of crack tip mechanics and crack tip oxidation kinetics10.1016/j.corsci.2009.10.041 ↗