Temperature-induced atypical oxidation in Sm2(Co, Fe, Cu, Zr)17 alloy systems: Dependency on oxygen-induced elemental migration
Source abstract
Abstract
This paper addresses temperature and/or oxygen-induced chemical segregation of elements in the growth of oxide scale on Sm 2(Co, Fe, Cu, Zr) 17 . Whereas, oxidation at T ≤ 573 K leads to primarily iron and cobalt segregation and subsequently their oxides, that at > 573 K, yields to largely CuO because of copper segregation. Only combination of higher sample temperature and environmental oxygen are found to have driven copper from alloy interior to its surface. Moreover, oxidation mechanism is considerably slowed down at higher temperature and is attributed to semi passivating surface copper oxide formation, impeding passage of oxygen to layers underneath to it.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Rare-earth and actinide compounds
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. M. Marinescu, J.F. Liu and M.H. Walmer, Recent Progress in Sm-Co Type Permanent Magnets M. Marinescu, J. F. Liu and M. H. Walmer Electron Energy Corporation, Landisville, PA, USA, (2008) 1–8.
2. RETM5 and RE2TM17 permanent magnets development10.1063/1.341084 ↗
3. Metallurgical behavior of Sm(Co,Fe,Cu,Zr)z alloys10.1063/1.333575 ↗
4. M.S. Walmer, M.H. Walmer, C.H. Chen, A new class of permanent-magnetic materials for high temperature applications in TWTs, Int. Vac. Electron. Conf. 2000, IVEC 2000. (2000). https://doi.org/10.1109/OVE:EC.2000.847557.10.1115/2000-GT-0412 ↗
5. Magnetic and structural properties of commercial Sm2(Co, Fe, Cu, Zr)17-based magnets10.1063/1.367565 ↗
6. High-temperature magnetic properties and microstructural analysis of Sm(Co, Fe, Cu, Zr)z permanent magnets10.1016/S0304-8853(99)00322-4 ↗
7. Investigation on microstructure and magnetic properties of Sm2Co17 magnets aged at high temperature10.1063/1.3563084 ↗
8. Anomalous high temperature oxidation of Sm2(Fe, Co, Cu, Zr)17 particles10.1016/j.corsci.2012.08.049 ↗
9. Thermal stability of Sm-Tm high temperature magnets at 300–550 °C10.1109/20.908773 ↗
10. Prediction of the oxidation behaviour of Sm-Co-based magnets10.1016/j.jmmm.2004.11.408 ↗
11. Corrosion behavior of Sm-Co-based permanent magnets in oxidizing environments10.1109/TMAG.2004.829195 ↗
12. The oxidation of SmCo magnets10.1063/1.2830559 ↗
13. The oxidation morphology of SmCo alloys10.1016/j.jallcom.2009.07.115 ↗
14. The oxidation kinetics of SmCo alloys10.1016/j.jallcom.2008.05.083 ↗
15. The mechanism of high temperature oxidation of a SmCo-based magnetic alloy10.1016/j.corsci.2012.04.028 ↗
16. Internal oxidation of Sm(CobalFe0.22Cu0.08Zr0.02)7.5 alloy at 700°C10.1016/j.corsci.2013.01.038 ↗
17. Decomposition behavior in the early-stage oxidation of Sm2Co17-type magnets10.1016/j.scriptamat.2021.113911 ↗
18. The effect of grain size on the internal oxidation of Sm2Co17-type permanent magnets10.1016/j.jmmm.2022.169219 ↗
19. Evolution and effects of surface degradation layer of Sm2Co17 magnets at high temperatures10.1063/1.4862857 ↗
20. The effect of a surface Cr film on the oxidation of SmCo-based magnetic alloy at 700°C10.1016/j.corsci.2013.07.033 ↗
21. Atomic Force Microscopy, Scanning Kelvin Probe Force Microscopy and magnetic measurements on thermally oxidized AISI 304 and AISI 316 stainless steels10.1016/j.corsci.2010.11.031 ↗
22. Nanoscale characterization of copper oxide films by Kelvin Probe Force Microscopy10.1016/j.tsf.2015.01.071 ↗
23. Effect of dry thermal oxidation on the microstructure and magnetic properties of SmCo5 permanent magnet10.1016/j.corsci.2021.109647 ↗
24. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni10.1016/j.apsusc.2010.10.051 ↗
25. Surface chemistry of zirconia nanopowders doped with Pr2O3: An XPS study10.12693/APhysPolA.114.S-125 ↗
26. Advanced analysis of copper X-ray photoelectron spectra10.1002/sia.6239 ↗
27. Thermodynamic properties of minerals and related substances at 298.15K and 1 Bar
28. The binary rare earth oxides10.1021/cr940055h ↗
29. R.T. Mittireddi, N.H., Makani, R.K. Singh, R. Banerjee, E. Panda, Heating/cooling induced formation, dissociation and phase separation during thermal oxidation of Sm2(Co, Fe, Cu, Zr)17 permanent magnet, (2023). [Manuscript submitted].10.1016/j.corsci.2023.111774 ↗
30. The ternary system Sm2O3-SrO-CuO: Compounds and phase relations10.1016/S0925-8388(00)01255-X ↗
31. Diffusion behaviour of creep-resistant steels
32. Oxidation behavior of copper at a temperature below 300°C and the methodology for passivation10.1590/1980-5373-MR-2015-0139 ↗
33. Self-limiting oxidation of copper10.1063/1.122608 ↗