Corrosion of engineering ceramic materials by molten iron part I: Silicon nitride and SiAlON
Source abstract
Abstract
Abstract The corrosion resistance of two different polycrystalline materials (Si 3 N 4 , SiAlON) by molten iron at 1600 °C has been investigated. Silicon nitride reacts with molten iron very rapidly while SiAlON exhibited the improved corrosion resistance. Better corrosion resistance of SiAlON is caused by the formation of protective layer of Al 2 O 3 in the initial stage of corrosion test. In the present work the influence of exposure time on the residual strength of the polycrystalline materials has also been estimated. The strength of the SiAlON after 8 h of corrosion was only 20% of the initial strength of the same material before corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Low cost preparation of Si3N4–SiC micro/nano composites by in-situ carbothermal reduction of silica in silicon nitride matrix10.1016/S0955-2219(03)00604-6 ↗
2. Carbothermal reduction and nitridation of powder pyrophyllite raw material10.1016/S0955-2219(03)00335-2 ↗
3. Liquid phase sintering of SiC with AlN and rare-earth oxide additives, silicon-based structural ceramics for the new millennium10.1002/9781118405970.ch12 ↗
4. Design of Si3N4 based layered composites for multifunctional application
5. Chemical resistance of ceramic materials in acid and alkalis10.1023/B:GLAC.0000048706.05368.71 ↗
6. Lavrenko · 1989
7. The corrosion behaviour of ceramic materials in caustic alkaline solutions at high temperature10.1016/0010-938X(92)90207-J ↗
8. Oxidation and liquid aluminium degradation of a nitride-Bonded SiC ceramic10.1016/0010-938X(93)90311-4 ↗
9. Corrosion of ceramics
10. Corrosion of silicon nitride ceramics in aqueous HCl and HF solutions at 27–80°C10.1016/S0010-938X(98)00011-0 ↗
11. Corrosion behaviour of Si3N4–TiN composite in sulfuric acid10.1016/j.corsci.2004.07.042 ↗
12. The corrosion of ceramics: where do we go from here?10.4028/www.scientific.net/KEM.113.1 ↗
13. High-temperature interactions of alumina-carbon refractories with molten iron10.2355/isijinternational.50.804 ↗
14. Behaviour of the wettability of a SiAlON-base ceramic by molten steel10.1016/j.jeurceramsoc.2004.02.020 ↗
15. Interaction of Si3N4 with carbonyl iron under nitrogen or argon atmosphere10.2109/jcersj.105.734 ↗
16. Phase diagrams of the ternary systems Mn, Fe Co, Ni–Si–N10.1016/0022-4596(87)90054-5 ↗
17. Structural properties of liquid Fe–Si alloys10.1016/S0022-3093(02)01051-7 ↗
18. Corrosion of β-sialon-based ceramics by molten steel10.1016/j.jeurceramsoc.2006.08.012 ↗