Study of the migration and distribution pathways of key corrosive species during high-temperature corrosion by means of atom probe tomography and δ35Cl isotope tracer

Wenchao Ma, Sixuan Zeng, Terrence Wenga

Corrosion Science· Volume 234
Publisher page

Abstract

This study investigated the migration pathways and the dominant chlorine- and alkali-induced corrosion mechanisms of Ni-28Cr-13Al-0.6B-0.5 W alloy at 600ºC. The distribution of key elements ( 35Cl, 37 Cl, Na, O, Ni, Cr, Al) at the alloy/oxide interface was analyzed by APT coupled with δ 35 Cl isotope labeling for tracing the competitiveness of organic chlorine and inorganic chlorine. The alloying element`s migration rate was in the order of Al > Cr > Ni > W. Cl diffused through oxide grain-boundaries as Cl - ions formed by the decomposition of sulfate-melt and corrosion in grain-boundaries was dominated by electrochemical reaction mechanisms. Na enhances the diffusion of elements by widening the grain-boundaries.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Materials Characterization Techniques · High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. NBSC, China Statistical Yearbook 2022. Available on: 〈http://www.stats.gov.cn/sj/ndsj/2015/indexeh.htm〉, (2022).
2. NBSC, China Statistical Yearbook 2015. Available on: 〈http://www.stats.gov.cn/sj/ndsj/2015/indexeh.htm〉, (2015).
3. The fate of chlorine during MSW incineration: Vaporization, transformation, deposition, corrosion and remedies10.1016/j.pecs.2019.100789 ↗
4. Waste to Energy Operability Enhancement under Waste Uncertainty via Oxygen Enrichment10.1021/es502106u ↗
5. Municipal solid waste fueled power generation in china: a case study of waste-to-energy in Changchun City10.1021/es071416g ↗
6. Dongyun · 2019
7. The effect of Cl, Br, and F on high-temperature corrosion of heat-transfer alloys10.1016/j.fuel.2023.128516 ↗
8. Chlorine-induced high-temperature corrosion characteristics of Ni-Cr alloy cladding layer and Ni-Cr-Mo alloy cladding layer10.1016/j.corsci.2023.111102 ↗
9. Zero Waste Europe, Understanding the carbon impacts of Waste to Energy incineration: Climate, Energy and Air Pollution, Available on 〈https://zerowasteeurope.eu/2020/03/understanding-the-carbon-impacts-of-waste-to-energy/〉 [Accessed on 11 January 2024].
10. Emissions from waste incineration
11. Carbon peak and carbon neutrality in China: goals, implementation path, and prospects
12. High-temperature corrosion evaluation and lifetime prediction of porous Fe22Cr stainless steel in air in temperature range 700–900 °C10.1016/j.corsci.2021.109589 ↗
13. Investigation into high-temperature corrosion in a large-scale municipal waste-to-energy plant10.1016/j.corsci.2010.07.032 ↗
14. High-temperature corrosion behavior of superalloys under actual waste incinerator environment10.1016/j.engfailanal.2016.02.016 ↗
15. Effect of hydrogen chloride on corrosion behaviour of Fe–Cr alloys in Wet CO2 Gas at 650 °C10.1007/s11085-020-09978-3 ↗
16. The influence of KCl and HCl on the high-temperature oxidation of a Fe-2.25Cr-1Mo steel at 400 °C10.1007/s11085-019-09943-9 ↗
17. Effect of pre-oxidation on high-temperature chlorine-induced corrosion properties of air plasma-sprayed Ni-5%Al coatings10.1007/s11666-021-01248-1 ↗
18. Oxidation driven permeation of iron oxide scales by chloride from experiment guided first-principles modeling10.1021/acs.jpcc.9b06497 ↗
19. High-temperature corrosion behavior of Ni and Co base HVOF coatings exposed to NaCl-KCl salt mixture10.1016/j.surfcoat.2021.127277 ↗
20. Long-term corrosion behavior of Cr diffusion coatings on ferritic–martensitic superheater tube material X20CrMoV12-1 under conditions mimicking biomass (co-)firing10.1021/acs.energyfuels.0c01474 ↗
21. Study on corrosion kinetics of 310H in different simulated MSW combustion environment. The influence of SO2 and H2O on NaCl assisted corrosion10.1016/j.corsci.2019.04.013 ↗
22. High-temperature corrosion of Hastelloy C22 in molten alkali salts: the effect of pre-oxidation treatment10.1016/j.corsci.2020.108761 ↗
23. Microstructural study of the influence of KCl and HCl on preformed corrosion product layers on stainless steel10.1007/s11085-017-9763-z ↗
24. An ESEM in situ investigation of initial stages of the KCl induced high-temperature corrosion of a Fe–2.25Cr–1Mo steel at 400°C10.1016/j.corsci.2011.03.007 ↗
25. Minor element effect on high-temperature corrosion of low-alloyed steel: Insight into alkali- and chlorine induced corrosion by means of atom probe tomography10.1016/j.corsci.2021.109779 ↗
26. Alkali Induced High-Temperature Corrosion of Stainless Steel: The Influence of NaCl, KCl and CaCl210.1007/s11085-012-9293-7 ↗
27. Corrosion of superheater materials in a waste-to-energy plant10.1016/j.fuproc.2011.06.017 ↗
28. Superheater deposits and corrosion in temperature gradient e Laboratory studies into effects of flue gas composition, initial deposit structure, and exposure time10.1016/j.energy.2021.120494 ↗
29. High-temperature corrosion mechanism of Ni–5W–6B–28Cr–13Al alloy in simulated MSW incineration environment10.1016/j.jmrt.2022.11.175 ↗
30. Corrosion behavior of Ni-based alloys in molten NaCl-CaCl2-MgCl2 eutectic salt for concentrating solar power10.1016/j.solmat.2017.05.050 ↗
31. Chloridation, and oxidation of iron, chromium, nickel, and their alloys in chloridizing and oxidizing atmospheres at 400–700°C10.1016/S0010-938X(99)00142-0 ↗
32. Long-term corrosion behavior of FeCr(Al, Ni) alloys in O2 + H2O with KCl(s) at 600 °C: Microstructural evolution after breakaway oxidation10.1016/j.corsci.2023.111654 ↗
33. KCl-induced corrosion of the FeCrAl alloy kanthal® AF at 600 °C and the effect of H2O10.1007/s11085-014-9506-3 ↗
34. The role of chromium in the hot corrosion of metals10.1149/1.3159332 ↗
35. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor.10.1023/A:1018875024306 ↗
36. Some thermodynamic aspects of the oxides of chromium10.1007/s11663-014-0027-x ↗
37. X. Ren, J.R. Riley, D.D. Koleske, L.J. Lauhon, Correlated High-Resolution X-ray Diffraction, Photoluminescence, and Atom Probe Tomography Analysis of Continuous and Discontinuous InxGa1-xN Quantum Wells, SAND2015–5515 J.10.1063/1.4926808 ↗
38. Miller · 2014
39. Kaur · 1989
40. Atom probe tomography of oxide scales10.1007/s11085-012-9330-6 ↗
41. STEM and APT characterization of scale formation on a La, Hf, Ti-doped NiCrAl model alloy10.1016/j.micron.2018.01.011 ↗
42. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
43. M. McNallan, W.W. Liang, S.H. Kim, C.T. Kang, Acceleration of the high-temperature oxidation of metals by chlorine, 1983.
44. The hot corrosion of 310 stainless steel with pre-coated NaCl/Na2SO4 mixtures at 750 °C10.1016/j.matchemphys.2004.10.002 ↗
45. Beyond breakaway corrosion – Influence of chromium, nickel, and aluminum on corrosion of iron-based alloys at 600 °C10.1016/j.corsci.2020.108961 ↗
46. The influence of small amounts of KCl(s) on the high-temperature corrosion of a Fe-2.25Cr-1Mo steel at 400 and 500 °C10.1002/maco.201005942 ↗
47. A microstructural and kinetic investigation of the KCl-induced corrosion of a FeCrAl alloy at 600 °C10.1007/s11085-015-9546-3 ↗