journal article·2019-08Open access

Steam oxidation behavior of Ni-base superalloys 690, 725 and X-750 at 600 and 650 °C

L. Tan, T. Chen, B.A. Pint

Corrosion Science· Volume 157

Abstract

Abstract The 1-bar steam oxidation behavior of Ni-base superalloys 690, 725, and X-750 was evaluated at 600 and 650 °C for up to 5000 h. In addition to monitoring mass changes, microstructures of the 5000-h-exposed samples were characterized using scanning and transmission electron microscopy and energy dispersive x-ray spectroscopy. Together with thermodynamic calculations, the scale constitution and possible exfoliation was discussed. Alloy X-750 exhibited the best resistance to steam oxidation with the least metal thickness loss at 600 °C while alloy 690 at 650 °C. Alloy 725 exhibited more than two times metal thickness loss than the other two alloys at 650 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Farrar · 2004
2. Crack growth and high temperature thermal stability of Inconel alloy 725
3. Smith · 2006 · Vol. 1 · 256
4. Structural materials for fission & fusion energy10.1016/S1369-7021(09)70294-9 ↗
5. The oxidation of alloy 690 in simulated pressurized water reactor primary water10.1016/j.corsci.2017.07.004 ↗
6. Oxidation of alloy 600 and alloy 690: experimentally accelerated study in hydrogenated supercritical water10.1007/s11661-016-3897-5 ↗
7. Corrosion behavior of alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
8. Characteristics of oxidation and oxygen penetration of alloy 690 in 600 °C aerated supercritical water10.1016/j.jmst.2016.11.001 ↗
9. Oxide evolution on alloy X-750 in simulated BWR environment10.1016/j.jnucmat.2016.09.026 ↗
10. High resolution electron microscopy study on oxide films formed on nickel-base alloys X-750, 182 and 82 in simulated high flow velocity BWR water conditions
11. Corrosion behavior of Ni-base alloys in supercritical water10.5516/NET.2009.41.1.107 ↗
12. 1988
13. Oxidation behavior of grain boundary engineered alloy 690 in supercritical water environment10.1016/j.jnucmat.2011.12.022 ↗
14. Survey of oxidation in steamside conditions
15. Oxidation behavior of austenitic heat-resisting steels in a high temperature and high pressure steam environment10.2355/isijinternational1966.28.761 ↗
16. Oxidation model for construction materials in supercritical water–estimation of kinetic and transport parameters10.1016/j.corsci.2015.06.033 ↗
17. Internal oxidation of alloy 690 in hydrogenated steam10.1016/j.corsci.2014.11.006 ↗
18. 2018
19. More features, more tools, more CrysTBox10.1107/S1600576717006793 ↗
20. Protective oxide film on alloy X750 formed in air at 973 K10.1080/18811248.1994.9735190 ↗
21. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗
22. Thermal expansion
23. Thermal expansion of corundum structure Ti2O3 and V2O310.1063/1.1662787 ↗
24. Zaplatynsky · 1971
25. Stress effects in high temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
26. Thermodynamic investigation of the vaporization of molybdenum trioxide10.1016/0925-8388(92)90442-C ↗
27. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗