In situ synthesis, mechanical properties, and oxidation resistance of (SiC+ZrB 2 )/Zr 3 [Al(Si)] 4 C 6 composites

Lei Yu, Limei Pan, Jian Yang, Yongbao Feng, Jingxian Zhang, Tai Qiu

Corrosion Science· Volume 110
Publisher page

Abstract

Abstract In situ (SiC+ZrB 2 )/Zr 3 [Al(Si)] 4 C 6 composites with 0–15 vol.% SiC and 15 vol.% ZrB 2 were prepared. As reinforcements, the incorporation of SiC and ZrB 2 shows significant strengthening and toughening effect by the synergistic action of mechanisms including particulate reinforcement, grain-refinement, and grain’s pull-out, etc. The oxidation kinetics of the composites at 1000–1300 °C in air follows a parabolic law. With the incorporation and increase of SiC, the oxidation resistance of the composites is improved remarkably. It is attributed to the formation of a protective oxide scale containing borosilicate glass and more mullite, which effectively prevents the inward diffusion of oxygen.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Recent progress in theoretical prediction, preparation, and characterization of layered ternary transition-metal carbides10.1146/annurev-matsci-082908-145340 ↗
2. Synthesis and structure-property relationships of a new family of layered carbides in Zr-Al(Si)-C and Hf-Al(Si)-C systems10.1016/j.jeurceramsoc.2013.05.020 ↗
3. Synthesis, crystal structure, and thermoelectric properties of a new layered carbide (ZrC)3[Al3.56Si0.44]C310.1557/JMR.2007.0372 ↗
4. Oxidation of Zr2[Al(Si)]4C5 and Zr3[Al(Si)]4C6 in air10.1557/JMR.2008.0411 ↗
5. Atomic-scale microstructure and elastic properties of quaternary Zr-Al-Si-C ceramics10.1016/j.actamat.2007.12.055 ↗
6. High-temperature internal friction, stiffness and strength of Zr-Al(Si)-C ceramics10.1016/j.scriptamat.2009.03.004 ↗
7. Mechanical and thermophysical properties of Zr-Al-Si-C ceramics10.1111/j.1551-2916.2008.02879.x ↗
8. Effect of grain size, notch width, and testing temperature on the fracture toughness of Ti3Si(Al)C2 and Ti3AlC2 using the chevron-notched beam (CNB) method10.1016/j.jeurceramsoc.2007.07.011 ↗
9. Oxidation behaviour of Ti3SiC2-based ceramic at 900–1300°C in air10.1016/S0010-938X(00)00142-6 ↗
10. Cyclic oxidation of Ti3AlC2 at 1000–1300°C in air10.1016/j.corsci.2010.09.033 ↗
11. Oxidation of Ti2AlC bulk and spray deposited coatings10.1016/j.corsci.2010.08.004 ↗
12. Oxidation behavior and kinetics of in situ (TiB2+TiC)/Ti3SiC2composites in air10.1016/j.ceramint.2011.05.156 ↗
13. Reciprocating friction and wear behavior of Zr2[Al(Si)]4C5 and Zr2[Al(Si)]4C5-SiC composite against Si3N4 ball10.1111/j.1551-2916.2010.03718.x ↗
14. Microstructure, mechanical, thermal and oxidation properties of a Zr2[Al(Si)]4C5-SiC composite prepared by in situ reaction/hot-pressing10.1016/j.jeurceramsoc.2010.02.005 ↗
15. Microstructure and properties of hot pressed Zr2[Al(Si)]4C5/SiC composites10.1016/j.jallcom.2009.03.142 ↗
16. Oxidation resistance of Zr2[Al(Si)]4C5 based composites at ultra-high-temperature10.1016/j.scriptamat.2009.06.004 ↗
17. Isothermal oxidation of Zr2[Al(Si)]4C5-SiC composites at 1000–1300°C in air10.1016/j.corsci.2011.09.016 ↗
18. Improvement of mechanical properties of Al2O3/Ti3SiC2 multilayer ceramics by adding SiC whiskers into Al2O3 layers10.1016/j.ceramint.2005.10.007 ↗
19. Microstructure and mechanical properties of in situ synthesized (TiB2+TiC)/Ti3SiC2 composites10.1016/j.ceramint.2011.06.066 ↗
20. In situ synthesis of (TiB2+SiC)/Ti3SiC2 composites by hot pressing10.1016/j.matlet.2012.01.061 ↗
21. High-strength zirconium diboride-based ceramics10.1111/j.1551-2916.2004.01170.x ↗
22. Oxidation mechanism and resistance of ZrB2-SiC composites10.1016/j.corsci.2009.07.005 ↗
23. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
24. Effects of ZrB2 and SiC dual addition on the oxidation resistance of graphite at 1600–2000°C10.1016/j.corsci.2013.06.041 ↗
25. Oxidation behavior and phase transition of ZrB2-SiCw-ZrO2f ceramic10.1016/j.corsci.2013.08.002 ↗
26. Mechanical and thermal physical properties, and thermal shock behavior of (ZrB2+SiC) reinforced Zr3[Al(Si)]4C6 composite prepared by in situ hot-pressing10.1016/j.jallcom.2014.08.247 ↗
27. Microstructure, mechanical, and thermal properties of (ZrB2+ZrC)/Zr3[Al(Si)]4C6 composite10.1111/jace.13038 ↗
28. In situ reaction synthesis and characterization of Ti3Si(Al)C2/SiC composites10.1016/j.ceramint.2005.07.004 ↗
29. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
30. Microstructure and oxidation behavior of C/C-ZrB2-SiC composites coated with SiC coating at high temperature10.1016/j.corsci.2015.08.015 ↗
31. Coatings of metastable ceramics deposited by solution-precursor plasma spray: I. Binary ZrO2-Al2O3 system10.1016/j.actamat.2006.06.025 ↗
32. Dense alumina-zirconia coatings using the solution precursor plasma spray process10.1111/j.1551-2916.2007.02023.x ↗
33. Isothermal oxidation of bulk Zr2Al3C4 at 500–1000°C in air10.1557/JMR.2008.0042 ↗
34. Phase stability of zirconia
35. Zirconium aluminum carbides: new precursors for synthesizing ZrO2-Al2O3 composites10.1111/j.1551-2916.2009.03281.x ↗
36. Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si-B-C coating in static air10.1016/j.corsci.2012.08.003 ↗
37. The thermal stability in air of hot-pressed diboride matrix composites for uses at ultra-high temperatures10.1016/j.corsci.2004.09.019 ↗
38. Microstructure and oxidation resistance of Mo-Si-B coating on Nb based in situ composites10.1016/j.corsci.2014.07.006 ↗
39. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si-B-C/SiC coatings under wet oxygen atmosphere10.1016/j.apsusc.2015.06.153 ↗
40. Structure and properties of mullite-a review10.1016/j.jeurceramsoc.2007.03.017 ↗
41. Oxidation behavior of Al4SiC4 ceramic up to 1700°C10.1016/j.corsci.2006.10.028 ↗
42. Infrared spectra of alkali-free aluminoborosilicate glass structure
43. Mechanisms of room temperature metastable tetragonal phase stabilisation in zirconia10.1179/174328005X14267 ↗
44. Polymer-derived SiAlCN ceramics resist oxidation at 1400°C10.1016/j.scriptamat.2006.05.004 ↗
45. ZrB2-SiC(Al) ceramics with high resistance to oxidation at 1500°C10.1016/j.corsci.2013.04.037 ↗
46. Chiang · 1997