Corrosion characterisation of laser beam and tungsten inert gas weldment of nickel base alloys: Micro-cell technique
Source abstract
Abstract
Abstract The electrochemical studies using micro-cell technique gave new understanding of electrochemical behaviour of nickel base alloys in solution annealed and welded conditions. The welding simulated regions depicted varied micro structural features. In case of tungsten inert gas (TIG) weldments, the weld fusion zone (WFZ) showed least corrosion resistance among all other regions. For laser beam (LB) weldments it was the heat-affected zone (HAZ) that showed comparatively high stable anodic current density. The high heat input of TIG welding resulted in slower heat dissipation hence increased carbide precipitation and segregation in WFZ resulting in high stable anodic current density.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Smith · 1993 · 321
2. Uhlig · 1991 · 12
3. Jones · 1996
4. Sedriks · Corrosion · 1986 · 42 · 37610.5006/1.3584918 ↗
5. Lohrengel · Elecrochim. Acta · 2004 · 49 · 286310.1016/j.electacta.2004.01.068 ↗
6. Andreatta · Electrochim. Acta · 2003 · 48 · 323910.1016/S0013-4686(03)00379-7 ↗
7. Isaacs · 1981 · 3
8. Alpeter · Werkst. Korros. · 1992 · 43 · 9610.1002/maco.19920430303 ↗
9. Isaacs · J. Electrochem. Soc. · 1988 · 135 · 218010.1149/1.2096235 ↗
10. Pistorius · Corros. Sci. · 1992 · 33 · 188510.1016/0010-938X(92)90191-5 ↗
11. Krolikowski · Electrochim. Acta · 1987 · 32 · 61510.1016/0013-4686(87)87050-0 ↗
12. Briant · Corrosion · 1986 · 42 · 1510.5006/1.3584874 ↗
13. Was · Metall. Trans. · 1987 · 18A · 131310.1007/BF02647201 ↗
14. Berge · Nucl. Technol. · 1981 · 55 · 8810.13182/NT81-A32833 ↗
15. Bandy · Corrosion · 1983 · 39 · 39110.5006/1.3593878 ↗
16. Choi · Corrosion · 1992 · 48 · 292-0510.5006/1.3315935 ↗
17. Newman · Corrosion · 1982 · 38 · 26110.5006/1.3577348 ↗
18. Newman · Corrosion · 1989 · 45 · 28210.5006/1.3577855 ↗
19. ASTM Annual Book of Standards E 1473 · 2009
20. Bohni · Electrochim. Acta · 1995 · 40 · 136110.1016/0013-4686(95)00072-M ↗
21. Suter · Electrochim. Acta · 1997 · 42 · 327510.1016/S0013-4686(70)01783-8 ↗
22. P.W. Fuerschbach, D.O. MacCallum, in: Proc. 14th Int. Congress on The Applications of Lasers and Electro-Optics (ICALEO ’95), California, 1995, p. 493.
23. Fuerschbach · Weld. J. · 1996 · 75 · 24
24. The geometric and thermodynamic properties of grain boundary junction10.1023/A:1008769209265 ↗
25. Meng · Corros. Sci. · 2010 · 52 · 92710.1016/j.corsci.2009.11.015 ↗
26. Ferry · Acta Mater. · 2005 · 53 · 109710.1016/j.actamat.2004.11.006 ↗
27. Novikov · Scripta Mater. · 2006 · 55 · 24310.1016/j.scriptamat.2006.04.006 ↗
28. Radaj · 1992
29. Lee · Corros. Sci. · 2009 · 51 · 73310.1016/j.corsci.2009.02.004 ↗
30. G.J. Abraham, Establishing localized corrosion behaviour of Ni–Cr–Fe alloy using electrochemical techniques, Ph.D. Thesis, IIT Bombay, Mumbai, 2012.
31. Takaya · J. Appl. Phys. · 2002 · 91 · 701110.1063/1.1452198 ↗
32. Lu · Electrochim. Acta · 2005 · 50 · 139110.1016/j.electacta.2004.08.036 ↗
33. Kuo · Mater. Sci. Eng. A · 2002 · 338 · 20210.1016/S0921-5093(02)00063-1 ↗
34. Jeng · Mater. Trans. JIM · 2007 · 48 · 48110.2320/matertrans.48.481 ↗