Distinct oxidation behaviour attributed to phase constitution transformation at different hot processing temperatures in Fe-10Mn-5.5Al-0.25C steel
Source abstract
Abstract
Abstract Oxidation behaviour of Fe-10Mn-5.5Al-0.25C (wt.%) steel at 950–1150 °C has been investigated, which showed that oxidation resistance decreased largely with the elevated temperature. Phase constitution transformation included both the high-temperature austenite transformed into ferrite and into martensite. Phase constitution was modified by temperature which led to the transition of elements diffusing from the interface to volume diffusion, degrading the interface concentrations. The oxidation behaviour was changed from internal oxidation to homogeneous oxidation. The continuous and compact Al2O3 layers were more easily formed beneath inner oxide scales when oxidation at relatively low temperature and prevented further oxidation of the experimental steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. An analysis of the deformation characteristics of a dual phase twinning-induced plasticity steel in warm working temperature regime10.1016/j.matdes.2012.04.019 ↗
2. Evolution of microstructure and mechanical properties during thermomechanical processing of a low-density multiphase steel for automotive application10.1016/j.actamat.2014.04.031 ↗
3. Effect of annealing temperature on microstructural modification and tensile properties in 0.35C-3.5Mn-5.8Al lightweight steel10.1016/j.actamat.2013.04.038 ↗
4. Mechanical properties of Fe-Al-M-C (M=Ti, V, Nb, Ta) alloys with strengthening carbides and laves phase10.1016/j.intermet.2004.05.010 ↗
5. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility10.1038/nature14144 ↗
6. κ-carbide hardening in a low-density high-Al high-Mn multiphase steel10.1016/j.matlet.2014.09.104 ↗
7. Designing duplex, ultrafine-grained Fe-Mn-Al-C steels by tuning phase transformation and recrystallization kinetics10.1016/j.actamat.2017.09.026 ↗
8. On the deformation behavior of k-carbide-free and k-carbidecontaining high-Mn light-weight steel10.1016/j.actamat.2016.10.006 ↗
9. Microband-induced plasticity in a high Mn-Al-C light steel10.1016/j.msea.2008.05.042 ↗
10. Microstructures and mechanical properties of high-strength Fe-Mn-Al-C light-weight TRIPLEX steels10.1002/srin.200606440 ↗
11. Origin of extended tensile ductility of a Fe-28Mn-10Al-1C steel10.1007/s11661-009-9862-9 ↗
12. Tensile deformation behavior analysis of low density Fe-18Mn-10Al-xC steels10.1016/j.msea.2015.11.071 ↗
13. The microstructural evolution and mechanical properties of resistance spot welded Fe–31Mn–3Al–3Si TWIP steel10.1016/j.matdes.2014.10.090 ↗
14. Twinning and dynamic strain aging behavior during tensile deformation of Fe-Mn-C TWIP steel10.1016/j.msea.2017.06.012 ↗
15. Correlation between deformation behavior and austenite characteristics in a Mn-Al type TRIP steel10.1016/j.msea.2017.05.058 ↗
16. Tensile deformation behavior of Fe-Mn-Al-C low density steels10.1016/S1006-706X(16)30145-5 ↗
17. Texture, microstructure and mechanical properties of aluminum modified ultra-pure 429 ferritic stainless steels10.1016/j.matdes.2015.09.147 ↗
18. Effect of aluminum on microstructure, mechanical properties and pitting corrosion resistance of ultra-pure 429 ferritic stainless steels10.1016/j.matdes.2014.09.074 ↗
19. Effect of modification treatment on inclusions in 430 stainless steel by Mg-Al alloys10.1016/S1006-706X(13)60089-8 ↗
20. Oxidation of an austenitic stainless steel with or without alloyed aluminum in O2 + 10% H2O environment at 800 °C10.1016/j.corsci.2017.03.015 ↗
21. Improved oxidation resistance of 15 wt.% Cr ferritic stainless steels containing 0.08–2.45 wt.% Al at 1000 °C in air10.1016/j.corsci.2015.08.007 ↗
22. High temperature oxidation of Fe-Al and Fe-Cr-Al alloys: the role of Cr as a chemically active element10.1016/j.corsci.2010.06.019 ↗
23. The effects of Cr and Al concentrations on the oxidation behavior of oxide dispersion strengthened ferritic alloys10.1016/j.corsci.2013.07.004 ↗
24. Criteria for the formation of protective Al2O3 scales on Fe-Al and Fe-Cr-Al alloys10.1016/j.corsci.2005.01.012 ↗
25. A study of the oxidation of FeCrAl alloy in pressurized water and high-temperature steam environment10.1016/j.corsci.2015.02.027 ↗
26. High temperature oxidation behavior of a high Al-containing ferritic heat-resistant stainless steel10.1016/j.matchar.2017.11.038 ↗
27. Effect of alloy grain size on the high-temperature oxidation behaviour of the austenitic steel TP 34710.1590/S1516-14392005000400003 ↗
28. TEM study of the internal oxidation of an Fe-Mn-Al-C alloy after hot corrosion10.1023/A:1014834620707 ↗
29. NaCl-induced hot corrosion of Fe-Mn-Al-C alloys10.1016/S0254-0584(01)00515-6 ↗
30. The hot corrosion of Fe-Mn-Al-C alloy with NaCl/Na2SO4 coating mixtures at 750 °C10.1023/A:1023022100300 ↗
31. Formation and growth morphology of nodules in the high-temperature oxidation of Fe-Mn-Al-C alloy10.1016/S0254-0584(02)00134-7 ↗
32. Oxidation kinetics of an Fe-31.8Mn-6.09Al-1.60Si-0.40C alloy at temperatures from 600 to 900 °C10.1016/j.corsci.2003.10.015 ↗
33. Internal oxidation behavior of Fe-Mn-Al-C duplex steels with good combination of strength and ductility10.1016/j.corsci.2017.03.005 ↗
34. Insights into the role of grain refinement on high-temperature initial oxidation phase transformation and oxides evolution in high aluminium FeMn-Al-C duplex lightweight steel10.1016/j.corsci.2017.07.002 ↗
35. Microstructure and tensile behaviour of duplex low-density steel containing 5 mass % aluminum10.1016/j.scriptamat.2012.09.030 ↗
36. Novel ferrite-austenite duplex lightweight steel with 77% ductility by transformation induced plasticity and twinning induced plasticity mechanisms10.1016/j.actamat.2014.06.059 ↗
37. Effect of annealing temperature on microstructural modification and tensile properties in 0.35C–3.5Mn-5.8Al lightweight steel10.1016/j.actamat.2013.04.038 ↗
38. The thermo-calc databank system10.1016/0364-5916(85)90021-5 ↗
39. Thermo-Calc. Database TCFE2000, upgraded by B.-J. Lee, B. Sundman, KTH, StoCkholm (1999).
40. Thermodynamic calculation on the stability of (Fe, Mn)3AlC carbide in high aluminum steels10.1016/j.jallcom.2010.06.032 ↗
41. SEM, EDX and XRD studies of the scales formed on the Fe-Mn-Al-C system in oxidizing-sulphidizing environments10.1002/xrs.1300200504 ↗
42. Glass coating on stainless steels for high temperature oxidation protection: mechanisms10.1016/j.corsci.2014.01.033 ↗
43. High-temperature oxidation of duplex stainless steels S32101 and S32304 in air and simulated industrial reheating atmosphere10.1016/j.corsci.2010.04.033 ↗
44. Effect of carbon on cavity formation during the high-temperature oxidation of Ni10.1007/BF00603786 ↗
45. The high temperature oxidation of metals forming cation-diffusing scales10.1007/BF02644552 ↗
46. Influence of the alloy grain size on the oxidation behaviour of PM2000 alloy10.1016/S0010-938X(01)00182-2 ↗
47. The oxidation of iron-chromium-manganese alloys at 900 °C10.1007/BF00938460 ↗
48. Fabrication of Cu2O/Fe-O heterojunction solar cells by electrodeposition10.1016/j.tsf.2015.11.034 ↗
49. Raman microspectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
50. High-temperature oxidation studies of low-nickel austenitic stainless steel. Part I: isothermal oxidation10.1023/A:1010329310030 ↗
51. Byzantine wall paintings from Kastoria, northern Greece: spectroscopic study of pigments and efflorescing salts
52. Synthesis of nanocrystalline iron oxide ultrathin films by thermal decomposition of iron nitropruside: structural and optical properties10.1016/j.materresbull.2010.08.006 ↗
53. Peculiar porous α-Fe2O3, γ-Fe2O3 and Fe3O4 nanospheres: facile synthesis and electromagnetic properties10.1016/j.powtec.2014.09.045 ↗
54. Raman studies of corrosion films grown on Fe and Fe-6Mo in pitting conditions10.1016/0010-938X(91)90103-V ↗
55. Raman spectroscopy of thin corrosion films on iron at 100–150 C in air10.5006/1.3583054 ↗
56. The air oxidation of an austenitic Fe-Mn-Cr stainless steel for fusion-reactor applications10.1007/BF00655899 ↗
57. Lattice vibrations of materials for lithium rechargeable batteries V. Local structure of Li0.3MnO210.1016/S0921-5107(03)00079-5 ↗
58. A parametric study on the rapid synthesis of one dimensional (1D) α-MnO2 nanowires10.1016/j.mee.2014.05.028 ↗
59. Re-investigating the CO oxidation mechanism over unsupported MnO, Mn2O3 and MnO2 catalysts10.1016/j.cattod.2007.10.061 ↗
60. Kinetic and spectroscopic study of methane combustion over α-Mn2O3 nanocrystal catalysts10.1016/j.jcat.2007.11.010 ↗
61. Controlled synthesis of Mn3O4 and MnCO3 in a solvothermal system10.1016/j.materresbull.2009.03.004 ↗