Abstract The aerobic corrosion of pipeline steel was investigated in an aqueous sulfide solution by monitoring the corrosion potential and periodically measuring the polarization resistance. The properties and composition of the corrosion product deposits formed were determined using scanning electron microscopy, energy dispersive X-ray analysis, and Raman spectroscopy. The establishment of aerobic conditions leads to corrosion and (oxyhydr)oxide deposition beneath the anaerobically-formed mackinawite film originally present on the steel surface. This leads to blistering and spalling of the sulfide film. Chemical conversion of the mackinawite to Fe(III) (oxyhydr)oxides also occurs but is a relatively slow reaction.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Indicator minerals formed during external corrosion of line pipe
2. External corrosion of line pipe – A summary of research activities
3. Formation of poorly crystalline iron monosulfides: surface redox reactions on high purity iron, spectroelectrochemical studies10.1016/j.corsci.2006.03.010 ↗
4. The transformation of mackinawite into greigite studied by Raman spectroscopy10.1002/jrs.2729 ↗
5. Characterisation of mackinawite by Raman spectroscopy: effects of crystallisation, drying and oxidation10.1016/j.corsci.2008.08.041 ↗
6. The effect of sulfide on the aerobic corrosion of carbon steel in near-neutral pH saline solutions10.1016/j.corsci.2012.09.027 ↗
7. The dry oxidation of tetragonal FeS1−x mackinawite10.1007/s002690100193 ↗
8. The effect of sulfide on carbon steel corrosion behaviour in anaerobic near-neutral pH saline solutions10.5006/0687 ↗
9. Nominally anaerobic corrosion of carbon steel in near-neutral pH saline environments10.5006/1.3381566 ↗
10. Carbon steel corrosion under anaerobic–aerobic cycling conditions in near-neutral pH saline solutions. Part 2: Corrosion mechanism10.1016/j.corsci.2011.07.008 ↗
11. Carbon steel corrosion under anaerobic–aerobic cycling conditions in near-neutral pH saline solutions – Part 1: Long term corrosion behaviour10.1016/j.corsci.2011.07.015 ↗
12. Characterizing the effect of carbon steel exposure in sulfide containing solutions to microbially induced corrosion10.1016/j.corsci.2010.11.027 ↗
13. Cathodic protection potential penetration under disbonded pipeline coating
14. Rate and extent of aqueous perchlorate removal by iron surfaces10.1021/es026007t ↗
15. The preparation of magnetite, goethite, hematite and maghemite of pigment quality from mill scale iron waste10.1016/j.dyepig.2006.01.038 ↗
16. Discrimination among carbonate minerals by Raman-spectroscopy using the laser microsprobe10.1366/0003702874448841 ↗
17. Laser Raman spectroscopy as a technique for identification of seafloor hydrothermal and cold seep minerals10.1016/j.chemgeo.2008.11.008 ↗
18. Phase transformation characterization of olivine subjected to high temperature in air10.1016/j.ceramint.2012.12.031 ↗
19. Fe(II) hydroxycarbonate Fe2(OH)2CO3 (chukanovite) as iron corrosion product: synthesis and study by fourier transform infrared spectroscopy10.1016/j.poly.2008.12.034 ↗
20. The effect of precorrosion on the corrosion rate of steel in neutral solutions containing sulfide – relevance to microbially influenced corrosion10.1016/0010-938X(92)90190-E ↗