Surface oxidation of Alloy 617 in low oxygen partial pressure He–CO–CO2 environments at 750–850 °C

G. Gulsoy, G.S. Was

Corrosion Science· Volume 90

Abstract

Abstract Surface Cr oxidation mechanism of Alloy 617 was investigated in He–CO–CO2 environments with P CO / P CO 2 of either 9 or 1320 at temperatures 750–850 °C. The activation energy for surface oxidation was 169.0 ± 13.2 kJ/mol in He – P CO / P CO 2 = 9 and 234.4 ± 8.9 kJ/mol in He – P CO / P CO 2 = 1320 . The ambient oxygen partial pressure dependence of the measured oxidation rates was consistent with n-type behavior of Cr2O3, in which Cr interstitials are the primary mobile species. The oxidation rates measured were greater than that can be sustained only by lattice diffusion of Cr in Cr2O3, indicating that grain boundary diffusion of Cr plays a role in the Cr2O3 growth kinetics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. R.E. Mizia, Next generation nuclear plant intermediate heat exchanger acquisition strategy, INL/EXT-08-14054, 2008.10.2172/1389177 ↗
2. J.K. Wright, Next generation nuclear plant steam generator and intermediate heat exchanger materials research and development plan, INL/EXT-08-14107, 2010.10.2172/993192 ↗
3. High temperature corrosion of structural materials under gas-cooled reactor helium10.1002/maco.200503901 ↗
4. High temperature reactivity of two chromium-containing alloys in impure helium10.1016/j.jnucmat.2007.11.006 ↗
5. Material performance in helium-cooled systems10.1016/B978-0-08-056033-5.00099-9 ↗
6. Natesan · 2003
7. Characterization of elevated temperature properties of heat exchanger and steam generator alloys10.1016/j.nucengdes.2011.10.034 ↗
8. R.N. Wright, Summary of studies of aging and environmental effects on Inconel 617 and Haynes 230; INL/EXT-06-11750, 2006.
9. Mechanisms of high-temperature corrosion in helium containing small amounts of impurities. I. Theoretical and experimental characterization of the gas phase10.1007/BF00656642 ↗
10. Mechanisms of high-temperature corrosion in helium containing small amounts of impurities. II. Corrosion of the nickel-base alloy Inconel 61710.1007/BF00656643 ↗
11. Thermodynamic and kinetic aspects of the corrosion of high-temperature alloys in high-temperature gas-cooled reactor helium10.13182/NT84-A33441 ↗
12. High-temperature oxidation of Alloy 617 in helium containing part-per-million levels of CO and CO2 as impurities10.1007/s11661-011-0603-5 ↗
13. Carburization of W- and Re-rich Ni-based alloys in impure helium at 1000°C10.1016/j.corsci.2010.09.049 ↗
14. Mechanism of internal oxidation of Alloy 617 in He–CO–CO2 environments at 850°C
15. Effect of oxide grain structure on the high-temperature oxidation of Cr10.1007/BF00611694 ↗
16. On high temperature oxidation of chromium: II. Properties of formula and the oxidation mechanism of chromium10.1149/1.2129481 ↗
17. On high temperature oxidation of chromium I. Oxidation of annealed, thermally etched chromium at 800–1100°C10.1149/1.2129478 ↗
18. Chromium transport through Cr2O3 scales I. On lattice diffusion of chromium10.1007/BF00738381 ↗
19. Reoxidation of chromium with densified Cr2O3 Scales10.1007/BF00606196 ↗
20. Kofstad · 1988
21. The oxidation of TD NiC (Ni–20Cr–2 vol pct ThO2) between 900°C and 1200°C10.1007/BF02664238 ↗
22. The influence of grain-boundary segregation of Y in Cr2O3 on the oxidation of Cr metal10.1007/BF00665014 ↗
23. Microstructure, adhesion and growth kinetics of protective scales on metals and alloys10.1007/BF00656571 ↗
24. Evidence for the growth mechanism of Cr2O3 at low oxygen potentials10.1149/1.2120023 ↗
25. Growth mechanism of Cr2O3 scales: oxygen and chromium diffusion, oxidation kinetics and effect of yttrium10.1016/0921-5093(96)10173-8 ↗
26. Electronic transport in thermally grown Cr2O310.1007/BF00665668 ↗
27. A. Atkinson, T. R., Transport in Nonstoichiometric Oxides, in: G. Simkovich, V.S. Stubican (Eds.), NATO ASI Ser. B, 1984, p. 285.
28. Beitrag zur theorie des anlaufvorgangs10.1515/zpch-1933-2105 ↗
29. Self-diffusion in Cr2O3 III. Chromium and oxygen grain-boundary diffusion in polycrystals10.1080/01418619208201562 ↗
30. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
31. G. Gulsoy, G.S. Was, Enhanced oxygen diffusion within the internal oxidation zone of Alloy 617 in controlled impurity helium environments at 750–850°C, Metall. Mater. Trans. A. (in press).
32. Oxidation kinetics of some Nickel-based superalloy foils in humidified hydrogen and electronic resistance of the oxide scale formed Part II10.1149/1.1354611 ↗
33. Assessing the kinetics of high temperature oxidation of Inconel 617 in a dedicated HTR impure helium facility coupling thermogravimetry and gas phase chromatography10.1016/j.jnucmat.2013.06.012 ↗
34. Kinetics and mechanism of reaction between water vapor, carbon monoxide and a chromia-forming nickel base alloy10.1016/j.corsci.2012.09.045 ↗
35. Influence of hydrogen and water vapour on the kinetics of chromium oxide growth at high temperature10.1007/s11085-011-9246-6 ↗
36. Oxidation kinetics of some nickel-based superalloy foils and electronic resistance of the oxide scale formed in air Part I10.1149/1.1392454 ↗
37. Kubaschewski · 1993