Environmental degradation of fracture resistance in high-temperature water environments of low-alloy reactor pressure vessel steels with high sulphur or phosphorus contents

Z. Que, H.P. Seifert, P. Spätig, J. Holzer, A. Zhang, G.S. Rao, S. Ritter

Corrosion Science· Volume 154

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Integrity and embrittlement management of reactor pressure vessels (RPVs) in light-water reactors
2. Low temperature fracture properties of DIN 22NiMoCr37 steel in fine-grained bainite and coarse-grained tempered embrittled martensite microstructures10.1016/j.engfracmech.2007.07.023 ↗
3. "Reactor pressure vessel (RPV) components: processing and properties,"
4. Irradiation embrittlement of reactor pressure vessels (RPVs)
5. Irradiation embrittlement of cladding and HAZ of RPV steel
6. Stability of ferritic steel to higher doses: survey of reactor pressure vessel steel data and comparison with candidate materials for future nuclear systems10.1016/j.ijpvp.2014.06.001 ↗
7. Review of thermal ageing data and its application to operation reactor pressure vessels10.1016/0308-0161(93)90126-E ↗
8. Seifert · 2016
9. Effect of high-temperature water environment on the fracture behaviour of low-alloy RPV steels
10. High-temperature water effects on the fracture behaviour of low-alloy RPV steels
11. Environmental reduction effect of high temperature water and hydrogen on fracture resistance of low alloy reactor pressure vessel steels
12. Effect of dynamic strain ageing on environmental degradation of fracture resistance of low-alloy RPV steels in high-temperature water environments
13. Effect of high-temperature water and hydrogen on the fracture behavior of a low-alloy reactor pressure vessel steel10.1016/j.jnucmat.2016.05.033 ↗
14. Seifert · 2018
15. Nagumo · 2016
16. Gangloff · 2012
17. Effect of hydrogen on tensile behavior of low alloy steel in the regime of dynamic strain ageing
18. Combination of radiation and hydrogen damage of reactor pressure vessel materials10.1016/0308-0161(93)90057-Z ↗
19. Hydrogen-involved tensile and cyclic deformation behavior of low-alloy pressure vessel steel10.1007/s11661-004-0256-8 ↗
20. Effects of strain rate and temperature on tensile behavior of hydrogen-charged SA508 Cl.3 pressure vessel steel10.1016/S0921-5093(02)00737-2 ↗
21. The effect of an elevated temperature aqueous environment upon the J-controlled tearing of a low-alloy steel10.1016/S0308-0161(99)00054-X ↗
22. JR curves of the low alloy steel 20 MnMoNi 5 5 with two different sulphur contents in oxygen-containing high temperature water at 240 °C10.1016/0029-5493(94)90187-2 ↗
23. Reactor pressure vessel steel embrittlement under the combined action of neutron field and hydrogen
24. Small-angle neutron scattering study on the effect of hydrogen in irradiated reactor pressure vessel steels10.1016/j.jnucmat.2004.09.005 ↗
25. Hänninen · 1992
26. Effects of hydrogen on tensile properties of SA508 Cl.3 reactor pressure vessel steel at high temperature10.4028/www.scientific.net/MSF.475-479.4121 ↗
27. Corrosion and environmentally-assisted cracking of carbon and low-alloy steels
28. Seifert · 2006
29. Modelling of water and material chemistry effect on crack-tip chemistry and resulting crack growth kinetics
30. Ford · 1992
31. Status of research on environmentally assisted cracking in LWR pressure vessel steels10.1115/1.3265576 ↗
32. On the mechanisms of environment sensitive cyclic crack growth of nuclear reactor pressure vessel steels10.1016/0010-938X(83)90126-9 ↗
33. Sendai, JapanProc. 2nd Int. IAEA Specialist’s Meeting on Sub-Critical Crack Growth1985
34. Que · 2019
35. Grain boundary phosphorous segregation and its influence on the ductile brittle transition temperature in reactor pressure vessel steels
36. Effect of ageing on properties of pressure vessel steels10.1016/0001-6160(86)90179-3 ↗
37. Phosphorus segregation and intergranular embrittlement in thermally aged and neutron irradiated reactor pressure vessel steels10.1520/JAI100690 ↗
38. Review of phosphorus segregation and lntergranular embrittlement in reactor pressure vessel steels
39. Effect of thermal ageing on properties of pressure vessel low alloy steel
40. Investigation of temper embrittlement in reactor pressure vessel steels following thermal aging, irradiation, and thermal annealing
41. Strain-induced corrosion cracking of low-alloy steels in LWR systems - case histories and identification of conditions leading to susceptibility10.1016/0029-5493(86)90084-1 ↗
42. Emerging issues and fundamental processes in environmental cracking in hot water10.5006/1.3278483 ↗
43. Strain-induced corrosion cracking behaviour of low-alloy steels under boiling water reactor conditions10.1016/j.jnucmat.2008.06.035 ↗
44. Stress corrosion cracking of low-alloy reactor pressure vessel steels under boiling water reactor conditions10.1016/j.jnucmat.2007.03.048 ↗
45. Influences of the dynamic strain aging on the J–R fracture characteristics of the ferritic steels for reactor10.1016/j.nucengdes.2003.06.014 ↗
46. Investigation of dynamic strain aging in SA106 Gr.C piping steel10.1016/S0029-5493(97)00045-9 ↗
47. Effect of dynamic strain aging on mechanical and fracture properties of A516Gr70 steel10.1016/S0308-0161(99)00075-7 ↗
48. Effects of dynamic strain ageing on environment-assisted cracking of Low alloy pressure vessel and piping steels
49. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
50. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
51. Equilibrium segregation of phosphorus at grain boundaries of Fe–P, Fe–C–P, Fe–Cr–P, and Fe–Cr–C–P alloys10.1179/030634581790426877 ↗
52. Temper-Embrittlement in 15Cr2NiMoV Steel10.1016/0308-0161(92)90074-P ↗
53. Standard test method for measurement of fracture toughness
54. A.E399 · 2019
55. Effects of loading rate and temperature on J–R fracture resistance of an SA516-Gr.70 steel for nuclear piping10.1016/S0308-0161(99)00033-2 ↗
56. Effects of loading rate and temperature on J–R fracture resistance of an SA516-Gr.70 steel for nuclear piping10.1016/S0308-0161(99)00033-2 ↗
57. On the experimental calibration of a potential drop system for crack length measurements in a compact tension specimen10.1520/JTE12346J ↗
58. A comparison of theoretical and experimental methods of calibrating the electrical potential drop technique for crack length determination10.1007/BF01141259 ↗
59. Single-specimen test measurement of Ji and J-Δa with a pulsed D-C potential-drop technique
60. High resolution mapping of strains and rotations using Electron backscatter diffraction10.1179/174328406X130966 ↗