Abstract

Abstract Ni2Al3 and Ni2Al3/Ni-Re coatings deposited on Fe-Cr-Ni alloy were oxidized in dry and wet CO2 gas at 650 °C. Ni2Al3/Ni-Re coating shows higher oxidation resistance to both dry and wet CO2 gas than Ni2Al3 coating. It is attributed to the retarding effect of Ni-Re interlayer on interdiffusion between Ni2Al3 out-layer and substrate, which inhibits the subsequent inner oxidation during corrosion. θ-Al2O3 is found in α-Al2O3 scales of both coatings during wet CO2 corrosion. Water vapor accelerates the oxidation rate of both coatings in CO2 gas by promoting the formation of the fast growing θ-Al2O3 on the surface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Synthesis and stability of the austenite phase in mechanically alloyed Fe-Cr-Ni alloys10.1016/j.matlet.2016.10.084 ↗
2. Internal-external transition for the oxidation of Fe-Cr-Ni austenitic stainless steels in steam10.1007/BF00665267 ↗
3. Effect of water vapour on the oxidation of Fe-13Cr-5Ni martensitic alloy at 973K10.1016/j.corsci.2012.04.008 ↗
4. Impact of oxyfuel atmospheres H2O/CO2/O2 and H2O/CO2 on the oxidation of ferritic-martensitic and austenitic steels10.1016/j.corsci.2011.03.015 ↗
5. Mechanism of breakaway oxidation of Fe-Cr and Fe-Cr-Ni alloys in dry and wet carbon dioxide
6. Kinetics of breakaway oxidation of Fe-Cr and Fe-Cr-Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗
7. Water vapor effects on corrosion of Fe-Cr and Fe-Cr-Ni alloys containing silicon in CO2 gas at 818 ºC10.1007/s11085-015-9536-5 ↗
8. Water vapour effects on corrosion of Fe-Cr and Fe-Cr-Ni alloys containing cerium and manganese in CO2 gas at 818 °C10.1016/j.corsci.2014.08.029 ↗
9. Aluminide coating formation on nickel-base superalloys by pack cementation process10.1023/A:1012534220165 ↗
10. Corrosion resistance of chromised and aluminised coatings in wet CO2 gas at 650 °C10.1016/j.surfcoat.2017.03.028 ↗
11. Degradation kinetics at 650 °C and lifetime prediction of Ni2Al3/Ni hybrid coating for protection against high temperature oxidation of creep resistant ferritic steels10.1016/j.corsci.2011.06.022 ↗
12. Long term oxidation resistance and thermal stability of Ni-aluminide/Fe-aluminide duplex diffusion coatings formed on ferritic steels at low temperatures10.1016/j.intermet.2008.11.009 ↗
13. Oxidation behavior of nickel-base single-crystal superalloy with rhenium-base diffusion barrier coating system at 1,423 K in air10.1007/s11085-007-9079-5 ↗
14. Formation of a rhenium-base coating on a Nb-base alloy10.1023/A:1026075420438 ↗
15. Formation and oxidation behavior of a diffusion barrier-coating system on a Ni-Mo base alloy at 1,373 K in air10.1007/s11085-007-9078-6 ↗
16. Oxidation of Ni-Al-base electrodeposited composite coatings. I: oxidation kinetics and morphology at 800 °C10.1023/A:1013398830293 ↗
17. Oxidation of Ni-Al-base electrodeposited composite coatings. II: oxidation kinetics and morphology at 1000 °C10.1023/A:1013350914363 ↗
18. High-temperature oxidation behavior of aluminide coatings on a new cobalt-base superalloy in air10.1016/S0010-938X(00)00137-2 ↗
19. Corrosion resistance of chromised and aluminised coatings in wet CO2, gas at 650, ºC10.1016/j.surfcoat.2017.03.028 ↗
20. Inhibiting effect of Ni-Re interlayer between Ni-Al coating and steel substrate on interdiffusion and carburization10.1016/j.surfcoat.2017.12.065 ↗
21. Oxidation behavior of Ni-Al coating with and without a Ni-Re diffusion barrier in dry CO2 gas at 650 ºC10.1016/j.corsci.2019.01.021 ↗
22. Transient-alumina transformations during the oxidation of magnetron-sputtered CoCrAl nanocrystalline coatings10.1023/A:1026015101783 ↗
23. Long term oxidation resistance and thermal stability of Ni-aluminide/Fe-aluminide duplex diffusion coatings formed on ferritic steels at low temperatures10.1016/j.intermet.2008.11.009 ↗
24. The crystallographic template effect assisting the formation of stable α-Al2O3 during low temperature oxidation of Fe-Al alloys10.1016/j.corsci.2016.01.007 ↗
25. Localized epitaxial growth of α-Al2O3 thin films on Cr2O3 template by sputter deposition at low substrate temperature10.1063/1.1544442 ↗
26. Characterization of topologically close-packed phases in secondary reaction zone in a coated CMSX-4 single crystal Ni-based superalloy10.1007/s10853-012-6840-1 ↗
27. Formation of secondary reaction zones in diffusion aluminide-coated Ni-base single-crystal superalloys containing ruthenium10.1007/s11661-008-9534-1 ↗
28. Precipitation phases in the nickel-based superalloy DZ 125 with YSZ/CoCrAlY thermal barrier coating10.1016/j.jallcom.2011.05.102 ↗
29. Influence of water vapor on the oxidation behavior of aluminized coatings under low oxygen partial pressure10.1016/j.corsci.2011.07.045 ↗
30. Modeling of θ→α alumina lateral phase transformation with applications to oxidation kinetics of NiAl-based alloys10.1016/j.matdes.2016.10.001 ↗
31. Effect of rhenium addition to a nickel-base single crystal superalloy on isothermal oxidation of the aluminide coating10.1016/j.surfcoat.2004.05.008 ↗
32. Oxidation behavior and breakdown of an aluminide coating on DZ40M alloy at high temperatures10.1023/A:1010363916459 ↗