Theoretical and experimental analysis of selective oxide and nitride formation in Fe–Al alloys
Source abstract
Abstract
Selective oxidation experiments of four iron-aluminum model alloys, containing 1–8 wt.% Al, at temperatures up to 1285 °C have been performed. The total corrosion depth and composition of formed nitride and oxide phases have been analyzed by means of SEM/EDX and XRD. Experimental findings and the interplay between formed oxide and nitride phases were compared to theoretical predictions from numerical simulations and critically discussed. Conditions for the formation of a continuous oxide band underneath the sample surface will be highlighted, which represent a critical parameter window in industrial processes that may lead to severe mechanical damage during rolling.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. High strength Fe–Mn–(Al, Si) TRIP/TWIP steels development – properties – application10.1016/S0749-6419(00)00015-2 ↗
2. The influence of the substitution of Si by Al on the properties of cold rolled C–Mn–Si TRIP steels10.2355/isijinternational.39.813 ↗
3. Grabke · 2007
4. The oxidation behavior of Fe–Al alloys10.4028/www.scientific.net/MSF.461-464.799 ↗
5. Influence of S and AlN on hot ductility of high Al, TWIP steels10.1179/1743284711Y.0000000109 ↗
6. Pinning of austenite grain boundaries by AIN precipitates and abnormal grain growth10.1007/BF02646005 ↗
7. Selective oxidation and internal nitridation during high-temperature exposure of single-crystalline nickel-base superalloys10.1007/s11661-000-0051-0 ↗
8. The role of nitrogen in the corrosion of iron and steels10.2355/isijinternational.36.777 ↗
9. Modelling and experiment of selective oxidation and nitridation of binary model alloys at 700°C – the systems Fe, 1wt.%{Al, Cr, Mn, Si}10.1016/j.corsci.2014.06.049 ↗
10. FactSage thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
11. Modelling high temperature oxidation in iron-chromium systems: combined kinetic and thermodynamic calculation of the long-term behaviour and experimental verification10.1007/s11085-011-9252-8 ↗
12. Internal corrosion of engineering alloys: experiment and computer simulation10.1007/s11669-005-0040-5 ↗
13. A finite-difference model to predict 2D depletion profiles arising from high temperature oxidation of alloys10.1088/0965-0393/14/4/014 ↗
14. Modelling the thermal oxidation of ternary alloys – compositional changes in the alloy and the development of oxide phases10.1016/S1359-6454(03)00381-1 ↗
15. High-temperature oxidation of iron and the decay of wustite studied with in situ ESEM10.1023/A:1013346813454 ↗
16. Two-dimensional transition metal compounds with carbon, nitrogen and oxygen on bcc(100) metal and alloy surfaces10.1016/S0079-6786(98)00002-8 ↗
17. A novel laboratory set-up for investigating surface and interface reactions during short term annealing cycles at high temperatures10.1063/1.4817310 ↗
18. Thermogravimetry and insitu mass spectrometry at high temperatures compared to thermochemical modelling – the weight loss during selective decarburisation at 800°C10.1016/j.corsci.2013.09.015 ↗
19. The thermochemistry library ChemApp and its applications10.3139/146.101551 ↗
20. Solubility, permeability, and diffusivity of oxygen in solid iron
21. On the solubility of nitrogen in pure iron and in austenitic chromium-nickel-steels
22. Mehrer · 1990 · vol. 26
23. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
24. Reaktionstypen bei der Oxydation von Legierungen
25. The influence of the rate of oxidation upon the properties of internally oxidized silver-magnesium alloys
26. Temperature and gas composition dependence of internal oxidation kinetics of an Fe–10%Cr alloy in water vapour containing environments10.1002/maco.201005865 ↗
27. Observations of nodule growth during the oxidation of pure binary iron-aluminum alloys10.1007/BF00666643 ↗
28. Development of a comprehensive oxide failure diagram10.1007/s11085-009-9185-7 ↗
29. SiAlON Ceramics10.1111/j.1151-2916.1992.tb08175.x ↗
30. AlN formation in Fe–Al alloys in N2–O2 atmospheres10.1002/maco.201307257 ↗
31. Behavior of carbon in low temperature plasma nitriding layer of austenitic stainless steel10.1016/j.surfcoat.2004.08.179 ↗
32. Coupling diffusion and thermodynamics – exemplified for the gas nitriding of iron-chromium alloys10.3139/105.110096 ↗
33. Effect of water vapour on the oxidation of Fe–13Cr–5Ni martensitic alloy at 973K10.1016/j.corsci.2012.04.008 ↗
34. Internal-oxide-band formation during oxidation of Ag–Mg alloys10.1007/BF00665660 ↗
35. Anomalous behavior during internal oxidation and nitridation10.1007/BF03222725 ↗
36. The transition from internal to external oxidation and the formation of interruption bands in silver-indium alloys10.1016/0001-6160(61)90103-1 ↗
37. Internal oxidation of Cu–Pd and Cu–Pt alloys10.1016/S0010-938X(68)80142-8 ↗
38. Young · 2008
39. The influence of oxygen partial pressure on the kinetics of duplex scale formation on 316 stainless steel10.1016/0010-938X(82)90081-6 ↗