journal article·2013-12

The effect of a surface Cr film on the oxidation of SmCo-based magnetic alloy at 700°C

Z. Dong, X. Peng, Zh. Guo, W. Li, F. Wang

Corrosion Science· Volume 77
Publisher page

Abstract

Abstract A 4.5 μm-thick Cr film prepared by a double glow sputtering technique was deposited on a magnetic Sm(CobalFe0.22Cu0.08Zr0.02)7.5 alloy to improve its oxidation resistance. Oxidation tests in air at 700 °C indicate that the Cr film grew a Cr2O3 scale, profoundly preventing the oxidation of the SmCo-based alloy. The coated alloy only formed a ∼2.9 μm-thick internal-oxidation-affected zone (IOAZ) for 20 h. The mechanism for the formation of this IOAZ, together with its induced alloy magnetic phase transformation, is presented.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. High-performance permanent magnets10.1007/s001140050755 ↗
2. Micromagnetism and the microstructure of high-temperature permanent magnets10.1063/1.1809250 ↗
3. Recent progress in 2:17-type permanent magnets10.1007/BF02648616 ↗
4. Thermal stability of Sm–TM high temperature magnets at 300–550°C10.1109/20.908773 ↗
5. A new class of Sm-TM magnets for operating temperatures up to 550°C10.1109/20.908807 ↗
6. The oxidation morphology of SmCo alloy10.1016/j.jallcom.2009.07.115 ↗
7. The mechanism of high temperature oxidation of a SmCo-based magnetic alloy10.1016/j.corsci.2012.04.028 ↗
8. Thermal stability and the effectiveness of coatings for SmCo 2:17 high temperature magnets at temperatures up to 550°C10.1109/TMAG.2004.829323 ↗
9. Oxidation protection of Sm2Co17-based alloys10.1016/j.jallcom.2011.12.031 ↗
10. Effect of a thin Cr2O3 film on oxidation at 600°C of a Sm(CobalFe0.22Cu0.08Zr0.02)7.5 alloy10.1016/j.surfcoat.2013.03.031 ↗
11. A Cr2O3-deposited Sm(Co0.68Fe0.22Cu0.08Zr0.02)7.5 magnet with increased oxidation resistance at 700°C10.1016/j.corsci.2013.01.038 ↗
12. Twinning structure in Sm(Co, Fe, Cu, Zr)z permanent magnet10.1016/j.intermet.2010.02.008 ↗
13. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
14. Identification of the cell boundary phase in the isothermally aged commercial Sm(Co0.75Fe0.1Cu0.12Zr0.04)7.4 sintered magnet10.1016/j.scriptamat.2005.12.009 ↗
15. Cr-O (Chromium–Oxygen)10.1007/s11669-997-0072-0 ↗
16. Intense white-luminescence of Sm2O3 irradiated with ultraviolet laser light under vacuum10.1016/j.physb.2003.09.253 ↗
17. Enthalpies of formation of Sm2O3 (monoclinic) and Sm2O3 (cubic)10.1016/0021-9614(72)90083-3 ↗
18. Internal oxidation of Sm(CobalFe0.22Cu0.08Zr0.02)7.5 alloy at 700°C10.1016/j.corsci.2013.01.038 ↗
19. Barin · 1995
20. Uber die innere oxydation von metallegierungen10.1016/0001-6160(64)90036-7 ↗
21. CVM calculation of the ternary system Co–Cu–Fe10.1016/S0925-8388(00)01198-1 ↗
22. Co–Cu–Fe (cobalt–copper–iron)10.1007/s11669-004-0158-x ↗
23. Co–Fe–Zr (cobalt–iron–zirconium)10.1361/105497103770330820 ↗