Dissolution of magnetite coupled galvanically with iron in environmentally friendly chelant solutions
Source abstract
Abstract
Abstract The galvanic coupling between magnetite and iron in ethylenediaminedisuccinic acid (EDDS) solutions both with and without added iron(II) ions has been studied using electrochemical methods. The galvanic coupling accelerates the corrosion of iron due to the small shift in its potential in the anodic direction. At the same time, the potential of magnetite is cathodically polarized away from the potential range where the only faradaic process—the reductive dissolution of magnetite—takes place and results in a considerable decrease in its dissolution. Magnetite dissolves faster at the galvanic potential when [EDDS] ⩾ [Fe2+] whereas iron is affected to a much lesser extent. The ratio between the rates of dissolution of magnetite at the galvanic potential to that at its steady state potential tends to decrease at higher temperatures and at higher EDDS and Fe2+ concentrations. This study shows that temperature plays a decisive role in the dissolution of magnetite coupled to iron. To completely remove it from the iron surface, high temperatures should be used. Corrosion inhibitors have to be considered when high losses of the base metal cannot be tolerated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Iron oxide chemistry and applications · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Mehra · Clays Clay Miner. · 1960 · 7 · 31710.1346/CCMN.1958.0070122 ↗
2. van Oorschot · Earth Planet Sci. Lett. · 1999 · 167 · 28310.1016/S0012-821X(99)00033-3 ↗
3. Baumgartner · J. Chem. Soc. Dalton Trans. I · 1982 · 164910.1039/dt9820001649 ↗
4. Afonso · J. Colloid Interf. Sci. · 1990 · 138 · 7410.1016/0021-9797(90)90181-M ↗
5. Segal · J. Chem. Soc. Chem. Commun. · 1980 · 99110.1039/c39800000991 ↗
6. Allen · J. Chem. Soc. Trans. · 1988 · 1 · 355
7. Hidalgo · J. Chem. Soc. Faraday Trans. · 1988 · 1 · 910.1039/f19888400009 ↗
8. Borghi · Langmuir · 1991 · 7 · 165210.1021/la00056a018 ↗
9. Blesa · Inorg. Chem. · 1987 · 26 · 371310.1021/ic00269a019 ↗
10. Taxiarchou · Trans. Inst. Miner. Metall. Sect. (C) · 1998 · 107 · C37
11. Borghi · J. Colloid Interf. Sci. · 1989 · 130 · 29910.1016/0021-9797(89)90109-4 ↗
12. Rueda · Clays Clay Miner. · 1992 · 40 · 57510.1346/CCMN.1992.0400512 ↗
13. Shoesmith · Corros. Sci. · 1989 · 45 · 14910.5006/1.3577833 ↗
14. Shailaja · J. Nucl. Sci. Technol. · 1993 · 30 · 52410.3327/jnst.30.524 ↗
15. Kaplan · Mater. Perform. · 1984 · 40
16. Abdul-Latif · Ind. Eng. Chem. Res. · 1988 · 27 · 154810.1021/ie00080a035 ↗
17. Brouillette · Pulp Paper Canada · 1990 · 91 · 39
18. Bosholm · Kerntechnik · 1993 · 58 · 3710.1515/kern-1993-580115 ↗
19. Vorob’eva · Coke Chem. · 1991 · 5 · 38
20. Hoffmann · Mater. Perform. · 1997 · 56
21. Hur · J. Nucl. Mater. · 1995 · 224 · 17910.1016/0022-3115(95)00011-9 ↗
22. Williams · Chem. Britain · 1998 · 4 · 48
23. Takahashi · Biosci. Biotech. Biochem. · 1997 · 61 · 195710.1271/bbb.61.1957 ↗
24. Metsarinne · Chemosphere · 2001 · 45 · 94910.1016/S0045-6535(01)00022-4 ↗
25. Jones · Appl. Radiat. Isotop. · 2001 · 54 · 58710.1016/S0969-8043(00)00297-9 ↗
26. Pryor · J. Chem. Soc. · 1950 · 125910.1039/jr9500001259 ↗
27. Haruyama · Corros. Sci. · 1978 · 18 · 26310.1016/S0010-938X(78)80043-2 ↗
28. Gorichev · Russ. J. Phys. Chem. · 1981 · 55 · 1558
29. Bruyere · J. Electroanal. Chem. · 1985 · 182 · 14110.1016/0368-1874(85)85447-2 ↗
30. Plonski · J. Appl. Electrochem. · 1997 · 27 · 118410.1023/A:1018471617720 ↗
31. Abellà · Corros. Sci. · 1998 · 40 · 156110.1016/S0010-938X(98)00067-5 ↗
32. Plonski · J. Mater. Sci. Forum · 1995 · 185 · 64910.4028/www.scientific.net/MSF.185-188.649 ↗
33. S. Brunet, G. Turluer, in: Proceedings of the 5th European Symposium of Corrosion Inhibitors, Italy, Ferrara, September 1980, pp. 513–538.
34. S. Brunet, G. Pinard-Legry, G. Turluer, in: Proceedings of the 8th International Congress of Metallic Corrosion, Germany, Frankfurt am Main, Dechema 1981, pp. 1634–1639.
35. Mancey · J. Electrochem. Soc. · 1993 · 140 · 63710.1149/1.2056136 ↗
36. Al-Mayouf · Corrosion · 2002 · 58 · 51910.5006/1.3277643 ↗
37. Al-Mayouf · J. Nucl. Mater. · 2003 · 320 · 18410.1016/S0022-3115(03)00109-0 ↗
38. White · Geochim. Cosmochim. Acta · 1994 · 58 · 185910.1016/0016-7037(94)90420-0 ↗
39. Das · J. Appl. Electrochem. · 2003 · 33 · 33310.1023/A:1024187216639 ↗
40. Fetisov · Dokl. Phys. Chem. · 2003 · 388 · 5710.1023/A:1022543516218 ↗
41. Engell · Z. Phys. Chem. · 1956 · 7 · 15810.1524/zpch.1956.7.3_4.158 ↗
42. Vermilyea · J. Electrochem. Soc. · 1966 · 113 · 1067
43. Severa · 1991
44. Cornell · 1996
45. Prince · J. Nucl. Mater. · 2001 · 289 · 28110.1016/S0022-3115(01)00425-1 ↗
46. Borghi · J. Nucl. Mater. · 1996 · 229 · 11510.1016/0022-3115(95)00201-4 ↗
47. Sato · Corros. Sci. · 2000 · 42 · 195710.1016/S0010-938X(00)00014-7 ↗
48. Pourbaix · 1974
49. Bessone · Electrochim. Acta · 1983 · 28 · 17110.1016/0013-4686(83)85105-6 ↗
50. Blesa · Trends Inorg. Chem. · 1993 · 3 · 25
51. Fushimi · Corros. Sci. · 2002 · 44 · 61110.1016/S0010-938X(01)00093-2 ↗
52. Cumper · Corros. Sci. · 1982 · 22 · 55110.1016/0010-938X(82)90054-3 ↗
53. Buecker · Mater. Perform. · 2001 · 52