Abstract

Abstract A hydrophobic oxide film was formed on aluminium by anodizing followed by desiccation treatment. Films subjected to gradual heating and cooling exhibit larger water contact angles than samples exposed to fast heating and cooling at the same temperature. From SEM and Auger Electron Spectroscopic observations, the low wettability surface shows a regular porous morphology with no significant chemical composition differences due to the different treatments. The desiccation process improves the corrosion resistance, shown by immersion in NaCl. The change in morphology by the desiccation processes is considered a main reason to lower the wettability, which further affects the corrosion properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Shirtcliffe · Langmuir · 2005 · 21 · 93710.1021/la048630s ↗
2. Miyauchi · Nanotechnology · 2006 · 17 · 515110.1088/0957-4484/17/20/019 ↗
3. Fu · Appl. Surf. Sci. · 2008 · 255 · 177610.1016/j.apsusc.2008.06.018 ↗
4. Wang · Corros. Sci. · 2011 · 53 · 208010.1016/j.corsci.2011.02.025 ↗
5. Wang · Appl. Surf. Sci. · 2010 · 256 · 383710.1016/j.apsusc.2010.01.037 ↗
6. Zhang · Angew. Chem. Int. Ed. · 2008 · 47 · 246610.1002/anie.200704694 ↗
7. Wu · J. Colloid Interf. Sci. · 2008 · 326 · 47810.1016/j.jcis.2008.06.041 ↗
8. Yin · Appl. Surf. Sci. · 2008 · 255 · 297810.1016/j.apsusc.2008.08.088 ↗
9. Weibel · J. Phys. Chem. C · 2010 · 114 · 1321910.1021/jp103702d ↗
10. Hoar · 1959 · vol. II
11. Leach · Corros. Sci. · 1969 · 9 · 41310.1016/S0010-938X(69)80037-5 ↗
12. Thompson · Thin Solid Films · 1997 · 299 · 19210.1016/S0040-6090(96)09440-0 ↗
13. Garcia-Vergara · Corros. Sci. · 2007 · 49 · 377210.1016/j.corsci.2007.03.036 ↗
14. Asoh · Corros. Sci. · 2009 · 51 · 149610.1016/j.corsci.2008.11.018 ↗
15. Ma · Corros. Sci. · 2011 · 53 · 414110.1016/j.corsci.2011.08.023 ↗
16. Mombello · Sens. Actuators B · 2009 · 137 · 7610.1016/j.snb.2008.11.046 ↗
17. Jha · Mater. Lett. · 2009 · 63 · 145110.1016/j.matlet.2009.03.046 ↗
18. Jha · Nanotechnology · 2008 · 19 · 39560310.1088/0957-4484/19/39/395603 ↗
19. M. Zheng, H. Jha, M. Sakairi, in: Proceedings of the 12th International Conference on Aluminum Alloys, 2010, 2E-03.
20. M. Zheng, H. Jha, M. Sakairi, T. Kikuchi, in: Proceedings of the Fifth International Symposium on Marine Corrosion and Control, 2010, p. 283–289.
21. Zheng · Zairyo Kankyo · 2010 · 59 · 33510.3323/jcorr.59.335 ↗
22. Stephen D. Cramer, Bernard S. Covino, ASM Handbook Vol. 13A: Corrosion: Fundamentals, Testing, and Protection, ASM International, Ohio, USA, 2003, p. 736.10.31399/asm.hb.v13a.9781627081825 ↗
23. Wenzel · Ind. Eng. Chem. · 1936 · 28 · 98810.1021/ie50320a024 ↗
24. Cassie · Trans. Faraday Soc. · 1944 · 40 · 54610.1039/tf9444000546 ↗
25. Wang · Langmuir · 2008 · 24 · 1017410.1021/la801092y ↗
26. Young · 2008