IGSCC crack growth in simulated BWR environment – Effect of nitrogen content in non-sensitised and warm rolled austenitic stainless steel
Source abstract
Abstract
Effect of nitrogen level in strain hardened stainless steel (SS) on crack growth rate (CGR) in simulated boiling water reactor conditions has been the focus of this study. Type 304 LN stainless steel has been used in a warm rolled condition containing two different levels of nitrogen. Clear intergranular (IG) fracture was observed in both the stainless steels. The CGR increased 3 times in the stainless steel with higher level of nitrogen at all levels of dissolved oxygen and this was related to the increase in yield strength due to rolling and dynamic strain aging (DSA).
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Horn · Nucl. Eng. Des. · 1997 · 174 · 31310.1016/S0029-5493(97)00131-3 ↗
2. Weeks · Corros. Sci. · 1985 · 25 · 75710.1016/0010-938X(85)90009-5 ↗
3. Scott · Corros. Sci. · 1985 · 25 · 58310.1016/0010-938X(85)90001-0 ↗
4. Andresen · Corrosion · 1989 · 45 · 44810.5006/1.3582044 ↗
5. Intergranular cracking of AISI 316 NG stainless steel in BWR environment
6. Kain · Corrosion · 2002 · 58 · 1510.5006/1.3277301 ↗
7. Kain · J. Nucl. Mater. · 2004 · 334 · 11510.1016/j.jnucmat.2004.05.008 ↗
8. V. Kain, R. Samantray, S. Acharya, P.K. De, V.S. Raja, Influence of low-temperature sensitisation on stress corrosion cracking of SS 304 LN stainless steels, in: S.A. Shipilov, R.H. Jones, J.M. Olive, R.B. Rebak (Eds.), Environment-Induced Cracking of Materials: Prediction, Industrial Developments and Evaluation, Elsevier, Oxford, 2007, pp. 163–172. Proceedings of the International Conference on Environment Induced Cracking of Materials, EICM-2, held at Banff Centre, Elsevier, Alberta, Canada, September 19–23, 2004.
9. Characteristics of crack propagation through SCC under BWR conditions in stainless steels stabilized with titanium or niobium
10. Stress corrosion cracking of stabilized austenitic stainless steels in various types of nuclear power plants
11. Erve · Nucl. Eng. Des. · 1997 · 171 · 11310.1016/S0029-5493(96)01320-9 ↗
12. Beneke · Corros. Sci. · 1989 · 29 · 54310.1016/0010-938X(89)90006-1 ↗
13. Cracking data base as a basis for risk informed inspection
14. Progress in the mechanistic understanding of BWR SCC and its implication to the prediction of SCC growth behavior in plants
15. Wang · Corrosion · 2006 · 62 · 65110.5006/1.3278292 ↗
16. Andresen · J. Nucl. Mater. · 2008 · 383 · 9710.1016/j.jnucmat.2008.08.005 ↗
17. T.M. Angeliu, P.L. Andresen, E. Hall, J.A. Sutliff, S. Sitzman, Strain and microstructure characterization of austenitic stainless steel weld HAZ’s, Corrosion/2000, NACE, Paper no. 186 (2000).
18. R. Magdowski, M.O. Spiedel, Effect of cold work on the growth rates of stress corrosion cracks in structural materials of nuclear systems, Corrosion/1996, NACE, Paper no 112 (1996).
19. P.L. Andresen, M.L. Pollick, T.M. Angeliu, The deformation response of L-Grade stainless steels relative to IGSCC in 288°C water, Corrosion/98, NACE, Paper no. 135 (1998).
20. P.L. Andresen, T.M. Angeliu, W.R. Catlin, L.M. Young, R.M. Horn, Effect of deformation on SCC of unsensitised stainless steel, Corrosion/2000, NACE, Paper no. 203 (2000).
21. Andresen · Corros. Sci. · 1993 · 49 · 71410.5006/1.3316104 ↗
22. Lu · Corros. Sci. · 2008 · 50 · 69810.1016/j.corsci.2007.08.022 ↗
23. Ruther · Corrosion · 1988 · 44 · 79110.5006/1.3584950 ↗
24. P.L. Andresen, T.M. Angeliu, L.M. Young, Effect of martensite and hydrogen on SCC of stainless steels and alloy 600, Corrosion/2001, NACE, Paper no. 1228 (2001).
25. M. Akashi, G. Nakayama, H. Komatsu, S. Abe, Metallurgical factors influencing the susceptibility of non-sensitised stainless steel to intergranular stress corrosion cracking in high temperature, high purity water environments, Corrosion/99, NACE, Paper no. 451 (1999).
26. Was · Corrosion · 2007 · 63 · 1910.5006/1.3278331 ↗
27. T.M. Angeliu, P.L. Andresen, M.L. Pollick, The IGSCC behavior of L-grade stainless steels in 288°C water, Corrosion/97, NACE, Paper no. 97 (1997).
28. Andresen · Int. J. Pres. Ves. Pip. · 1994 · 59 · 6110.1016/0308-0161(94)90142-2 ↗
29. Ford · Corrosion · 1996 · 52 · 37510.5006/1.3292125 ↗
30. Satoh · J. Nucl. Mater. · 1998 · 258–263 · 205410.1016/S0022-3115(98)00421-8 ↗
31. Stoltz · Metall. Trans. A · 1980 · 11A · 103310.1007/BF02654717 ↗
32. Gavriljuk · Mater. Sci. Eng. A · 1999 · 271 · 1410.1016/S0921-5093(99)00272-5 ↗
33. Mullner · Mater. Sci. Eng. A · 1993 · 164 · 16410.1016/0921-5093(93)90655-X ↗
34. W. Wang, W. Yan, K. Yang, Y. Shan, Z. Jiang, J. Mater. Eng. Perfor. (2010). Available from: www.springerlink.com.
35. Soussan · Mater. Sci. Eng. A · 1991 · 142 · 16910.1016/0921-5093(91)90655-7 ↗
36. Simmons · Mater. Sci. Eng. A · 1996 · 207 · 15910.1016/0921-5093(95)09991-3 ↗
37. Palit · Corrosion · 1993 · 49 · 97910.5006/1.3316025 ↗
38. Olefjord · Corros. Sci. · 1996 · 38 · 120310.1016/0010-938X(96)00018-2 ↗
39. Mozhi · Corrosion · 1985 · 41 · 55510.5006/1.3582983 ↗
40. Eckel · Corrosion · 1970 · 26 · 25110.5006/0010-9312-26.8.351 ↗
41. Eckel · Corrosion · 1968 · 24 · 21810.5006/0010-9312-24.7.218 ↗
42. Mozhi · Corros. Sci. · 1987 · 27 · 25710.1016/0010-938X(87)90022-9 ↗
43. S. Roychowdhury, Unpublished results from Phd. Thesis, IGSCC of Nitrogen Containing Austenitic Stainless Steels in Simulated BWR Environment, Department of Metallurgical Engineering and Materials Science, Indian Institute of Technology, Bombay, Powai, Mumbai, to be approved in 2011.
44. Byrnes · Acta Metall. · 1987 · 35 · 185310.1016/0001-6160(87)90131-3 ↗
45. Simmons · Acta Mater. · 1997 · 45 · 246710.1016/S1359-6454(96)00343-6 ↗
46. Lu · Corros. Sci. · 2010 · 52 · 254710.1016/j.corsci.2010.03.027 ↗
47. Lu · Corros. Sci. · 2008 · 50 · 56110.1016/j.corsci.2007.08.005 ↗
48. P.L. Andresen, Effects of testing characteristics on observed SCC behavior in BWRs, Corrosion/98, NACE, Paper no. 137 (1998).
49. P.L. Andresen, L.M. Young, W.R. Catlin, R.M. Horn, Stress corrosion crack growth rate behavior of various grades of cold worked stainless steel in high temperature water, Corrosion/2002, NACE, Paper no. 2511 (2002).
50. Scott · J. Nucl. Mater. · 1994 · 21 · 10110.1016/0022-3115(94)90360-3 ↗
51. Andresen · Mater. Sci. Eng. A · 1988 · 103 · 16710.1016/0025-5416(88)90564-2 ↗
52. Shoji · Corros. Sci. · 2010 · 52 · 76910.1016/j.corsci.2009.10.041 ↗
53. Effects of yield strength, corrosion potential, stress intensity factor, silicon and grain boundary character on the SCC of stainless steels
54. Quantification of yield strength effects on IGSCC of austenitic stainless steels in high temperature water
55. Lo · Mater. Sci. Eng. R. · 2009 · 65 · 3910.1016/j.mser.2009.03.001 ↗
56. Karlsen · J. Nucl. Mater. · 2009 · 395 · 15610.1016/j.jnucmat.2009.10.047 ↗
57. Karaman · Acta Mater. · 2001 · 49 · 391910.1016/S1359-6454(01)00296-8 ↗
58. Byrives · Acta Metall. · 1987 · 35 · 185310.1016/0001-6160(87)90131-3 ↗
59. Newman · Corros. Sci. · 1987 · 27 · 82710.1016/0010-938X(87)90040-0 ↗
60. Ahila · Corros. Sci. · 1996 · 38 · 199110.1016/S0010-938X(96)00092-3 ↗
61. Takeda · Appl. Surf. Sci. · 2006 · 252 · 858010.1016/j.apsusc.2005.11.073 ↗
62. Vignal · Mater. Sci. Eng. A · 2001 · 303 · 17310.1016/S0921-5093(00)01843-8 ↗