journal article·2006-01

Complete protection of a passive film on iron from breakdown in a borate buffer containing 0.1M of Cl− by coverage with an ultrathin film of two-dimensional polymer

Kunitsugu Aramaki, Tadashi Shimura

Corrosion Science· Volume 48· Issue 1
Publisher page

Abstract

An ultrathin film of two-dimensional polymer was prepared on a passivated iron electrode by modification of a 16-hydroxyhexadecanoate ion HO(CH2)15CO2- self-assembled monolayer with 1,2-bis(triethoxysilyl)ethane (C2H5O)3Si(CH2)2Si(OC2H5)3 and octadecyltriethoxysilane C18H37Si(OC2H5)3. This film prevented passive film breakdown examined by potentiodynamic anodic polarization of the coated electrode in the borate buffer solution containing 0.1 M of Cl−. Neither current spikes nor the pitting potential was observed in the passive and transpassive regions of polarization curve. The anodic current density was decreased in these regions markedly, implying hindrance to permeation of Cl− and water through the film. Structure of the film was clarified by X-ray photoelectron and FTIR reflection spectroscopies and contact angle measurement with a drop of water. Electron-probe microanalysis of the passivated surface coated with the film after anodic polarization scanning up to the transpassive region revealed that the polymer film prevents pit initiation by an attack on the passive film with Cl−.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrochemical Analysis and Applications · Molecular Junctions and Nanostructures · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Aramaki · Corros. Sci. · 2003 · 45 · 263910.1016/S0010-938X(03)00071-4 ↗
2. Aramaki · Corros. Sci. · 2004 · 46 · 31310.1016/S0010-938X(03)00156-2 ↗
3. Pearson · J. Am. Chem. Soc. · 1963 · 85 · 353310.1021/ja00905a001 ↗
4. Aramaki · Zairyo-to-Kankyo · 1997 · 46 · 34210.3323/jcorr1991.46.342 ↗
5. Corros. Eng. · 1997 · 46 · 389
6. T. Shimura, K. Aramaki, in: Proc. 13th Asian-Pacific Corrosion Control Conference, Osaka University, Osaka, 2003, Paper No. Q-06.
7. Aramaki · Corros. Sci. · 2004 · 46 · 253310.1016/j.corsci.2003.08.003 ↗
8. Aramaki · Corros. Sci. · 2004 · 46 · 256310.1016/j.corsci.2004.01.024 ↗
9. Aramaki · Corros. Sci. · 2005 · 47 · 158210.1016/j.corsci.2004.07.046 ↗
10. Nozawa · Corros. Sci. · 1999 · 41 · 5710.1016/S0010-938X(98)00048-1 ↗
11. Aramaki · Corros. Sci. · 1999 · 41 · 171510.1016/S0010-938X(99)00008-6 ↗
12. Yamaguchi · Corros. Sci. · 1994 · 36 · 24110.1016/0010-938X(94)90156-2 ↗
13. Jones · 1982 · 191
14. Aramaki · J. Electrochem. Soc. · 1991 · 138 · 39410.1149/1.2085596 ↗
15. Sato · 1981 · vol. 4 · 193
16. Tackett · Appl. Spectrosc. · 1989 · 43 · 48310.1366/0003702894202931 ↗
17. Pawsey · Langmuir · 2000 · 16 · 329410.1021/la991273e ↗
18. Chen · Langmuir · 1989 · 5 · 97810.1021/la00088a017 ↗
19. Walczak · J. Am. Chem. Soc. · 1991 · 113 · 237010.1021/ja00007a004 ↗