journal article·2026-08

Role of grain boundary M23C6 and MC in hydrogen-induced cracking behavior of nickel-based alloy

Jiaxing Liu, Weiwei Xing, Mingjiu Zhao

Corrosion Science· Volume 268
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Catalysts for Methane Reforming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Hydrogen embrittlement of pipeline steels under gaseous and electrochemical charging: a comparative review on tensile properties10.1016/j.engfailanal.2024.108956 ↗
2. Overview of hydrogen-resistant alloys for high-pressure hydrogen environment: on the hydrogen energy structural materials10.1093/ce/zkad009 ↗
3. Differences between internal and external hydrogen effects on slow strain rate tensile test of iron-based superalloy A28610.1016/j.ijhydene.2021.10.178 ↗
4. Hydrogen in pipeline steels: Recent advances in characterization and embrittlement mitigation10.1016/j.jngse.2022.104709 ↗
5. Hydrogen embrittlement as a conspicuous material challenge─comprehensive review and future directions10.1021/acs.chemrev.3c00624 ↗
6. Review of the hydrogen embrittlement and interactions between hydrogen and microstructural interfaces in metallic alloys: Grain boundary, twin boundary, and nano-precipitate10.1016/j.ijhydene.2024.05.257 ↗
7. Hydrogen trapping and embrittlement in metals – a review10.1016/j.ijhydene.2024.04.076 ↗
8. Materials and corrosion trends in offshore and subsea oil and gas production10.1038/s41529-017-0003-4 ↗
9. Hydrogen embrittlement of nickel, cobalt and iron-based superalloys10.1533/9780857093899.3.624 ↗
10. Internal hydrogen effects on tensile properties of iron- and nickel-base superalloys10.1007/BF02782416 ↗
11. Influence of yttrium alloying on improving the resistance to hydrogen embrittlement of superalloy 71810.1016/j.ijhydene.2024.01.229 ↗
12. Hydrogen assisted intergranular cracking of alloy 725: the effect of boron and copper alloying10.1016/j.corsci.2022.110331 ↗
13. Combined thermal desorption spectroscopy, hydrogen visualization, HRTEM and EBSD investigation of a Ni–Fe–Cr alloy: the role of hydrogen trapping behavior in hydrogen-assisted fracture10.1016/j.msea.2022.143428 ↗
14. Characterising hydrogen induced cracking of alloy 625+ using correlative SEM - EDX and NanoSIMS10.1016/j.corsci.2020.109228 ↗
15. Strain localisation and failure at twin-boundary complexions in nickel-based superalloys10.1038/s41467-020-18641-z ↗
16. On the hydrogen embrittlement behavior of nickel-based alloys: Alloys 718 and 72510.1016/j.msea.2020.139785 ↗
17. The combined effects of hydrogen and aging condition on the deformation and fracture behavior of a precipitation-hardened nickel-base superalloy10.1016/j.actamat.2020.01.033 ↗
18. Effect of different microstructural features on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.ijhydene.2018.02.088 ↗
19. Tensile mechanical properties and fracture behaviors of nickel-based superalloy 718 in the presence of hydrogen10.1016/j.ijhydene.2018.08.179 ↗
20. Comprehensive effect of grain boundaries and grain boundary carbides on the hydrogen embrittlement of GH353610.1016/j.ijhydene.2023.10.150 ↗
21. The hydrogen-induced twin boundary cracking behavior in nickel-based alloy 625: Insights from secondary carbide dissolution10.1016/j.msea.2025.148624 ↗
22. Hydrogen environment embrittlement in nickel-base superalloy Alloy 61710.1016/j.ijhydene.2023.05.354 ↗
23. The influence of the processing route on the fragmentation of (Nb,Ti)C stringers and its role on mechanical properties and hydrogen embrittlement of nickel based alloy 71810.1016/j.ijhydene.2021.02.127 ↗
24. On the role of precipitates in hydrogen trapping and hydrogen embrittlement of a nickel-based superalloy10.1016/j.corsci.2018.10.019 ↗
25. The effect of carbide precipitation on the hydrogen-enhanced fracture behavior of alloy 69010.1007/s11661-998-0253-4 ↗
26. Unravelling the effect of F phase on hydrogen-assisted intergranular cracking in nickel-based Alloy 725: Experimental and DFT study10.1016/j.corsci.2023.111569 ↗
27. Multi-scale and spatially resolved hydrogen mapping in a Ni–Nb model alloy reveals the role of the δ phase in hydrogen embrittlement of alloy 71810.1016/j.actamat.2016.02.053 ↗
28. Microstructure and mechanical properties of nickel-based wrought superalloys under thermal-mechanical coupling: A review with Inconel 718, 625 as main cases10.1016/j.pnsc.2024.12.001 ↗
29. Role of γ′ characteristic on the hydrogen embrittlement susceptibility of Fe–Ni–Cr alloys10.1016/j.corsci.2015.09.003 ↗
30. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: The role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
31. Pronounced transition of crack initiation and propagation modes in the hydrogen-related failure of a Ni-based superalloy 718 under internal and external hydrogen conditions10.1016/j.corsci.2019.108186 ↗
32. Criteria for hydrogen-assisted crack initiation in Ni-based superalloy 71810.1016/j.actamat.2022.117789 ↗
33. Direct observation of individualhydrogen atoms at trapping sites ina ferritic steel10.1126/science.aal2418 ↗
34. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
35. Atom Probe Tomography for the Observation of Hydrogen in Materials: A Review10.1093/micmic/ozac005 ↗
36. Towards establishing best practice in the analysis of hydrogen and deuterium by atom probe tomography10.1093/mam/ozae081 ↗
37. Improving the hydrogen embrittlement resistance by straining the ferrite / cementite interfaces10.1016/j.actamat.2024.119850 ↗
38. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
39. Review of metal carbide nanoprecipitate effects on hydrogen embrittlement of high strength martensitic steel10.1108/ACMM-03-2022-2633 ↗
40. Hydrogen-assisted decohesion associated with nanosized grain boundary κ-carbides in a high-Mn lightweight steel10.1016/j.actamat.2022.118392 ↗
41. Effect of grain boundary carbide on hydrogen embrittlement in stable austenitic stainless steels10.2355/isijinternational.ISIJINT-2018-639 ↗
42. Abnormal difference of hydrogen-induced ductility loss in nickel-based alloy 625 at conventional and slow strain rate10.1016/j.ijhydene.2024.08.030 ↗
43. Hydrogen uptake in austenitic stainless steels by exposure to gaseous hydrogen and its effect on tensile deformation10.1016/j.corsci.2011.04.022 ↗
44. Observation of local hydrogen on nickel surfaces10.1007/BF02663321 ↗
45. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
46. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
47. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
48. Influence of heat treatment on Inconel 625 superalloy sheet: carbides, γ'', δ phase precipitation and tensile deformation behavior10.1016/j.jallcom.2022.167522 ↗
49. Effect of solution treatment temperature upon the microstructure and mechanical properties of hot rolled Inconel 625 alloy10.1007/s10853-020-04375-2 ↗
50. Tensile deformation modeling of a homogenized cast alloy 625: effects of large grain size10.1007/s11661-022-06666-6 ↗
51. Role of grain boundary carbides in cracking behavior of Ni base alloys10.5516/NET.07.2012.013 ↗
52. A nano-sized NbC precipitation strengthened FeCoCrNi high entropy alloy with superior hydrogen embrittlement resistance10.1016/j.corsci.2022.110636 ↗
53. First-Principles study of hydrogen solubility and embrittlement of Cr23C6 in nickel-based alloys10.1016/j.commatsci.2024.113304 ↗
54. Hydrogen retention behavior of primary precipitates in F82H steel: atomistic calculation based on the density functional theory10.1016/j.fusengdes.2020.111788 ↗
55. Mechanism of primary MC carbide decomposition in Ni-base superalloys10.1007/s11661-004-0076-x ↗
56. Microstructure of carbides at grain boundaries in nickel based superalloys10.1016/S1005-0302(12)60169-8 ↗
57. Formation of M23C6-type precipitates and chromium-depleted zones in austenite stainless steel10.1016/j.scriptamat.2011.06.010 ↗
58. Numerical analysis of hydrogen trap state by TiC and V4C3 in bcc-Fe10.2355/isijinternational.52.1693 ↗
59. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
60. A first-principles study on the hydrogen trap characteristics of coherent nano-precipitates in α-Fe10.1016/j.ijhydene.2020.07.123 ↗
61. First - principles study of hydrogen - carbide interaction in bcc Fe10.1016/j.ijhydene.2023.09.222 ↗
62. On the evolution of stresses due to lattice misfit at a Ni-superalloy and YSZ interface10.1016/j.surfin.2018.05.007 ↗
63. Principle of solid-state phase transformation
64. First-principles calculations and phenomenological modeling of lattice misfit in Ni-base superalloys10.1016/j.msea.2006.05.152 ↗
65. Synergistic evolution of MC/M23C6 carbides in a polycrystalline Ni-based superalloy during long-term aging: Elemental diffusion and interaction mechanisms10.1016/j.matchar.2025.115462 ↗
66. Predicting equilibrium shape of precipitates as function of coherency state10.1016/j.actamat.2012.04.019 ↗
67. Plastic deformation behavior and strengthening mechanism of SLM 316L reinforced by micro-TiC particles10.1016/j.msea.2023.145557 ↗
68. Grain boundary character correlated carbide precipitation and mechanical properties of Ni-20Cr-18W-1Mo superalloy10.1016/j.msea.2016.05.028 ↗
69. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
70. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
71. Nucleation and growth of carbo-nitride nanoparticles in α-Fe-based alloys and associated interfacial process10.1515/ntrev-2015-0032 ↗
72. Effects of annealing on microstructures and properties of cold-rolled GH3536 sheet10.1016/j.matchar.2021.111409 ↗
73. Effect of boron addition on hydrogen embrittlement sensitivity in Fe–Ni based alloys10.1016/j.msea.2010.06.073 ↗
74. Effect of boron on the hydrogen-induced grain boundary embrittlement in α-Fe10.1016/j.ijhydene.2017.11.083 ↗
75. Energetics and electronic structure of grain boundaries and surfaces of B- and H-doped Ni3Al10.1103/PhysRevB.67.224203 ↗
76. Equilibrium grain-boundary segregation and the effect of boron in B-doped Fe−3wt%Ni austenitic alloy10.1016/0956-7151(91)90290-H ↗