The influence of CO2 partial pressure on the hydrogen embrittlement behavior of pure iron in high-pressure hydrogen environment
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Hydrogen storage methods: review and current status10.1016/j.rser.2022.112743 ↗
2. Options of natural gas pipeline reassignment for hydrogen: cost assessment for a Germany case study10.1016/j.ijhydene.2020.02.121 ↗
3. Detecting hydrogen concentrations during admixing hydrogen in natural gas grids10.1016/j.ijhydene.2021.06.221 ↗
4. Gas detection of hydrogen/natural gas blends in the gas industry10.1016/j.ijhydene.2020.08.200 ↗
5. Hydrogen blending in gas pipeline networks—a review10.3390/en15103582 ↗
6. Thermodynamics of spontaneous dissociation and dissociative adsorption of hydrogen molecules and hydrogen atom adsorption and absorption on steel under pipelining conditions10.1016/j.ijhydene.2021.07.217 ↗
7. On the thermodynamics of adsorption at interfaces as it influences decohesion10.1007/BF02654514 ↗
8. Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels10.1007/s11661-001-0265-9 ↗
9. 9 - Metallographic and fractographic techniques for characterising and understanding hydrogen-assisted cracking of metals10.1533/9780857093899.2.274 ↗
10. Mobile effect of hydrogen on intergranular decohesion of iron: first-principles calculations10.1080/14786435.2011.645077 ↗
11. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
12. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
13. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
14. Prediction of hydrogen-assisted fracture under coexistence of hydrogen-enhanced plasticity and decohesion10.1016/j.ijhydene.2023.06.033 ↗
15. Hydrogen-prompted heterogeneous development of dislocation structure in Ni10.1016/j.actamat.2022.118660 ↗
16. Quantitative tests revealing hydrogen-enhanced dislocation motion in α-iron10.1038/s41563-023-01537-w ↗
17. Co-adsorption of H2+nCO+mO2 on α-Fe (110): effect on hydrogen adsorption, dissociation and diffusion10.1016/j.ijhydene.2023.09.017 ↗
18. Environmentally assisted fatigue crack propagation in steel10.1007/BF02661639 ↗
19. Inhibitory effect of oxygen on hydrogen-induced fracture of A333 pipe steel10.1111/ffe.12994 ↗
20. Coadsorption of CO and H2 on an iron surface and its implication on the hydrogen embrittlement of iron10.1021/acs.jpcc.9b06927 ↗
21. Use of existing steel pipeline infrastructure for gaseous hydrogen storage and transport: a review of factors affecting hydrogen induced degradation10.1016/j.jngse.2022.104534 ↗
22. Hydrogen uptake induced by CO2 enhances hydrogen embrittlement of iron in hydrogen blended natural gas10.1016/j.corsci.2022.110594 ↗
23. Effect of hydrogen gas impurities on the hydrogen dissociation on iron surface10.1002/qua.24633 ↗
24. A review of gas phase inhibition of gaseous hydrogen embrittlement in pipeline steels10.1016/j.ijhydene.2024.02.245 ↗
25. CO2 effect on the fatigue crack growth of X80 pipeline steel in hydrogen-enriched natural gas: experiment vs DFT10.1016/j.ijhydene.2024.04.116 ↗
26. Pressure dependence of CO2 effect on hydrogen-assisted fatigue crack growth in two pipeline steels10.1016/j.ijhydene.2024.10.032 ↗
27. Standard Test Method for Determination of Susceptibility of Metals to Embrittlement in Hydrogen Containing Environments at High Pressure, High Temperature, or Both. ASTM International, 2016.
28. Standard Practice for Slow Strain Rate Testing to Evaluate the Susceptibility of Metallic Materials to Environmentally Assisted Cracking 2021.
29. Standard Test Method for Measurement of Fatigue Crack Growth Rates.ASTM International, 2015.
30. Enhanced hydrogen embrittlement of steel by the premature hydrogen dissociation with the increasing inert gas pressure in hydrogen-containing mixtures10.1016/j.actamat.2023.119279 ↗
31. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
32. Permeability, solubility and diffusivity of hydrogen isotopes in stainless steels at high gas pressures10.1016/j.ijhydene.2006.05.008 ↗
33. A technique for the evaluation of hydrogen embrittlement characteristics of electroplating baths10.1149/1.2425894 ↗
34. Effect of heat treatment temperature on the hydrogen barrier properties of oxide films on the surface of X52 pipeline steel10.1016/j.corsci.2025.113085 ↗
35. QuantumATK: an integrated platform of electronic and atomic-scale modelling tools10.1088/1361-648X/ab4007 ↗
36. Unified approach for molecular dynamics and density-functional theory10.1103/PhysRevLett.55.2471 ↗
37. Self-consistent equations including exchange and correlation effects10.1103/PhysRev.140.A1133 ↗
38. Inhomogeneous electron gas10.1103/PhysRevB.7.1912 ↗
39. Ab initio pseudopotentials for electronic structure calculations of polyatomic systems using density-functional theory10.1016/S0010-4655(98)00201-X ↗
40. Basis set selection for molecular calculations10.1021/cr00074a002 ↗
41. Enhanced hydrogen embrittlement of low-carbon steel to natural gas/hydrogen mixtures10.1016/j.scriptamat.2020.08.011 ↗
42. Hydrogen-enhanced fatigue crack growth in a single-edge notched tensile specimen under in-situ hydrogen charging inside an environmental scanning electron microscope10.1016/j.actamat.2019.03.032 ↗
43. Analysis of hydrogen absorption under competitive adsorption conditions: effect of hexamethylenetetramine10.1149/1.1562594 ↗
44. Ab initio chemisorption studies of H on Fe(110)10.1016/0039-6028(95)00244-8 ↗
45. Processes of H2 adsorption on Fe(110) surface: a density functional theory study10.1016/j.apsusc.2014.01.028 ↗
46. Interpretation of hydrogen-assisted fatigue crack propagation in BCC iron based on dislocation structure evolution around the crack wake10.1016/j.actamat.2018.06.041 ↗
47. On the law of the diffusion of gases10.1016/0376-7388(94)00228-Q ↗
48. Content dependence of CO2 effect on the hydrogen embrittlement sensitivity of P110 steel for underground hydrogen storage: experiments and DFT calculations10.1016/j.engfailanal.2025.109808 ↗
49. The impact of impurity gases on the hydrogen embrittlement behavior of pipeline steel in high-pressure H2 environments10.3390/ma17092157 ↗
50. Hydrogen permeation and embrittlement susceptibility of X80 welded joint under high-pressure coal gas environment10.1016/j.corsci.2016.04.029 ↗
51. Effects of hydrogen blending ratios and CO2 on hydrogen embrittlement of X65 steel in high-pressure offshore hydrogen-blended natural gas pipelines10.1016/j.jmrt.2024.10.150 ↗