Experimental and modeling studies on the oxygen ingression behavior at the crevices of stainless steels in high-temperature water
Source abstract
Abstract
Experimental and modeling studies of the oxygen ingression at the crevices of stainless steels were conducted in high-temperature water (288°C). The limiting distance of oxygen ingression, d lim , was defined as the point beyond which the primary surface oxide changed (γ-Fe 2 O 3 –Fe 3 O 4 ), regardless of crevice gap, oxygen concentration, and time. In situ measurements revealed increased electrical conductivity around the d lim position indicating ion enrichment due to a differential oxygen concentration cell. d lim increased with increasing crevice gap, oxygen concentration, and immersion time. Modeling study suggested that oxide layer growth reduced anodic dissolution and slowed oxygen consumption , allowing oxygen ingression with time.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Hydrogen embrittlement and corrosion behaviors in metals · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. IAEA. Energy, Electricity and Nuclear Power Estimates for the Period up to 2050. International Atomic Energy Agency, Vienna, 2023. 〈https://doi.org/10.61092/iaea.e3qb-hsrr〉.10.61092/iaea.e3qb-hsrr ↗
2. Shah · 1993
3. Corrosion in the Nuclear Power Industry
4. Corrosion and Stress Corrosion Cracking of Austenitic Stainless Steels
5. Experience and assessment of stress corrosion cracking in L-grade stainless steel BWR internals10.1016/S0029-5493(97)00131-3 ↗
6. Stress corrosion cracking in low carbon stainless steel components in BWRs, E-journal
7. Experiences with austenitic steels in boilng water reactors10.1016/S0029-5493(96)01308-8 ↗
8. Emerging issues and fundamental processes in environmental cracking in hot water10.5006/1.3278483 ↗
9. Corrosion-assisted cracking of stainless and low-alloy
10. Facts and views on the role of anionic impurities, crack tip chemistry and oxide films in environmentally assisted cracking
11. Crevice chemistry and corrosion in high temperature water: a review10.1016/j.net.2024.03.010 ↗
12. Hydrazine and hydrogen coinjection to mitigate stress corrosion cracking of structural materials in boiling water reactors (VII)—effects of bulk water chemistry on ecp distribution inside a crack10.1080/18811248.2007.9711392 ↗
13. R.W. Staehle, Critical analysys of “Tight cracks” in: Proceedings of the 13th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors, Whistler, BC, 2007.
14. Crack tip microsampling and growth rate measurements in low-alloy steel in high-temperature water10.5006/1.3294365 ↗
15. The crack tip solution chemistry in sensitized stainless steel in simulated boiling water reactor water studied using a microsampling technique10.1080/18811248.2003.9715371 ↗
16. J. Kuniya, M. Yamamoto, S. Namatame, and S. Suzuki, Effects of Crevice Environment on the SCC Initiation of Alloy 600 and Ni Based Weld Metal in High Temperature Oxygenated Water, in: Proceedings of the 15th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors, Stevenson, WA, 2003. https://doi.org/10.1080/18811248.2003.9715371.10.1080/18811248.2003.9715371 ↗
17. Crevice corrosion of alloy 600 in high temperature aqueous environments10.5006/0010-9312-35.12.550 ↗
18. Some effects of electrolyte composition and heat treatment on the aqueous crevice corrosion of alloy 600 and type 304 stainless steel at 288C10.5006/0010-9312-36.9.447 ↗
19. The effect of hydrogen evolution on acidification in alloy 600 and 304 stainless steel crevices at 288C10.5006/0010-9312-36.10.544 ↗
20. Crevice corrosion of austenitic alloys in high-temperature water10.5006/1.3284889 ↗
21. Effects of potential on the electrical conductivity of a solution within a crevice of stainless steel in high-temperature water10.5006/3187 ↗
22. Stress corrosion cracking of iron and nickel based alloys in sulfate solutions at 289C10.5006/0010-9312-29.11.442 ↗
23. Effects of Cr and Mo content on the crevice corrosion of stainless steels in high temperature high purity water
24. T. Tsukada, M. Suzuki, K. Kiuchi, Y. Kaji, M. Kikuchi, F. Ueno, H. Ugachi, J. Nakano, Y. Miwa, N. Ebine, Y. Nishiyama, T. Motooka, C. Kato, Report of Examination of the Sample from Core Shroud (K1-H4) at the Kashiwazaki-Kariwa Nuclear Power Station Unit-1, JAERI-Tech 2004-011, 2004.
25. T. Tsukada, M. Suzuki, K. Kiuchi, Y. Kaji, M. Kikuchi, F. Ueno, H. Ugachi, J. Nakano, Y. Miwa, N. Ebine, Y. Nishiyama, T. Motooka, C. Kato, Report of Examination of the Sample from Core Shroud (O1-H2) at Onagawa Nuclear Power Station Unit-1, JAERI-Tech 2004-012, 2004.
26. T. Tsukada, M. Suzuki, K. Kiuchi, Y. Kaji, M. Kikuchi, F. Ueno, H. Ugachi, J. Nakano, Y. Miwa, N. Ebine, Y. Nishiyama, T. Motooka, and C. Kato, Report of Examination of the Sample from Core Shroud (2F3-H6a) at Fukushima Dai-ni Nuclear Power Station Unit-3, JAERI-Tech 2004-044, 2004.
27. D.J. Edwards, L.E. Thomas, K. Asano, S. Ooki and S.M. Bruemmer, Microstructure, Microchemistry and Stress Corrosion Crack Characteristics in a BWR 316LSS Core Shroud Weld, in: Proceedings of the 13th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors, Whistler, BC, 2007.
28. L. Thomas, D. Edwards, K. Asano, S. Ooki and S. Bruemmer, CRACK-TIP Characteristics in BWR Service Components, in: Proceedings of the 13th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors, Whistler, BC, 2007.
29. F. Cattant, The Underestimated Role of the Oxygen on RCS Components Failures, in: Proceeding of International Symposium Fontevraud 10, Avignon, France, 2002.
30. J.T.A. Roberts, Structural materials in nuclear power systems, Plenum Press, New York, 1981.10.1007/978-1-4684-7194-6 ↗
31. Effect of contaminants on resistance to stress corrosion cracking of Ni-Cr alloy 600 in pressurized water10.5006/0010-9312-21.1.1 ↗
32. Acceleration of Stress-Corrosion Cracking Test for High-Temperature, High-Purity Water Environments by Means of Artificial Crevice Application
33. Theoretical evaluation of the dissolved oxygen concentration in a crevice or crack in a metal in aqueous solution10.1179/000705980798275229 ↗
34. Multilayered surface oxides within crevices of type 316L stainless steels in high-temperature pure water10.5006/1106 ↗
35. Y. Soma, C. Kato, and F. Ueno, In Situ Electrochemical Study on Crevice Environment of Stainless Steel in High Temperature Water in: Proceedings of the 18th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors, Portland, OR, 2017.10.1007/978-3-030-04639-2_116 ↗
36. Temperature dependence of oxygen diffusion in H2O and D2O10.1021/jp952903y ↗
37. Oxidation BEhavior of 304 stainless steel during crevice corrosion in high-temperature pure water10.5006/1705 ↗
38. Effects of crevice geometry on corrosion behavior of 304 stainless steel during crevice corrosion in high temperature pure water10.1016/j.corsci.2016.04.049 ↗
39. Effects of temperature on stress corrosion cracking behavior of stainless steel and outer oxide distribution in cracks due to exposure to high-temperature water containing hydrogen peroxide10.1016/j.jnucmat.2013.10.031 ↗
40. Irradiation assisted stress corrosion cracking of 347 stainless steel in simulated PWR primary water containing lithium hydroxide or potassium hydroxide10.1016/j.jnucmat.2023.154676 ↗
41. Modelling of crack chemistry in sensitized stainless steel in boiling water reactor environments10.1016/S0010-938X(97)89342-0 ↗
42. M. Tachibana, Y. Wada, T. Arakawa, Y. Kikuchi, and T. Seto, Development of the Fundamental Multiphysics Analysis Model for Crevice Corrosion Using a Finite Element Method in: Proceedings of the 18th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors, Portland, OR, 2017.10.1007/978-3-030-04639-2_115 ↗
43. Simple and robust external reference electrodes for high-temperature electrochemical measurements10.5006/1.3277546 ↗
44. Vibrational spectroscopic characterization of hematite, maghemite, and magnetite thin films produced by vapor deposition10.1021/am1004943 ↗
45. Raman spectroscopy to unravel the magnetic properties of iron oxide nanocrystals for bio-related applications10.1039/C9NA00064J ↗
46. Raman spectroscopy of iron oxides and (oxy)hydroxides at low laser power and possible applications in environmental magnetic studies10.1111/j.1365-246X.2009.04122.x ↗
47. Characterization of oxide layers on SUS304 stainless steel by raman spectroscopy10.2355/tetsutohagane1955.79.1_48 ↗
48. Corrosion potential measurements on type 304 SS and alloy 182 in simulated BWR environments10.5006/1.3316038 ↗
49. Study of polarization curve measurement for type 304 stainless steel in BWR high temperature-high purity water10.1080/18811248.2007.9711514 ↗
50. Potential-pH diagrams for alloy-water systems under LWR conditions10.1016/0022-3115(93)90173-V ↗
51. Pourbaix diagrams for the ternary system of iron-chromium-nickel10.5006/1.3283945 ↗
52. Influence of oxygen concentration of 288°C water and alloy composition on the films formed on Fe-Ni-Cr alloys10.5006/1.3278328 ↗
53. Surface oxide layers on 316L stainless steel formed in 561 K pure water at different potentials10.1149/2.030208jes ↗
54. COMSOL documentation, 〈https://doc.comsol.com/6.2/docserver/#!/com.comsol.help.corr/corr_ug_electrochem.06.0〉.
55. Determining factors for anodic polarization curves of typical structural materials of boiling water reactors in high temperature – high purity water10.1080/00223131.2011.649077 ↗
56. Cathodic polarization curves of the oxygen reduction reaction on various structural materials of boiling water reactors in high temperature–high purity water10.1080/00223131.2012.676880 ↗
57. V12 OLI Studio/Analyzer User Guide. 〈https://support.olisystems.com/hc/en-us/article_attachments/29861127045011〉.
58. Study on kinetics of Fe (II) oxidized by air in FeSO4-H2SO4 solutions10.1016/j.mineng.2018.03.013 ↗
59. Kinetics of the ferrous iron-oxygen reaction in sulfuric acid solution10.1021/ja01600a004 ↗