journal article·2025-11

Suppressing gaseous hydrogen embrittlement of Cr–Mo steel by introducing water vapor: Insights from experiments and calculations

Juan Shang, Shunsuke Umezaki, Tatsuhito Masuda, Vanadia Irisca Yussalla, Hiroshi Okano, Inoue Naho, Aleksandar Staykov, Masanobu Kubota

Corrosion Science· Volume 256
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Natural hydrogen in the energy transition: fundamentals, promise, and enigmas10.1016/j.rser.2023.113888 ↗
2. Greenhouse gas reduction potential and cost-effectiveness of economy-wide hydrogen-natural gas blending for energy end uses10.1016/j.rser.2022.112962 ↗
3. Hydrogen blending in natural gas pipelines: a comprehensive review of material compatibility and safety considerations10.1016/j.ijhydene.2024.10.384 ↗
4. A review of hydrogen embrittlement in gas transmission pipeline steels10.1515/corrrev-2022-0052 ↗
5. Enhanced hydrogen degradation of two pipeline steels by increasing inert gas pressure in hydrogen-containing mixtures: experimental and theoretical insights10.1016/j.corsci.2024.112466 ↗
6. Hydrogen embrittlement as a conspicuous material challenge─comprehensive review and future directions10.1021/acs.chemrev.3c00624 ↗
7. Effect of hydrogen gas impurities on the hydrogen dissociation on iron surface10.1002/qua.24633 ↗
8. Inhibitory effect of oxygen on hydrogen-induced fracture of A333 pipe steel10.1111/ffe.12994 ↗
9. Assessing the effect of low oxygen concentrations in gaseous hydrogen embrittlement of DIN 1.4301 and 1.1200 steels at high gas pressures10.1016/j.corsci.2012.08.015 ↗
10. Elucidating the variables affecting accelerated fatigue crack growth of steels in hydrogen gas with low oxygen concentrations10.1016/j.actamat.2013.07.001 ↗
11. Coadsorption of CO and H2 on an iron surface and its implication on the hydrogen embrittlement of iron10.1021/acs.jpcc.9b06927 ↗
12. Inhibiting effect of carbon monoxide on gaseous hydrogen embrittlement of pipelines transporting hydrogen10.1016/j.corsci.2023.111789 ↗
13. The inhibitory effect of carbon monoxide contained in hydrogen gas environment on hydrogen-accelerated fatigue crack growth and its loading frequency dependency10.1016/j.ijhydene.2019.09.146 ↗
14. Mitigation of hydrogen embrittlement of iron and steels by carbon monoxide in gaseous H2
15. Material defects, gas purity and hydrogen embrittlement10.1016/0360-3199(85)90087-4 ↗
16. Control of hydrogen embrittlement of metals by chemical inhibitors and coatings
17. A review of gas phase inhibition of gaseous hydrogen embrittlement in pipeline steels10.1016/j.ijhydene.2024.02.245 ↗
18. Feasibility of the use of gas phase inhibition of hydrogen embrittlement in gas transmission pipelines carrying hydrogen: a review10.1007/s11837-022-05559-8 ↗
19. CO2 effect on the fatigue crack growth of X80 pipeline steel in hydrogen-enriched natural gas: experiment vs DFT10.1016/j.ijhydene.2024.04.116 ↗
20. Pressure dependence of CO2 effect on hydrogen-assisted fatigue crack growth in two pipeline steels10.1016/j.ijhydene.2024.10.032 ↗
21. S. Fukuyama, K. Yokogawa, Prevention of hydrogen environmental assisted crack growth of 2.25Cr-Mo steel by gaseous inhibitors, 1992. 〈https://www.osti.gov/etdeweb/biblio/6626516〉.
22. Hydrogen-induced slow crack growth of a plain carbon pipeline steel under conditions of cyclic loading
23. Effect of water vapour and H2S content on the hydrogen embrittlement sensitivity of low alloy steels for underground storage10.1016/j.ijhydene.2024.02.331 ↗
24. Data and prediction of water content of high pressure nitrogen, methane and natural gas10.1016/j.fluid.2006.12.018 ↗
25. Kidnay · 2019
26. Corrosion fatigue crack growth of AISI 4340 steel10.1016/j.ijfatigue.2012.10.015 ↗
27. Fracture mechanics and surface chemistry studies of subcritical crack growth in AISI 4340 steel10.1007/BF02652220 ↗
28. The effects of partial pressure and strain rate on water vapor- and hydrogen gas-induced embrittlement of Co3Ti alloys10.1016/S1359-6454(97)00091-8 ↗
29. ASTM E647. Standard test method for measurement of fatigue crack growth rates, 2015.
30. Inhomogeneous electron gas10.1103/PhysRev.136.B864 ↗
31. Self-consistent equations including exchange and correlation effects10.1103/PhysRev.140.A1133 ↗
32. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
33. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
34. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
35. VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data10.1107/S0021889811038970 ↗
36. A climbing image nudged elastic band method for finding saddle points and minimum energy paths10.1063/1.1329672 ↗
37. Effects of stress concentration on the mechanical properties of X70 in high-pressure hydrogen-containing gas mixtures10.1016/j.ijhydene.2020.02.125 ↗
38. A coupled cohesive modeling approach for predicting fractures in low alloy steel under high-pressure hydrogen gas10.1016/j.ijhydene.2020.10.064 ↗
39. Current challenges in the utilization of hydrogen energy-a focused review on the issue of hydrogen-induced damage and embrittlement10.1016/j.adapen.2024.100168 ↗
40. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
41. Effect of mechanical strength on the hydrogen embrittlement susceptibility and fracture behavior of a modified AISI 4130 steel
42. Transition mechanism of cycle- to time-dependent acceleration of fatigue crack-growth in 0.4%C Cr-Mo steel in a pressurized gaseous hydrogen environment10.1016/j.ijfatigue.2022.107039 ↗
43. Effects of hydrogen pressure and test frequency on fatigue crack growth properties of Ni–Cr–Mo steel candidate for a storage cylinder of a 70 MPa hydrogen filling station10.1016/j.engfracmech.2011.09.007 ↗
44. The slow fatigue crack growth and threshold behaviour of a medium carbon alloy steel in air and vacuum10.1016/0013-7944(75)90067-3 ↗
45. The influence of environment and stress ratio on fatigue crack growth at near threshold stress intensities in low-alloy steels10.1016/0013-7944(80)90078-8 ↗
46. Coverage dependent water dissociative adsorption on Fe(110) from DFT computation10.1039/C5CP00044K ↗
47. High coverage water aggregation and dissociation on Fe(100): a computational analysis10.1021/jp5081675 ↗
48. Adsorption of a water molecule on Fe(100): Density-functional calculations10.1103/PhysRevB.81.115460 ↗
49. Enhanced hydrogen embrittlement of steel by the premature hydrogen dissociation with the increasing inert gas pressure in hydrogen-containing mixtures10.1016/j.actamat.2023.119279 ↗
50. Co-adsorption of H2+nCO+mO2 on α-Fe (110): effect on hydrogen adsorption, dissociation and diffusion10.1016/j.ijhydene.2023.09.017 ↗