Corrosion behavior of Laves precipitates in FeCrAl-1Nb alloy at 290 °C and 7 MPa: The size effect and critical role of pH

Yunhan Hu, Yunhan Ling, Weipeng Wang, Fan Zhao, Zhengjun Zhang

Corrosion Science· Volume 240
Publisher page

Abstract

The corrosion behavior of Laves precipitates in FeCrAl-1Nb alloy was investigated in four different deoxygenated solutions at 290 °C and 7 MPa. The Laves precipitates exhibit potential size effect during corrosion in a weak alkaline solution: the microscale precipitates undergo oxidation with amorphization and element dissolution, and these phenomena are not observed in nanoscale precipitates. The corrosion of nanoscale precipitates is less insensitive to slight changes in pH; however, micro-galvanic corrosion was observed between some nanoscale precipitates and the ferrite phase. Deuterium isotope labeling experiments observed hydrogen enrichment in some oxidized precipitates.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Advanced oxidation-resistant iron-based alloys for LWR fuel cladding10.1016/j.jnucmat.2013.06.041 ↗
2. High temperature oxidation of fuel cladding candidate materials in steam–hydrogen environments10.1016/j.jnucmat.2013.05.047 ↗
3. Radioactivity release from the Fukushima accident and its consequences: a review10.1016/j.pnucene.2014.02.013 ↗
4. FeCrAl—iron–chromium–aluminum monolithic alloys – ScienceDirect10.1016/B978-0-12-817503-3.00005-5 ↗
5. K.G. Field, M.A. Snead, Y. Yamamoto, K.A. Terrani, Handbook on the Material Properties of FeCrAl Alloys for Nuclear Power Production Applications (FY18 Version: Revision 1). Oak Ridge National Lab.(ORNL), Oak Ridge, TN (United States), 2018.10.2172/1474581 ↗
6. In-situ tube burst testing and high-temperature deformation behavior of candidate materials for accident tolerant fuel cladding10.1016/j.jnucmat.2015.08.030 ↗
7. Micromechanical aspects of deformation and failure of advanced iron-chromium-aluminum alloys10.1016/j.mtla.2022.101592 ↗
8. Trifunctional Laves precipitates enabling dual-hierarchical FeCrAl alloys ultra-strong and ductile10.1016/j.ijplas.2022.103438 ↗
9. B. Qff. Strengthening mechanism of Nb addition in Fe–13Cr–4.5Al–2Mo alloys assessed by internal friction measurement
10. Effects of Nb-doping on the mechanical properties and high-temperature steam oxidation of annealing FeCrAl fuel cladding alloys
11. Development and property evaluation of nuclear grade wrought FeCrAl fuel cladding for light water reactors10.1016/j.jnucmat.2015.10.019 ↗
12. Effects of Nb addition and heat treatment on the microstructure, mechanical property and internal friction behavior of FeCrAlMo cladding alloys10.1016/j.jnucmat.2022.154044 ↗
13. Effects of Laves phase particles on recovery and recrystallization behaviors of Nb-containing FeCrAl alloys10.1016/j.actamat.2017.11.027 ↗
14. Plasticity improvement of Fe-13Cr-6Al-2Mo-0.5Nb alloy with yttrium addition by hindering Laves phase precipitation10.1016/j.matchar.2020.110647 ↗
15. Study on high temperature creep behavior of the accident-resistant cladding Fe–13Cr–4Al-1.85Mo-0.85Nb alloy10.1016/j.msea.2020.140688 ↗
16. Effects of annealing temperature on the microstructure, textures and tensile properties of cold-rolled Fe–13Cr–4Al alloys with different Nb contents10.1016/j.msea.2020.140236 ↗
17. Effect of niobium content on irradiation microstructure and hardening in FeCrAl-based alloys10.1016/j.jmst.2021.04.020 ↗
18. Effect of Nb content on the precipitation behaviors of Fe-Cr-Al fuel cladding alloys during long-term aging at 475 °C10.1016/j.msea.2021.141890 ↗
19. Synergistic effect of Laves phase evolution and porosity defects in nuclear-grade FeCrAl alloy laser welded joints: experiments and crystal plasticity modeling10.1016/j.optlastec.2022.108694 ↗
20. Effect of Nb on the surface composition of FeCrAl alloys after anodic polarization10.1016/j.matdes.2022.110728 ↗
21. Evolution of microstructure, mechanical and corrosion properties of Fe-13Cr-4Al-1.5Nb alloy aged at 450 °C10.1016/j.jmrt.2023.05.016 ↗
22. Exploring the high-temperature steam oxidation behaviors of the lean-Cr (7–10 wt%) FeCrAl alloys10.1016/j.corsci.2021.109927 ↗
23. Hydrothermal corrosion of latest generation of FeCrAl alloys for nuclear fuel cladding10.3390/ma17071633 ↗
24. Effects of Nb and Mo on 1200 °C steam oxidation and mechanical properties of FeCrAl alloys for fuel cladding materials10.1007/s11665-023-08232-6 ↗
25. Oxidation characteristics of Fe22Cr5Al3Mo-xNb alloys in high temperature steam10.1016/j.corsci.2021.109722 ↗
26. Effect of yttrium addition on nonmetallic inclusions in FeCrAl alloys10.1002/srin.202300212 ↗
27. Dynamic precipitation of laves phase in FeCrAl alloy with Zr addition10.1002/srin.202300015 ↗
28. Initial microzonal corrosion mechanism of inclusions associated with the precipitated (Ti, Nb)N phase of Sb-containing weathering steel10.1016/j.corsci.2019.108232 ↗
29. Microstructural understanding of general and localized corrosion of Fe13Cr4Al2Mo1.2Nb alloy in high temperature aerated water and superheated steam10.1016/j.corsci.2022.110341 ↗
30. Addition of niobium in Fe-13Cr-4.5 Al-2Mo alloy used as ATF cladding: effect on high temperature water corrosion and in-situ electrochemistry10.1016/j.matdes.2022.110854 ↗
31. Corrosion of FeCrAl-1 Nb alloy in deaerated water at 290 °C and 7 MPa: the oxidation behavior of grain boundary10.1016/j.corsci.2024.112159 ↗
32. Hydrogen embrittlement of FeCrAl alloys: the significant role of Laves phase and AlN particles10.1016/j.msea.2024.146292 ↗
33. Development of low-Cr wrought FeCrAl cladding alloys and its irradiation tolerance and steam oxidation resistance at 1200 °C10.1016/j.corsci.2021.109998 ↗
34. Grain structure and intermetallic evolution of Nb-containing FeCrAl alloy treated by cryogenic laser quenching10.1016/j.jallcom.2023.173050 ↗
35. Mechanistic study of incipient corrosion for nuclear grade lean-Cr FeCrAl alloys in a simulated PWR environment10.1016/j.matdes.2023.111948 ↗
36. Reassessment of oxidation-induced amorphization and dissolution of Nb precipitates in Zr-Nb nuclear fuel cladding tubes10.1016/j.actamat.2017.01.032 ↗
37. Analysis of the oxidized surface of 90Nb-10Zr alloy after exposure to lithiated water with 0.01 M LiOH at 360 °C/18.6 MPa10.1016/j.corsci.2015.12.019 ↗
38. Analysis of blister-like morphology on the oxide film of Zr-1Nb alloy corroded in lithiated water10.1016/j.corsci.2020.109075 ↗
39. Formation of Ti–Zr–Cu–Ni bulk metallic glasses10.1063/1.360537 ↗
40. Effect of the atomic size distribution on glass forming ability of amorphous metallic alloys10.1016/S0025-5408(01)00715-2 ↗
41. Uniform corrosion of FeCrAl alloys in LWR coolant environments10.1016/j.jnucmat.2016.06.047 ↗
42. The mechanism of high temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
43. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
44. Corrosion behavior of stainless steels in simulated PWR primary water: the effect of composition and matrix phases10.1016/j.corsci.2020.108991 ↗
45. Hydrothermal corrosion of 2nd generation FeCrAl alloys for accident tolerant fuel cladding10.1016/j.jnucmat.2020.152221 ↗
46. Early corrosion behaviour of irradiated FeCrAl alloy in a simulated pressurized water reactor environment10.1016/j.corsci.2020.108824 ↗
47. Diffusion in oxides10.2138/rmg.2010.72.17 ↗
48. Point defects and transport in non-stoichiometric oxides: solved and unsolved problems10.1016/S0022-3697(97)00205-9 ↗
49. Effect of molybdenum on the oxidation resistance of FeCrAl alloy in lower temperature (400 °C) and higher temperature (1200 °C) steam environments
50. Self-diffusion and impurity diffusion in oxides10.1007/BF00552089 ↗
51. Point defects and transport properties of binary and ternary oxides10.1016/0167-2738(84)90126-7 ↗
52. Point defects and transport in haematite (Fe2O3-ε)10.1080/01418619308213994 ↗
53. Oxide-based protonic conductors: point defects and transport properties10.1016/S0167-2738(01)00951-1 ↗