Iron oxide fluxing and precipitation in sulphate deposits during heat-resistant alloy corrosion in simulated combustion gas
Source abstract
Abstract
Two ferritic alloys, Fe-25Cr and Fe-25Cr-2Mn-1Si, and two austenitic alloys, Fe-25Cr-20Ni and 310SS, coated with a thin film of Na2SO4-K2SO4 mixture were exposed to a flowing wet CO2 gas at 650 and 750 °C for up to 300 h. In addition to oxide scaling, a new manifestation of Fe oxide fluxing into the salt layer was observed. The effects of alloy composition and reaction temperature on this phenomenon were determined. The process is attributed to formation of a low melting Na2O-Na2SO4 solution in the early stages of reaction, followed by basic fluxing of FeO and/or Fe3O4.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Oxy-fuel combustion technology for coal-fired power generation10.1016/j.pecs.2005.07.001 ↗
2. F. Chatel-Pelage, O. Marin, N. Perrin, R. Carty, G.R. Philo, H. Farzan, S.J. Vecci, A pilot-scale demonstration of oxy-combustion with flue gas recirculation in a pulverized coal-fired boiler, in: Proceedings of the Twenty Eightth International Technical Conference on Coal Utilization & Fuel Systems, 2003, Clearwater, FL.
3. Techno-economic study of CO2 capture from an existing coal-fired power plant: MEA scrubbing vs. O2/CO2 recycle combustion10.1016/S0196-8904(03)00040-2 ↗
4. Fireside issues in advanced power generation systems10.1179/1743284712Y.0000000133 ↗
5. Materials challenges in advanced coal conversion technologies10.1557/mrs2008.64 ↗
6. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe–Cr and Fe–Cr–X alloys10.1007/s11085-010-9215-5 ↗
7. Mechanism of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide
8. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
9. Scale formation mechanisms of martensitic steels in high CO2/H2O-containing gases simulating oxyfuel environments10.3184/096034009X438185 ↗
10. Fireside corrosion of superheaters: effects of air and oxy-firing of coal and biomass10.1016/j.fuel.2011.03.010 ↗
11. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
12. Invited review paper in commemoration of over 50 years of oxidation of metals: current aspects of deposit-induced corrosion10.1007/s11085-020-10015-6 ↗
13. Determination of the initiation and propagation mechanism of fireside corrosion10.1007/s11085-015-9559-y ↗
14. Fireside corrosion of P92 steel with mixed sulfate deposit at 650 °C10.1007/s11085-020-09994-3 ↗
15. Fireside corrosion in oxy-fuel combustion of coal10.1007/s11085-013-9399-6 ↗
16. Current limitations of high-temperature alloys in practical applications10.1007/BF01046730 ↗
17. Possible scenarios for the causes of accelerated fireside corrosion of superheater tubes in coal-fired boilers10.1080/09603409.2017.1334351 ↗
18. Reid · 1971
19. Fireside issues in advanced power generation systems10.1179/174892408X373509 ↗
20. Effect of pre-oxidation on hot corrosion resistance of HR3C stainless steel in sulfate salt with or without Fe2O310.1016/j.corsci.2021.109789 ↗
21. Effects of sulphate deposits on corrosion behaviour of Fe-based alloys in wet CO2 gas at 750 °C10.1007/s11085-020-10010-x ↗
22. Hot corrosion type II of FeCr-based model alloys for boiler and heat exchanger applications10.1002/maco.201810640 ↗
23. Effects of silicon and water vapour on corrosion of Fe–20Cr and Fe–20Cr–20Ni alloys in CO2 at 650 °C10.1007/s11085-016-9681-5 ↗
24. T.D. Nguyen, J. Zhang, D. Young, Water Vapor Effects on Corrosion of Fe–Cr and Fe–Cr–Ni Alloys Containing Silicon in CO2 Gas at 818 °C, 2015, 83.10.1007/s11085-015-9536-5 ↗
25. Corrosion behaviour of Fe-25Cr alloy in wet CO2 gas at 650 °C: Effects of chloride deposits and Si+Mn alloying addition10.1016/j.corsci.2021.110001 ↗
26. Effects of cerium and manganese on corrosion of Fe–Cr and Fe–Cr–Ni alloys in Ar–20CO2 and Ar–20CO2–20H2O gases at 650 °C10.1016/j.corsci.2015.08.012 ↗
27. Compositional changes in the underlying alloy during the protective oxidation of alloys10.1016/0001-6160(67)90173-3 ↗
28. Theoritical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
29. Reaktionstypen bei der oxydation von Legierungen
30. Diffusion of chromium in α-iron10.1002/pssa.2210900219 ↗
31. Volume and grain-boundary diffusion in 20 Cr/25 Ni/Nb stainless steel10.1179/msc.1969.3.1.93 ↗
32. Chemical volume diffusion coefficients for stainless steel corrosion studies10.1007/BF01161455 ↗
33. FactSage thermochemical software and databases, 2010–201610.1016/j.calphad.2016.05.002 ↗
34. Electrical conductivity of Na2SO4(I)10.1016/0167-2738(85)90136-5 ↗
35. The mechanism of sodium sulphate-induced low temperature hot corrosion of pure iron10.1016/0010-938X(90)90042-4 ↗
36. Na2SO4-induced accelerated oxidation (hot corrosion) of nickel10.1007/BF02642794 ↗
37. Accelerated oxidation of iron induced by Na2SO4 deposits in oxygen at 750°C—a new type low-temperature hot corrosion.10.1007/BF00665265 ↗
38. On the possibility of a Na2SO4-Na2O eutectic melt developing on metals coated with Na2SO4 deposit in oxygen/air at intermediate temperatures.10.1016/0010-938X(95)00032-F ↗
39. Über die thermischen Verhältnisse im System Natrium–Schwefel–Sauerstoff10.1002/zaac.19552810106 ↗
40. Solubility of α ‐ Fe2O3 in Fused Na2SO4 at 1200 K10.1149/1.2113943 ↗
41. Solubilities of α ‐ Fe2O3 and Fe3O4 in Fused Na2SO4 at 1200 K10.1149/1.2113608 ↗
42. The hot corrosion of metals by molten salts10.1149/198110.0159PV ↗
43. Hot corrosion of preoxidized Ni by a thin fused Na2SO4 film at 900°C.10.1149/1.2086436 ↗
44. Mechanisms for the hot corrosion of nickel-base alloys10.1007/BF02649626 ↗
45. Birks · 2006 · 1
46. The role of chromium in the hot corrosion of metals10.1149/1.3159332 ↗
47. Solubilities of Cr2O3 in fused Na2SO4 at 1200 K10.1149/1.2108648 ↗
48. Whitney Award Lecture—1986: chemistry and electrochemistry of the hot corrosion of metals10.5006/1.3583026 ↗
49. Kinetics of the low temperature hot corrosion of Co‐Cr‐Al alloys10.1149/1.2114105 ↗
50. A study of hot corrosion of Fe-Cr alloys induced by a thin film of fused (Na,K)2SO4 by electrochemical impedance spectroscopy.10.1515/htmp-2012-0171 ↗
51. Trends in fireside corrosion damage to superheaters in air and oxy-firing of coal/biomass10.1016/j.fuel.2013.04.005 ↗
52. Chapter 2 - enabling theory
53. Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650°C.10.1016/j.corsci.2016.07.014 ↗
54. T.D. Nguyen, J. Zhang, D. Young, Water vapour effects on corrosion of Fe–Cr and Fe–Cr–Ni alloys containing cerium and manganese in CO2 gas at 818 °C. 2014. 89, 220–235.10.1016/j.corsci.2014.08.029 ↗