Abstract
By performing microstructural characterization, tensile testing and failure analysis, the effects of electrochemical H-charging on microstructure and mechanical behaviour of two as-cast Mg-8Li (in wt%) based alloys were investigated and compared. Due to the in-situ formation of I-phase, the failure elongation ratio for Mg-8Li-6Zn-1Y alloy was 31.2 % and its hydrogen embrittlement (HE) susceptibility was about 1/4 that of Mg-8Li alloy after H-charging for 24 h. Moreover, the preferential location of H-induced pores transferred from two matrix phases to I-phase/matrix eutectic pockets due to the preferential H absorption of I-phase, resulting in the higher HE resistance of Mg-8Li-6Zn-1Y alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Plastic deformation and heat treatment of Mg-Li alloys: a review10.1016/j.jmst.2021.04.072 ↗
2. On the transformation characteristics of LA141A (Mg-Li·Al) alloy10.1016/0924-0136(95)01826-3 ↗
3. T.A. Samman, New hot rolled Mg-4Li-1Ca alloy: a potential candidate for automotive and biodegradable implant applications10.1016/j.matlet.2016.03.052 ↗
4. Composition and microstructure dependent corrosion behaviour of Mg-Li alloys10.1016/j.electacta.2017.11.091 ↗
5. Deformation mechanisms of β-Li in Mg-Li dual-phase alloy and effects of surface oxide layer10.1016/j.msea.2023.145856 ↗
6. Inhibiting effect of I-phase formation on the plastic instability of the duplex structured Mg-8Li-6Zn-1.2Y (in wt%) alloy10.1016/j.jma.2021.08.030 ↗
7. Microstructural evolution and mechanical response of duplex Mg-Li alloy containing particles during ECAP processing10.1016/j.matchar.2022.111910 ↗
8. Achieving high strength in a Mg-Li-Zn-Y alloy by α-Mg precipitation10.1016/j.msea.2022.143272 ↗
9. Design of a Mg-7Li-2.6Al-0.4Si alloy with simultaneously improved strength and ductility
10. Microstructure and mechanical properties of as-cast and extruded Mg-8Li-1Al-0.5Sn alloy10.1016/j.msea.2017.10.036 ↗
11. Anisotropic corrosion behaviour of hot-rolled Mg-8wt%Li alloy10.1016/j.jmst.2020.04.029 ↗
12. Effect of rolling ratios on the microstructural evolution and corrosion performance of an as-rolled Mg-8 wt%Li alloy10.1016/j.jma.2020.02.020 ↗
13. Microstructure and corrosion resistance of a duplex structured Mg-7.5Li-3Al-1Zn10.1016/j.jma.2020.07.007 ↗
14. Quantifying the influence of microstructure on the corrosion of Mg-Li alloys by using X-ray CT
15. Influence of erbium, cerium on the stress corrosion cracking behaviour of AZ91 Alloy in humid atmosphere10.1002/adem.201700021 ↗
16. Effect of air-formed film on corrosion behaviour of magnesium-lithium alloys10.1016/j.jma.2022.11.001 ↗
17. Evaluation of hydrogen entry into high strength steel under atmospheric corrosion10.1016/j.corsci.2009.11.046 ↗
18. In-situ measurement of hydrogen entry and hydrogen embrittlement of steel by atmospheric corrosion10.1016/j.corsci.2023.111212 ↗
19. Understanding the environmentally assisted cracking (EAC) initiation and propagation of new generation 7xxx alloys using slow strain rate testing10.1016/j.corsci.2022.110161 ↗
20. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
21. Negatively correlated corrosion and stress corrosion cracking of Mg-Al-Mn-Ca based alloys10.1016/j.corsci.2023.111747 ↗
22. Influence of phase dissolution and hydrogen absorption on the corrosion behaviour of Mg-7%Gd-5%Y-1%Nd-0.5%Zr alloy in 3.5 wt% NaCl solution10.1016/j.corsci.2018.07.019 ↗
23. Effect of hydrogen on stress corrosion cracking of magnesium alloy in 0.1 M Na2SO4 solution10.1016/j.msea.2007.11.035 ↗
24. Effect of solution treatment on stress corrosion cracking behaviour of an as-forged Mg-Zn-Y-Zr alloy
25. Hydrogen embrittlement of magnesium and magnesium alloys: a review10.1149/2.023304jes ↗
26. Effect of electrochemical hydrogen charging on the microstructure and mechanical behavior of a duplex structured Mg-8wt%Li alloy
27. Effect of Zn addition on the stress corrosion cracking of as-cast BCC Mg-11Li based alloys10.1016/j.corsci.2023.111707 ↗
28. Study on mechanical properties and hydrogen embrittlement susceptibility of 7075 aluminium alloy10.1179/1743278215Y.0000000004 ↗
29. Hydrogen trapping and embrittlement susceptibility in Al-Cu-Li alloys10.1016/j.corsci.2023.111628 ↗
30. Suppressed hydrogen embrittlement of high-strength Al alloys by Mn-rich intermetallic compound particles10.1016/j.actamat.2022.118110 ↗
31. Hydrogen trapping and hydrogen embrittlement in 15-5PH stainless steel10.1016/j.corsci.2022.110416 ↗
32. Hydrogen trapping and desorption of dual precipitates in tempered low-carbon martensitic steel10.1016/j.actamat.2020.06.046 ↗
33. Hydrogen trapping and hydrogen embrittlement of Mg alloys10.1007/s10853-017-1268-2 ↗
34. Hydrogen evolution from Zr-based amorphous and quasicrystalline alloys10.1016/S0925-8388(00)00717-9 ↗
35. Hydrogenation of (Zr69.5Al7.5Cu12Ni11)100 – xTix quasicrystalline alloys and its effect on their structural and microhardness behaviour10.1016/j.jnoncrysol.2013.08.024 ↗
36. The strengthening effect of icosahedral phase on as-extruded Mg-Li alloys10.1016/j.scriptamat.2007.03.017 ↗
37. Study on hydrogen absorption of pipeline steel under cathodic charging10.1016/j.corsci.2005.01.011 ↗
38. Effect of hydrogen charging on SCC of 2205 duplex stainless steel with varying microstructures in simulated deep-sea environment10.1016/j.corsci.2021.110026 ↗
39. Evaluation of electrochemical hydrogen absorption in welded pipe with steel API X5210.1016/j.ijhydene.2013.08.118 ↗
40. Influence of I-phase and W-phase on microstructure and mechanical properties of Mg-8Li-3Zn10.1016/S1003-6326(15)63656-1 ↗
41. Effect of icosahedral phase on the crystallographic texture and mechanical anisotropy of duplex structured Mg-Li alloys10.1016/j.matdes.2015.08.123 ↗
42. Effect of magnesium hydride on the corrosion behaviour of an AZ91 magnesium alloy in sodium chloride10.1016/j.corsci.2008.09.013 ↗
43. M. Pourbaix. Atlas of electrochemical equilibria in aqueous solution, second English Edition, National Association of Corrosion Engineers, U.S.A., 1974.10.5006/37502 ↗
44. Effect of quasicrystalline phase on improving the corrosion resistance of a duplex structured Mg-Li alloy10.1016/j.scriptamat.2013.09.025 ↗
45. Effect of icosahedral phase formation on the stress corrosion cracking (SCC) behaviors of the as-cast Mg-8%Li (in wt%) based alloys10.1016/j.jma.2022.08.007 ↗
46. Electrochemical corrosion and mechanical behaviors of the charged magnesium10.1016/j.msea.2008.04.012 ↗
47. Formation of hydrogen blister on AZ91 magnesium alloy during cathodic charging10.1016/j.corsci.2009.02.020 ↗
48. Evaluation of the delayed hydride cracking mechanism for transgranular stress corrosion cracking of magnesium alloys10.1016/j.msea.2007.03.020 ↗
49. Hydrogen embrittlement of aged and retrogressed-reaged Al-Li-Cu-Mg alloys10.1016/S1359-6454(96)00287-X ↗
50. II, Kinetic measurement and prediction of the hydrogen outgassing from the polycrystalline LiH/Li2O/LiOH system10.1016/j.jnucmat.2005.06.025 ↗
51. LiOH-embedded zeolite for carbon dioxide capture under ambient conditions10.1016/j.jiec.2014.07.030 ↗
52. Effect of the surface film formed by hydrogen charging on the corrosion behavior of an as-cast Mg-8%Li (in wt%) alloy10.3390/coatings13040800 ↗
53. Hydrogenation of Mg and two chosen Mg-Ni alloys10.1016/j.ijhydene.2008.09.042 ↗
54. Controllable hydrolysis performance of MgLi alloys and their hydrides10.1002/cphc.201900058 ↗
55. Stress corrosion cracking of A537 steel in simulated marine environments10.1016/j.corsci.2012.08.025 ↗
56. Corrosion behavior of a eutectic Mg-8Li alloy in NaCl solution10.1016/j.elecom.2021.107087 ↗
57. Precursor H-induced pyrolysis towards hydrogen storage properties enhancement of Mg-Y-Zn alloys with diverse Y level10.1016/j.jpowsour.2023.232695 ↗
58. Hydrolysis batteries: generating electrical energy during hydrogen absorption10.1002/anie.201711666 ↗
59. On the role of pre-exposure time and corrosion products in stress-corrosion cracking of ZK60 and AZ31 magnesium10.1016/j.msea.2021.140876 ↗
60. Effect of heat treatment on the stress corrosion cracking behavior of cast Mg-3Nd-3Gd-0.2Zn-0.5Zr alloy in a 3.5 wt% NaCl salt spray environment10.1016/j.matchar.2021.111630 ↗
61. Corrosion and stress corrosion cracking of ultra-high-purity Mg5Zn10.1016/j.corsci.2015.01.032 ↗
62. Hydrogen trapping in alloys studied by thermal desorption spectrometry10.1016/j.jallcom.2018.03.066 ↗
63. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
64. Effect of diffusible hydrogen content on embrittlement of P92 steel10.1016/j.ijhydene.2017.05.214 ↗
65. Hydrogen embrittlement susceptibility of a high strength steel X8010.1016/j.msea.2010.07.027 ↗
66. A nano-sized NbC precipitation strengthened FeCoCrNi high entropy alloy with superior hydrogen embrittlement resistance10.1016/j.corsci.2022.110636 ↗
67. Investigation of mechanical properties, formability, and anisotropy of dual phase Mg-7Li-1Zn10.1088/2053-1591/ab2de6 ↗
68. Effect of quasicrystal I-Phase on microstructure and mechanical properties of hot-rolled diphasic Mg-8wt% Li Alloy10.1007/s11665-021-06406-8 ↗
69. Effect of cross rolling on the microstructure and mechanical performance of a dual-phase structured Mg-8Li-6Zn-1Y (in wt%) alloy10.1016/j.jmst.2023.07.052 ↗
70. Effect of Nb-Ti multi-microalloying on the hydrogen trapping efficiency and hydrogen embrittlement susceptibility of hot-stamped boron steel10.1016/j.msea.2019.138788 ↗