Biomimetic structure-driven self-adapting oxidation barrier in continuous SiC skeleton reinforced graphite composites
Source abstract
Abstract
Inspired by the structural-functional feature of plant cells, herein, the intelligent biomimetic cellular-structured SiC-reinforced mesocarbon microbead composites were constructed via the combination of combustion synthesis and spark plasma sintering. Thanks to the functional adaptability of the SiC skeleton as cytoderm, the composites exhibited not only excellent oxidation resistance but also self-healing behavior of microcracks. The physical isolation of the SiC skeleton to O 2 at low temperatures (< 1200 °C), as well as the formation of self-healing oxide barriers and oxide shell arrays at high temperatures (1200–1500 °C), ensured the long-term oxidation resistance of the composites over a wide temperature range.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Surface Modification and Superhydrophobicity · Electrohydrodynamics and Fluid Dynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Graphite, ceramics, and ceramic composites for high-temperature nuclear power systems10.1557/mrs2009.9 ↗
2. A review on the mechanical and electrical properties of graphite and modified graphite reinforced polymer composites10.1016/j.progpolymsci.2010.11.003 ↗
3. Long-term ceramic matrix composite for aeroengine10.1007/s40145-022-0611-5 ↗
4. Double SiC coating on carbon/carbon composites against oxidation by a two-step method10.1016/S1003-6326(13)62703-X ↗
5. Investigation of oxidation behaviors of nuclear graphite being developed and IG-110 based on gas analysis10.1080/00223131.2017.1344579 ↗
6. Understanding the reaction of nuclear graphite with molecular oxygen: Kinetics, transport, and structural evolution10.1016/j.jnucmat.2017.06.001 ↗
7. High temperature oxidation behaviors of bulk SiC with low partial pressures of air and water vapor in argon10.1016/j.corsci.2020.108795 ↗
8. Nano-SiC/SiC anti-oxidant coating on the surface of graphite10.1016/j.apsusc.2012.09.139 ↗
9. A brief review of carbon nanotube reinforced metal matrix composites for aerospace and defense applications10.1007/s40089-021-00328-y ↗
10. Fabrication and oxidation behavior of a reaction derived graphite-ZrC composite for ultrahigh temperature applications10.1016/j.matlet.2009.07.022 ↗
11. SiC/HfB2-based ceramic/SiC multilayer coating to protect C/C composites against oxidation at medium and high temperatures for long-life service10.1016/j.corsci.2022.110299 ↗
12. C/SiC/Si-Mo-Cr multilayer coating for carbon/carbon composites for oxidation protection10.1016/S1872-5805(12)60006-7 ↗
13. High-temperature corrosion of HfSiO4 environmental barrier coatings exposed to water vapor/oxygen atmosphere and molten calcium magnesium aluminosilicate10.1016/j.corsci.2021.110081 ↗
14. Advances in ultra-high temperature ceramics, composites, and coatings10.1007/s40145-021-0550-6 ↗
15. Enhanced oxidation resistance of Mo-modified Si-SiC coating on C/C composites by laser-inducing10.1016/j.apsusc.2021.151786 ↗
16. A MoSi2-SiOC-Si3N4/SiC anti-oxidation coating for C/C composites prepared at relatively low temperature10.1016/j.ceramint.2016.11.151 ↗
17. Oxidation and ablation protection of graphite materials by monolayer MoSi2-CrSi2-SiC-Si multiphase coating10.1016/j.ceramint.2018.08.013 ↗
18. Preparation of ZrB2-MoSi2 high oxygen resistant coating using nonequilibrium state powders by self-propagating high-temperature synthesis10.1007/s40145-021-0485-y ↗
19. Oxidation behavior of C/C composites with SiC/ZrSiO4-SiO2 coating10.1016/S1003-6326(17)60045-1 ↗
20. A mullite/SiC oxidation protective coating for carbon/carbon composites10.1016/j.jeurceramsoc.2012.08.009 ↗
21. Oxidation behaviour of SiC ceramic coating for C/C composites prepared by pressure-less reactive sintering in wet oxygen: experiment and first-principle simulation10.1016/j.ceramint.2021.02.099 ↗
22. Deposition kinetics and boundary layer theory in the chemical vapor deposition of β-SiC on the surface of C/C composite
23. A multi-layered SiC coating to protect graphite spheres from high temperature oxidation in static air10.1016/j.corsci.2021.109325 ↗
24. A low-temperature prepared composite coating to protect SiC-coated C/C composites against oxidation in a wide temperature range for long-life service10.1016/j.jeurceramsoc.2023.03.037 ↗
25. Plant cell wall extensibility: Connecting plant cell growth with cell wall structure, mechanics, and the action of wall-modifying enzymes10.1093/jxb/erv511 ↗
26. Nanoscale structure, mechanics and growth of epidermal cell walls10.1016/j.pbi.2018.07.016 ↗
27. Exceptionally low ablation rates realized in the cellular-structured MCMB@WC composites via biomimetic design10.1016/j.compositesa.2024.108035 ↗
28. Biomimetic cellular-structured MCMB@WC composites with excellent mechanical properties10.1016/j.jeurceramsoc.2023.03.062 ↗
29. SiC coating toughened by SiC nanowires to protect C/C composites against oxidation10.1016/j.ceramint.2011.05.159 ↗
30. Investigating the properties of machinable ceramics SiC/C(graphite) prepared by plasma activated sintering10.4028/www.scientific.net/MSF.620-622.403 ↗
31. Recent advances and challenges in silicon carbide (SiC) ceramic nanoarchitectures and their applications
32. Opportunities for advanced ceramics and composites in the nuclear sector10.1111/jace.12406 ↗
33. All-carbon multi-scale and hierarchical fibers and related structural composites: a review10.1016/j.compscitech.2019.107932 ↗
34. Structural composites for multifunctional applications: current challenges and future trends10.1016/j.pmatsci.2017.04.005 ↗
35. Continuous SiC skeleton reinforced highly oriented graphite flake composites with high strength and specific thermal conductivity10.1007/s40145-021-0542-6 ↗
36. B4C-SiC skeleton reinforced graphite composites with excellent mechanical properties10.1007/s10853-023-08788-7 ↗
37. Self-lubrication behavior of the reaction-formed graphite/SiC composites with optimizing graphite content10.1016/j.wear.2023.204946 ↗
38. Design, preparation and properties of carbon fiber reinforced ultra-high temperature ceramic composites for aerospace applications: a review10.1016/j.jmst.2016.08.004 ↗
39. Preparation of SiC coated graphite composite powders by nitriding combustion synthesis10.26599/JAC.2023.9220798 ↗
40. SiC/SiC-YAG-YSZ oxidation protective coatings for carbon/carbon composites10.1016/j.corsci.2013.01.013 ↗
41. Water vapor corrosion behaviors of plasma sprayed RE2SiO5 (RE=Gd, Y, Er) coatings10.1016/j.corsci.2020.108529 ↗
42. Comparison of the oxidation behaviors of SiC coatings on C/C composites prepared by pack cementation and chemical vapor deposition10.1016/j.surfcoat.2016.05.071 ↗
43. Preparation and sintering of silica-coated silicon carbide composite powder, Funtai Oyobi Fummatsu Yakin/10.2497/jjspm.63.111 ↗
44. LPCVD-based SiO2/SiC multi-layers coating on graphite for improved anti-oxidation at wide-ranged temperatures10.1016/j.compositesb.2018.03.035 ↗
45. Growth of SiO2 on SiC by dry thermal oxidation: mechanisms10.1088/0022-3727/40/20/S10 ↗
46. Oxidation resistance and strength retention of ZrB2-SiC ceramics10.1016/j.jeurceramsoc.2010.01.028 ↗
47. Development and validation of a model for the chemical kinetics of graphite oxidation10.1016/j.jnucmat.2011.01.129 ↗
48. A carbon nanotube-enhanced SiC coating for the oxidation protection of C/C composite materials10.1016/j.compositesb.2011.05.012 ↗
49. Silicon carbide coating by reactive pack cementation-part II: Silicon monoxide/carbon reaction10.1002/(SICI)1521-3862(200002)6:1<41::AID-CVDE41>3.0.CO;2-8 ↗
50. Sealing plant surfaces: cuticular wax formation by epidermal cells10.1146/annurev.arplant.59.103006.093219 ↗
51. Epidermis: The formation and functions of a fundamental plant tissue10.1111/j.1469-8137.2010.03514.x ↗
52. Oxidation mechanism of SiC-Zirconia-Glass ceramic coated carbon/carbon composites at 1123–1273 K10.1016/j.materresbull.2017.03.046 ↗