Abstract
The flow-accelerated corrosion (FAC) behavior at different bending angles in bend pipe in simulated secondary circuit water environment of pressurized water reactor (PWR) was investigated. The results indicated that the FAC rates at different bending angles within the bend pipe strongly depended on the ferrite nanocrystallization degree and the mass transfer coefficients. Ferrite nanocrystallization played a dominant effect on FAC, and the mass transfer coefficient played a secondary role on FAC, causing the maximum FAC rate in bend pipe was transferred to the 45° position on the intrados.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgy and Material Forming · Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. A study on the dynamic characteristics of the secondary loop in nuclear power plant10.1016/j.net.2020.11.014 ↗
2. Flow-accelerated corrosion in nuclear power plants
3. Influence of elbow curvature on flow and turbulence structure through a 90° elbow10.1016/j.nucengdes.2018.09.011 ↗
4. Pipe wall thickness prediction with CFD based mass transfer coefficient and degradation feedback for flow accelerated corrosion10.1016/j.pnucene.2018.04.024 ↗
5. Flow accelerated corrosion: forms, mechanisms and case studies10.1016/j.proeng.2014.11.083 ↗
6. Flow-accelereted corrosion of pressure vessels in fossil plants10.1016/S0308-0161(99)00087-3 ↗
7. Influence of flow velocity and temperature on flow accelerated corrosion rate at an elbow pipe10.1016/j.nucengdes.2018.11.022 ↗
8. Modelling of erosion-corrosion in practical geometries10.1016/j.corsci.2008.12.025 ↗
9. Predictions of hydrodynamic characteristics and corrosion rates using CFD in the piping systems of pressurized-water reactor power plant10.1016/j.anucene.2013.11.007 ↗
10. The mechanism of asymmetric pipe-wall thinning behind an orifice by combined effect of swirling flow and orifice bias10.1016/j.nucengdes.2012.07.001 ↗
11. Influence of bend geometry on flow accelerated corrosion under neutral pH conditions10.1016/j.engfailanal.2020.105127 ↗
12. CFD study of flow accelerated corrosion in 3D elbows10.1016/j.anucene.2014.01.031 ↗
13. Flow and Mass Transfer in Bends Under Flow-Accelerated Corrosion Wall Thinning Conditions10.1115/1.4001061 ↗
14. Effect of bending process on microstructure, mechanical properties and crack formation of 5% Ni steel10.3390/met12071188 ↗
15. Influence of grain refinement on the corrosion behavior of metallic materials: A review10.1007/s12613-021-2308-0 ↗
16. Corrosion of ultra-fine grained copper fabricated by equal-channel angular pressing10.1016/j.corsci.2008.01.024 ↗
17. Corrosion behaviour of bulk ultra-fine grained AZ91D magnesium alloy fabricated by equal-channel angular pressing10.1016/j.corsci.2010.09.044 ↗
18. Evaluation of stress corrosion cracking susceptibility of stainless steel 304L with surface nanocrystallization by small punch test10.1016/j.msea.2012.10.071 ↗
19. Electrochemical characterization of the corrosion of mild steel in saline following mechanical deformation10.1080/00032719.2020.1793994 ↗
20. Ultrafine grained titanium sheets with high strength and high corrosion resistance10.1016/j.msea.2011.07.074 ↗
21. Improving corrosion resistance of pure Al through ECAP10.1179/147842209X12559428167562 ↗
22. Effect of additional axial tension on formability of equal curvature-diameter bending without mandrel for 0Cr18Ni9 stainless steel tube10.1088/2053-1591/ab09b1 ↗
23. Flow and mass transfer downstream of an orifice under flow accelerated corrosion conditions10.1016/j.nucengdes.2012.06.033 ↗
24. Microstructure evolution of railway pearlitic wheel steels under rolling-sliding contact loading10.1016/j.triboint.2020.106685 ↗
25. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
26. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
27. Continuous Dynamic Recrystallization in a Superplastic 7075 Aluminum Alloy10.2320/matertrans.43.2400 ↗
28. Developing stable fine-grain microstructures by large strain deformation10.1098/rsta.1999.0395 ↗
29. High angle boundaries formed by grain subdivision mechanisms10.1016/S1359-6454(97)00027-X ↗
30. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
31. Effect of plastic deformation on the corrosion of iron and steel10.5006/0010-9312-20.9.293t ↗
32. XRD and EBSD studies of severe shot peening induced martensite transformation and grain refinements in austenitic stainless steel10.1016/j.matchar.2020.110574 ↗
33. Making FAC calculations with BRT-CICERO™ and updating to version 3.0
34. Water chemistry of nuclear reactor systems 2, British Nuclear Energy Society
35. The mechanism of corrosion-erosion in steam extraction lines of power stations
36. Corrosion behavior of pipeline steel in oilfield produced water under dynamic corrosion system10.1007/s11595-022-2582-3 ↗
37. Cause analysis of flow accelerated corrosion and erosion-corrosion cases in korea nuclear power plants10.14773/cst.2016.15.4.182 ↗
38. Galvanic effect of magnetite on the corrosion behavior of carbon steel in deaerated alkaline solutions under flowing conditions10.1016/j.corsci.2017.10.017 ↗