Abstract

The effect of Si and prolonged time on interfaces and cavitation erosion behavior of directionally solidified (DS) Fe-B alloy in flowing liquid zinc was investigated. The results show Si enriches in α-Fe intragranular and α/Fe 2B boundaries to refine textured grains. DS Fe-B alloy with 2.5 wt%Si exhibits the best cavitation erosion resistance to flowing zinc, which is attributed to formation of alternating distributed Γ-Fe 3Zn 10 and FeSi and subsequently columnar ζ-FeZn 13. Cavitation erosion resistance mechanism of DS Fe-B alloy with 2.5 wt%Si is manifested that Si-induced Γ-Fe 3Zn 10 and FeSi and the rooting-whisker ζ-FeZn 13 layer can inhibit spallation and cracks of Fe 2B and products.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Surface roughness changes on a hot-dipped galvanized sheet steel during deformation at low strain levels10.1016/j.actamat.2003.11.005 ↗
2. Interface fracture behavior of zinc coatings on steel: experiments and finite element calculations10.1016/j.surfcoat.2006.08.046 ↗
3. Tuning of WO3 nanoparticles integration into Fe-Zn intermetallic layers of hot-dip zinc coating to control corrosion10.1016/j.mseb.2021.115539 ↗
4. Simulation of flow in a continuous galvanizing bath: Part I. Thermal effects of ingot addition10.1007/s11663-004-0106-5 ↗
5. Simulation of flow in a continuous galvanizing bath: Part II. Transient aluminum distribution resulting from Ingot addition10.1007/s11663-004-0107-4 ↗
6. Numerical simulation of flow, temperature and composition variations in a galvanizing bath10.1179/cmq.2005.44.3.369 ↗
7. Friction and wear characterization of some cobalt and iron-based superalloys in zinc alloy10.1016/S0043-1648(01)00889-4 ↗
8. The corrosion of Fe3Al alloy in liquid zinc10.1016/j.corsci.2006.10.002 ↗
9. Degradation behaviour of boronized carbon and high alloy steels in molten aluminium and zinc10.1016/S0167-577X(98)00077-9 ↗
10. Liquid metal corrosion of 316L, Fe3Al, and FeCrSi in molten Zn-Al baths10.1007/s11661-005-0325-7 ↗
11. Multiphase interface structure induced erosion resistance of directional solidified Fe-B alloy in flow liquid zinc10.1016/j.matlet.2017.10.027 ↗
12. Effects of boron concentration on the corrosion resistance of Fe-B alloys immersed in 460°C molten zinc bath10.1016/j.surfcoat.2009.12.010 ↗
13. Hardness and modulus of Fe2B, Fe3(C,B), and Fe23(C,B)6 borides and carboborides in the Fe-C-B system10.1016/j.matchar.2017.11.012 ↗
14. Microstructure and mechanical properties of high boron white cast iron10.1016/j.msea.2007.10.017 ↗
15. Microstructure and mechanical properties of high boron white cast iron with about 4 wt% chromium10.1007/s10853-010-4840-6 ↗
16. Interface characterization and erosion-corrosion behavior of directional Fe-3.5 wt% B steel in flowing liquid zinc at various temperatures10.1016/j.corsci.2015.12.018 ↗
17. Interface characteristics and corrosion behavior of oriented bulk Fe2B alloy in liquid zinc10.1016/j.corsci.2013.08.033 ↗
18. Effect of erosion angle and Fe2B orientation on cavitation erosion and interfaces of Fe-B alloy in high- velocity flowing liquid zinc10.1016/j.wear.2018.04.007 ↗
19. Microstructure and interface characteristics of Fe-B alloy in liquid 0.25wt% Al-Zn at various bath temperatures10.1016/j.matchemphys.2011.12.044 ↗
20. Effects of erosion angle on erosion properties of Fe-B alloy in flowing liquid zinc10.1007/s11661-015-2820-9 ↗
21. Influences of Si on corrosion of Fe-B alloy in liquid zinc10.1179/174327808X315696 ↗
22. A review on relationship between morphology of boride of Fe-B alloys and the wear/corrosion resistant properties and mechanisms10.1016/j.jmrt.2019.09.004 ↗
23. Metallurgy of galvanized coating
24. Surface effects in batch galvanizing of silicon containing steels10.1179/mst.1990.6.8.681 ↗
25. The metallurgy of zinc-coated steel10.1016/S0079-6425(98)00006-1 ↗
26. Reactivity of silicon steels in hot-dip galvanizing10.1179/cmq.1972.11.4.609 ↗
27. Reaction between Fe-Si alloys and liquid zinc10.2320/matertrans1960.24.272 ↗
28. Immersion time dependence of reaction between Fe-Si alloys in liquid zinc10.2320/matertrans1960.25.545 ↗
29. Effect of silicon on the microstructure and growth kinetics of intermetallic phases formed during hot-dip aluminizing of ferritic steel10.1016/j.surfcoat.2017.03.040 ↗
30. Influence of silicon on the α-Fe/Γ interface of hot-dip galvanized steels10.1016/j.surfcoat.2005.06.017 ↗
31. Effect of silicon on corrosion of directional Fe-B-Si alloy in liquid Zinc10.1007/s11661-020-06110-7 ↗
32. Effect of Fe2B orientation on erosion-corrosion behavior of Fe-3.5wt% B steel in flowing zinc10.1016/j.corsci.2015.05.039 ↗
33. Effect of orientation and lamellar spacing of Fe2B on interfaces and corrosion behavior of Fe-B alloy in hot-dip galvanization10.1016/j.actamat.2016.06.016 ↗
34. Microstructure and corrosion behavior of cast Fe-B alloys dipped into liquid zinc bath10.1016/j.matchar.2010.05.009 ↗
35. Investigation of flowing liquid zinc erosion and corrosion of the Fe-B alloy at various times10.1557/jmr.2015.27 ↗
36. Transformation behavior of low carbon steels containing two different Si contents10.1016/S1006-706X(09)60028-5 ↗
37. Carbides in high-speed steels containing silicon10.1007/s11661-004-0222-5 ↗
38. Microstructure and crystallography of borides and secondary precipitation in 18 wt% Cr–4 wt% Ni–1 wt% Mo–3.5 wt% B–0.27 wt% C steel10.1016/j.actamat.2011.11.004 ↗
39. Orientation relationship and interface of the Fe-Zn intermetallic phases in galvannealed CMnSi-Trip steels10.1016/j.matchar.2015.06.041 ↗
40. 450 °C isothermal section of the Fe-Zn-Si ternary phase diagram10.1179/cmq.2001.40.3.377 ↗
41. The iron-silicon-zinc ternary system
42. The 480 °C and 405 °C isothermal sections of the phase diagram of Fe–Zn–Si ternary system10.1016/j.jallcom.2005.03.043 ↗
43. Fe-Si-Zn (iron-silicon-zinc)10.1007/s11669-007-9108-8 ↗
44. Effects of Si solid solution in Fe substrate on the alloying reaction between Fe substrate and liquid Zn10.2355/isijinternational.ISIJINT-2017-410 ↗
45. Role of silicon in steels on galvanized coatings10.1016/S1006-7191(08)60081-2 ↗
46. Corrosion of Fe-B-Si alloys in liquid zinc10.1016/j.matchemphys.2021.124933 ↗
47. High-temperature batch hot-dip galvanizing. Part 1. General description of coatings formed at 560 ° C10.1016/S0257-8972(96)02941-6 ↗
48. Reaction mechanisms for the coatings formed during the hot dipping of iron in 0 to 10 pct Al-Zn baths at 450 °C to 700 °C10.1007/BF02813270 ↗
49. High-temperature batch hot-dip galvanizing, Part 2. Comparison of coatings formed in the temperature range 520-555◦C10.1016/S0257-8972(96)02940-4 ↗
50. Experimental investigation and thermodynamic reassessment of the Fe-Si-Zn system10.1016/j.calphad.2010.07.006 ↗
51. A crystallographically consistent optimization of the Zn–Fe system10.1016/j.calphad.2005.08.005 ↗
52. Formation of Fe5Si3 precipitate in the Fe2Al5 intermetallic layer of the Al/steel dissimilar arc welding joint: a transmission electron microscopy (TEM) study10.1016/j.matchar.2021.111236 ↗
53. Miedema calculator: a thermodynamic platform for predicting formation enthalpies of alloys within framework of Miedema’s theory10.1016/j.cpc.2016.08.013 ↗