journal article·2024-12

Hydrogen-induced crack behavior of a precipitation-strengthened Ni50Cr20Co15Al10V5 high entropy alloy

Qiancheng Zhao, Hong Luo, Milos B. Djukic, Zhimin Pan, Hongxu Cheng, R.K. Islamgaliev

Corrosion Science· Volume 241
Publisher page

Abstract

The hydrogen-induced cracking behavior and mechanism of an L1 2-strengthened Ni 50Cr 20Co 15Al 10V 5 high entropy alloy was evaluated using the tensile test after hydrogen charging. The microstructures and hydrogen-induced cracks were characterized by electron backscatter diffraction and electron channeling contrast imaging methods. The results revealed that hydrogen decreased the strain hardening rate and induced pronounced cracks, leading to significant degradation in elongation. After deformation, the local strain was concentrated in the precipitate-matrix interfaces. The precipitate-matrix boundary and the interior of precipitates were prone to hydrogen embrittlement, where hydrogen-induced cracks tended to propagate, attributing to the hydrogen-enhanced decohesion mechanism.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (84)

Show source-provided references
1. High-entropy alloys10.1038/s41578-019-0121-4 ↗
2. High-entropy alloys: emerging materials for advanced functional applications10.1039/D0TA09601F ↗
3. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
4. Alloy design strategies and future trends in high-entropy alloys10.1007/s11837-013-0761-6 ↗
5. Corrosion-resistant high entropy alloy with high strength and ductility10.1016/j.scriptamat.2019.03.028 ↗
6. Nanocrystalline high-entropy alloys: a new paradigm in high-temperature strength and stability10.1021/acs.nanolett.6b04716 ↗
7. Microstructure and wear behavior of AlxCo1. 5CrFeNi1. 5Tiy high-entropy alloys10.1016/j.actamat.2011.06.041 ↗
8. Recent advances on environmental corrosion behavior and mechanism of high-entropy alloys10.1016/j.jmst.2020.11.044 ↗
9. Corrosion behavior of an equiatomic CoCrFeMnNi high-entropy alloy compared with 304 stainless steel in sulfuric acid solution10.1016/j.corsci.2018.02.031 ↗
10. A comprehensive review on advances in high entropy alloys: Fabrication and surface modification methods, properties, applications, and future prospects10.1016/j.jmapro.2023.12.039 ↗
11. Solid solution strengthening in medium-to high-entropy alloys10.1016/j.msea.2022.144271 ↗
12. Strengthening mechanisms in equiatomic ultrafine grained AlCoCrCuFeNi high-entropy alloy studied by micro-and nanoindentation methods10.1016/j.actamat.2016.11.046 ↗
13. Compositionally complex coherent precipitation-strengthened high-entropy alloys: a critical review10.1007/s12598-021-01953-4 ↗
14. Transformation-enhanced strength and ductility in a FeCoCrNiMn dual phase high-entropy alloy10.1016/j.msea.2020.139182 ↗
15. Nanoprecipitate-strengthened high-entropy alloys10.1002/advs.202100870 ↗
16. Effect of lattice distortion on solid solution strengthening of BCC high-entropy alloys10.1016/j.jmst.2017.07.013 ↗
17. Strong grain-size effect on deformation twinning of an Al0. 1CoCrFeNi high-entropy alloy10.1080/21663831.2016.1257514 ↗
18. Ultrahigh hardness in nanostructured dual-phase high-entropy alloy AlCrFeCoNiNb developed by high-pressure torsion10.1016/j.jallcom.2021.161101 ↗
19. Thermal stability and grain boundary strengthening in ultrafine-grained CoCrFeNi high entropy alloy composite10.1016/j.matdes.2017.08.053 ↗
20. Outstanding tensile properties of a precipitation-strengthened FeCoNiCrTi0. 2 high-entropy alloy at room and cryogenic temperatures10.1016/j.actamat.2018.11.049 ↗
21. Metastable high-entropy dual-phase alloys overcome the strength–ductility trade-off10.1038/nature17981 ↗
22. Enhancing fatigue life by ductile-transformable multicomponent B2 precipitates in a high-entropy alloy10.1038/s41467-021-23689-6 ↗
23. Precipitation-hardened high-entropy alloys for high-temperature applications: A critical review10.1557/mrs.2019.255 ↗
24. Achieving ultrahigh strength and ductility in high-entropy alloys via dual precipitation10.1016/j.jmst.2023.05.021 ↗
25. Effect of coherent L12 nanoprecipitates on the tensile behavior of a fcc-based high-entropy alloy10.1016/j.msea.2017.04.111 ↗
26. Nanoscale L12 phase precipitation induced superb ambient and high temperature mechanical properties in Ni–Co–Cr–Al system high-entropy superalloys10.1016/j.msea.2023.145995 ↗
27. A novel L12-strengthened multicomponent Co-rich high-entropy alloy with both high γ′-solvus temperature and superior high-temperature strength10.1016/j.scriptamat.2021.113826 ↗
28. Low-density nano-precipitation hardened Ni-based medium entropy alloy with excellent strength-ductility synergy10.1016/j.jallcom.2023.171213 ↗
29. Resistance of CoCrFeMnNi high-entropy alloy to gaseous hydrogen embrittlement10.1016/j.scriptamat.2017.03.029 ↗
30. Strong resistance to hydrogen embrittlement of high-entropy alloy10.1016/j.msea.2018.08.101 ↗
31. Role of hydrogen and temperature in hydrogen embrittlement of equimolar CoCrFeMnNi high-entropy alloy10.1007/s12540-020-00752-3 ↗
32. Grain refinement effect on hydrogen embrittlement resistance of an equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.ijhydene.2019.04.280 ↗
33. Influence of pre-strain on the gaseous hydrogen embrittlement resistance of a high-entropy alloy10.1016/j.msea.2018.01.107 ↗
34. Gradient-structured high-entropy alloy with improved combination of strength and hydrogen embrittlement resistance10.1016/j.corsci.2022.110253 ↗
35. Microstructure and defect effects on strength and hydrogen embrittlement of high-entropy alloy CrMnFeCoNi processed by high-pressure torsion10.1016/j.msea.2022.143179 ↗
36. High strength and high ductility of a severely deformed high-entropy alloy in the presence of hydrogen10.1016/j.corsci.2023.111097 ↗
37. Effect of Mo doping on the gaseous hydrogen embrittlement of a CoCrNi medium-entropy alloy10.1016/j.corsci.2021.109628 ↗
38. Hydrogen embrittlement of the equi-molar FeNiCoCr alloy10.1016/j.actamat.2018.07.032 ↗
39. Hydrogen induced microstructure evolution and cracking mechanism in a metastable dual-phase high-entropy alloy10.1016/j.msea.2021.141490 ↗
40. Hydrogen embrittlement of additively manufactured AlCoCrFeNi2. 1 eutectic high-entropy alloy10.1016/j.corsci.2021.110007 ↗
41. Hydrogen embrittlement and failure mechanisms of multi-principal element alloys: A review10.1016/j.jmst.2022.01.008 ↗
42. Hydrogen induced cracking behavior of the dual-phase Co30Cr10Fe10Al18Ni30Mo2 eutectic high entropy alloy10.1016/j.ijhydene.2023.09.053 ↗
43. A strong and ductile medium-entropy alloy resists hydrogen embrittlement and corrosion10.1038/s41467-020-16791-8 ↗
44. Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging10.1016/j.corsci.2011.05.060 ↗
45. J.-j. Kai, Synergistic effect of Ti and Al on L12-phase design in CoCrFeNi-based high entropy alloys10.1016/j.intermet.2019.106476 ↗
46. Effect of Al/Ni ratio, heat treatment on phase transformations and microstructure of AlxFeCoCrNi2− x (x= 0.3, 1) high entropy alloys10.1016/j.matdes.2015.05.027 ↗
47. Microstructure and texture evolution in dual-phase steels: Competition between recovery, recrystallization, and phase transformation10.1016/j.msea.2010.03.028 ↗
48. The formation of cellular precipitate and its effect on the tensile properties of a precipitation strengthened high entropy alloy10.1016/j.matchemphys.2017.09.057 ↗
49. Microstructure and mechanical behavior in a spherical L12 nanoprecipitates strengthened Ni35Co27. 5Cr27. 5Al5Ti5 high-entropy alloy fabricated by direct casting and heat treatment
50. Role of copper on L12 precipitation strengthened fcc based high entropy alloy10.1016/j.mtla.2019.100282 ↗
51. Superior high-temperature properties and deformation-induced planar faults in a novel L12-strengthened high-entropy alloy10.1016/j.actamat.2020.02.028 ↗
52. Design and high-strength origin of novel (CoFeNi) 80Ti5V15 medium entropy alloy with “fcc+ L12” structure10.1016/j.jmst.2023.01.002 ↗
53. Pre-strain and hydrogen charging effect on the plastic and fracture behavior of quenching and partitioning (Q&P) steel10.1016/j.actamat.2023.119524 ↗
54. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: the role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
55. A systematic study on the influence of electrochemical charging conditions on the hydrogen embrittlement behaviour of a pipeline steel10.1016/j.ijhydene.2023.01.149 ↗
56. Hydrogen embrittlement of an interstitial equimolar high-entropy alloy10.1016/j.corsci.2018.03.040 ↗
57. Comparative study of hydrogen embrittlement in stable and metastable high-entropy alloys10.1016/j.scriptamat.2018.03.003 ↗
58. Mechanical and microstructural analysis on hydrogen-related fracture in a martensitic steel10.1016/j.ijhydene.2019.09.097 ↗
59. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
60. Comparative study on hydrogen embrittlement resistance in additive manufactured and forged austenitic stainless steel
61. An analysis of the tensile elongation to failure of laminated metal composites in the presence of strain-rate hardening10.1016/j.actamat.2011.12.041 ↗
62. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
63. Comprehensive study of strain hardening behavior of CrCoNi medium-entropy alloy10.1016/j.jallcom.2021.160623 ↗
64. Hydrogen embrittlement resistance of precipitation-hardened FeCoNiCr high entropy alloys10.1016/j.intermet.2022.107800 ↗
65. Hydrogen embrittlement and associated surface crack growth in fine-grained equiatomic CoCrFeMnNi high-entropy alloys with different annealing temperatures evaluated by tensile testing under in situ hydrogen charging10.1016/j.ijhydene.2021.07.136 ↗
66. Simultaneous enhancement of strength and ductility via microband formation and nanotwinning in an L12-strengthened alloy
67. Non-monotonous effect of pre-strain on the precipitates and strengthening mechanisms of high-entropy alloys10.1016/j.jallcom.2022.164338 ↗
68. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
69. The effect of nitrogen alloying on hydrogen-assisted plastic deformation and fracture in FeMnNiCoCr high-entropy alloys10.1016/j.scriptamat.2020.113642 ↗
70. Effect of electrochemical charging on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.actamat.2019.08.020 ↗
71. Effect of hydrogen charging time on hydrogen embrittlement of CoCrFeMnNi high-entropy alloy10.1016/j.corsci.2021.110073 ↗
72. Distinct effects of in-situ and ex-situ hydrogen charging methods on the mechanical behavior of CoCrFeNi high-entropy alloy fabricated by laser-powder bed fusion10.1016/j.jallcom.2023.168858 ↗
73. Effect of cell wall on hydrogen response in CoCrFeMnNi high-entropy alloy additively manufactured by selective laser melting10.1016/j.jallcom.2022.166735 ↗
74. Hydrogen embrittlement in different materials: A review10.1016/j.ijhydene.2018.09.201 ↗
75. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
76. Hydrogen embrittlement and hydrogen-induced crack initiation in additively manufactured metals: A critical review on mechanical and cyclic loading10.1016/j.ijhydene.2024.01.232 ↗
77. Investigation of fine-scale dislocation distributions at complex geometrical structures by using HR-EBSD and a comparison with conventional EBSD10.1016/j.matchar.2023.113498 ↗
78. Ultrahigh strength-high ductility 1 GPa low density austenitic steel with ordered precipitation strengthening phase and dynamic slip band refinement10.1016/j.msea.2022.142829 ↗
79. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
80. In situ study on plastic deformation mechanism of Al0. 3CoCrFeNi high-entropy alloys with different microstructures10.1016/j.msea.2022.144134 ↗
81. An investigation of micro-mechanisms in hydrogen induced cracking in nickel-based superalloy 71810.1016/j.jallcom.2016.01.033 ↗
82. Effects of interstitial C and N on hydrogen embrittlement behavior of non-equiatomic metastable FeMnCoCr high-entropy alloys10.1016/j.corsci.2021.109933 ↗
83. Effect of anisotropy and slip transfer on hydrogen-assisted cracking of a 2205 duplex stainless steel: a critical analysis10.1016/j.corsci.2023.110988 ↗
84. Study of hydrogen-induced delayed fracture in high-Mn TWIP/TRIP steels during in situ electrochemical hydrogen-charging: Role of microstructure and strain rate in crack initiation and propagation10.1016/j.corsci.2019.108191 ↗