Abstract

Grain-oriented silicon steel is decarburized in N 2-H 2-H 2 O at 835 ℃ for different time. The oxide is spherical, spherical-lamellar and lamellar from outside to inside, and lamellar oxide would gradually degenerate to spheroid as oxidation front moves inward. Concentration-depth profiles for silicon exhibit damping-like oscillations. Wagner’s model is extended to illustrate the intrinsic mechanism by introducing the hypothesis of flux imbalance at oxidation front with finite thickness. Based on the extended model, the dissolved oxygen concentration at steel surface is lower at initial decarburization, and the damping-like oscillations of concentration profile for silicon follow from cyclic change in oxidation front velocity.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties and Applications · Metallurgical Processes and Thermodynamics · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Electrical Steels
2. P. Beckley, G.K. Sujan. Steels, Silicon Iron-Based: Magnetic Properties. In. Reference Module in Materials Science and Materials Engineering. Elsevier, 2016.10.1016/B978-0-12-803581-8.02475-9 ↗
3. Magnetism in solids: hysteresis
4. Magnetic aging effect losses on electrical steels10.1109/TMAG.2016.2517942 ↗
5. Magnetic ageing characteristics of low silicon electrical steels10.1016/0304-8853(82)90027-0 ↗
6. Consequences of magnetic aging for iron losses in electrical steels10.1016/j.jmmm.2006.02.185 ↗
7. Reactions during decarburization annealing of electrical steel
8. The formation of protective films on iron-silicon alloys10.1016/0010-938X(79)90012-X ↗
9. Numerical Simulation of Decarburization Kinetics for Fe-3%Si Steel during Annealing10.2355/isijinternational.ISIJINT-2018-547 ↗
10. Modelling decarburization in electrical steels
11. Modeling decarburization kinetics of grain-oriented silicon steel10.1007/s11434-014-0156-2 ↗
12. Decarburization rate related to surface oxidation of grain oriented silicon steel10.1016/0304-8853(82)90105-6 ↗
13. Formation mechanism of surface oxide layer of grain-oriented silicon steel10.1007/s42243-020-00464-3 ↗
14. J. De Castro, M.F. Campos. Modeling descarburisation process of heat treatment of electrical steels, 2022.
15. Decarburizing Annealing of grain-oriented solicon steel. J Iron
16. S. Yang. The study of Decarburization Process in the Oriented Silicon Steel Production [D]. Wuhan: Wuhan University of Science and Technology, 2016.(in Chinese with English Abstract).
17. The influence of internal oxidation during decarburization of a grain oriented silicon steel on the morphology of the glass film formed at high temperature annealing10.1016/j.jmmm.2014.01.019 ↗
18. Formation mechanism and microstructure of a forsterite film in grain-oriented electrical steel10.1016/j.tsf.2022.139258 ↗
19. Morphologies and influential factors of forsterite film in grain-oriented silicon steel10.1016/S1006-706X(13)60204-6 ↗
20. Nitrogen behavior during nitriding treatment of electrical steel (in Chinese with English abstract)
21. Experimental studies and numerical simulation on the nitriding process of grain-oriented silicon steel
22. G.C. Yan, C.X. He, L. Meng, et al. Structure of surface oxide layer and effect on nitriding of grain-oriented silicon steel. 43, 2015: 89–94. (in Chinese with English Abstract) https://doi.org/10.11868/j.issn.1001–4381.2015.12.015.
23. Effect of annealing time on oxides phases and morphology along oxidized depth of Fe-3% Si steel during decarburization
24. Characterization of chemical information and morphology for in-depth oxide layers in decarburized electrical steel with glow discharge sputtering10.1002/sia.5237 ↗
25. Reaktionstypen bei der Oxydation von Legierungen
26. Kinetics, microstructures and mechanism of internal oxidation - its effect and prevention in high temperature alloy oxidation10.5006/0010-9312-21.12.382 ↗
27. Oxidation of metals and alloys (american society for
28. Meijering · 1971 · 1
29. Gibbs-Thomson formula for small island sizes: Corrections for high vapor densities10.1103/PhysRevB.54.8899 ↗
30. Decay of isolated surface features driven by the Gibbs-Thomson effect in an analytic model and a simulation10.1103/PhysRevB.55.1811 ↗
31. Adsorbate‐promoted mass flow on the gold (111) surface observed by scanning tunneling microscopy10.1116/1.578006 ↗
32. In Evolution of Surface and Thin Film Microstructures
33. Decay of two-dimensional Ag islands on Ag (111)10.1103/PhysRevLett.76.2113 ↗
34. Characterization of Surface Oxidation and Numerical Simulation of Oxidation Kinetics for Fe-3%Si Steel during Decarburization10.2355/isijinternational.ISIJINT-2017-492 ↗
35. Diffusion of oxygen in the scales of Fe–Cr alloy interconnects and oxide coating layer for solid oxide fuel cells10.1016/j.ssi.2008.07.024 ↗
36. Justification of the local space charge neutrality hypothesis in metal oxidation10.1016/0375-9601(76)90516-8 ↗
37. Über die innere Oxydation von Eisenlegierungen10.1002/srin.196401702 ↗
38. Extended Wagner-type models and their application to the prediction of the transition from internal to external oxidation10.1016/j.commatsci.2022.111334 ↗
39. A TEM study of oxide layers formed during decarburization annealing of electrical steel10.2355/isijinternational.51.1163 ↗
40. Numerical simulation of internal oxidation of steels during annealing treatments10.1007/s11085-005-5718-x ↗
41. Transition from Internal to External Oxidation of Mn Steel Alloys10.1007/s11085-013-9456-1 ↗
42. N. Kiyoshi, K. Akihiko, I. Koin, S. Kokichi. The Solubility of Oxygen in δ-Iron. 54, 1968: 553–560.(in Chinese with English Abstract). https://doi.org/10.2355/tetsutohagane1955.54.5_553.10.2355/tetsutohagane1955.54.5_553 ↗
43. Solid solubility of oxygen in columbium10.1007/BF03377426 ↗
44. Solubility of oxygen in alpha iron10.1007/BF03398887 ↗
45. Effect of the alloy elements on the solubility of oxygen in δ-Iron
46. Continuous monitoring of oxygen chemical potential at the surface of growing oxide scales during high temperature oxidation of metals10.2320/matertrans.MER2007263 ↗
47. Longer Term Oxidation Kinetics of Low Carbon Low Silicon Steel in 17H2O–N2 at 900°C
48. Effect of surface oxidation on decarburization of a Fe-3%Si steel during annealing10.2355/isijinternational.ISIJINT-2018-233 ↗
49. The transition from internal to external oxidation and the formation of interruption bands in silver-indium alloys10.1016/0001-6160(61)90103-1 ↗
50. Störungslinien und Störungsbänder in innerlich oxydierten Kupfer‐und Silberlegierungen
51. A mathematical model for internal oxidation10.1007/BF00611351 ↗
52. Internal oxidation of Fe-Si alloys in γ-phase region10.1007/BF00549838 ↗
53. High temperature oxidation and corrosion of metals