The influence of oxygen partial pressure on the base oxide of chromia forming steels: The story prior to breakaway oxidation

M. Sattari, H. Hooshyar, J. Liske, T. Jonsson

Corrosion Science· Volume 213

Abstract

The influence of pO2 on the base oxide formed on 304 L stainless steel has been investigated at 600 °C. The alloy was exposed in 5%O2-95%N2 and 10%H2-20%H2O-Ar atmospheres and the initial stages of oxidation were analysed by TEM and EDX. In both environments, the thin scale consists of a Cr-rich oxide overlaid by a FeCrMn oxide. However, the subscale formed in H2-H2O is richer in Cr compared to the 5%O2-95%N2 case (∼90 cation% and ∼70 cation% respectively). The findings are in good agreement with thermodynamic calculations and can explain breakaway oxidation of marginal chromia forming steels in H2-H2O.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Kofstad · 1998
2. D.J. Young, High Temperature Oxidation and Corrosion of Metals, First, 2008.
3. Mechanisms of breakaway oxidation and application to a chromia-forming steel10.1023/A:1018855914737 ↗
4. Effect of water vapor on high-temperature oxidation of FeCr alloys10.1007/s11837-009-0102-y ↗
5. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
6. International workshop on high-temperature corrosion10.1007/BF01046850 ↗
7. Role of water vapor in chromia-scale growth at low oxygen partial pressure10.1023/A:1023040010859 ↗
8. The effect of water vapor on selective oxidation of Fe–Cr alloys10.1007/s11085-007-9090-x ↗
9. Water vapour effects on Fe-Cr alloy oxidation10.1007/s11085-009-9183-9 ↗
10. Chen · 2022
11. Oxidation of Fe-10Cr in O2 and in O2+H2O environment at 600°C: a microstructural investigation10.1016/j.corsci.2013.06.016 ↗
12. Evidence for chromium evaporation influencing the oxidation of 304L: the effect of temperature and flow rate10.1023/A:1014877600235 ↗
13. The effects of water vapor and hydrogen on the high-temperature oxidation of alloys10.1007/s11085-012-9349-8 ↗
14. The role of alloy composition, environment and stresses for the oxidation resistance of modern 9% Cr steels for fossil power stations10.1590/S1516-14392004000100016 ↗
15. The kinetic behaviour of metals in water vapour at high temperatures: can general rules be proposed?10.4028/www.scientific.net/MSF.369-372.231 ↗
16. Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments10.1016/j.corsci.2006.02.002 ↗
17. Modeling the effect of water vapor on the interfacial behavior of high-temperature air in contact with Fe20Cr surfaces10.1016/j.scriptamat.2011.02.013 ↗
18. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
19. Thermo-Calc & Dictra, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
20. An assessment of the Fe-O system10.1007/BF02645709 ↗
21. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600°C10.1016/j.corsci.2005.08.012 ↗
22. J.E. Tang, M. Halvarsson, H. Asteman, J. Svensson, The microstructure of the base oxide on 304L steel, 32 (2001) 799–805.10.1016/S0968-4328(00)00087-1 ↗
23. Oxidation of binary FeCr alloys (Fe-2.25Cr, Fe-10Cr, Fe-18Cr and Fe-25Cr) in O 2 and in O 2 + H 2O environment at 600 °C10.1007/s11085-010-9229-z ↗
24. H. Hooshyar, M. Sattari, T. Jonsson, J. Liske, J.-E. Svensson, L.-G. Johansson, A mechanistic study of high temperature oxidation of marginal chromia formers in presence of water vapor at low pO2 environment, Unpubl. Manuscr. (2016).
25. Oxidation after breakdown of the chromium-rich scale on stainless steels at high temperature: internal oxidation10.1007/s11085-016-9610-7 ↗
26. Paralinear oxidation of chromium in O 2 + H 2O environment at 600-700 °c10.1007/s11085-008-9114-1 ↗
27. The effect of water vapor on high temperature oxidation of Fe-Cr alloys at 1073 K10.2320/matertrans.M2009212 ↗