Hydrogen absorption and embrittlement of Zn-Al coated medium-Mn steel
Source abstract
Abstract
In this study, we investigated the influence of the austenitizing condition on H absorption and hydrogen embrittlement (HE) in a Zn-Al coated medium-Mn steel. The specimen, which underwent austenitization at 750 °C for 5 min, demonstrated high resistance to HE due to its low diffusible H content. The presence of a uniform Al 2O 3 oxide layer and a low H diffusion rate contributed to this low H content. However, an increase in austenitizing temperature accelerated H absorption due to the enhanced diffusion rate of H atoms, resulting in decreased resistance to HE.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Introduction to a Third-Generation automobile steel and its optimal warm-stamping process
2. An introduction to medium-Mn steel: Metallurgy, mechanical properties and warm stamping process10.1016/j.matdes.2016.01.048 ↗
3. Comparison of the hot-stamped boron-alloyed steel and the warm-stamped medium-Mn steel on microstructure and mechanical properties10.1016/j.msea.2016.10.045 ↗
4. Investigation on microstructure and martensitic transformation mechanism for the warm-stamped Third-Generation automotive medium-Mn Steel
5. Microstructure evolution and enhanced performance of a novel Nb-Mo microalloyed medium Mn alloy fabricated by low-temperature rolling and warm stamping10.1016/j.matdes.2017.08.047 ↗
6. The effects of process temperatures on the microstructure and tensile properties of warm-stamped Nb-bearing medium-Mn Steel10.1007/s11661-019-05570-w ↗
7. Evaluations of tensile properties as a function of austenitizing temperature and springback by V-bending testing in medium-Mn steels10.1016/j.msea.2020.139534 ↗
8. Design of high strength medium-Mn steel using machine learning10.1016/j.msea.2022.143148 ↗
9. Enhancing Hydrogen Embrittlement Resistance of Lath Martensite by Introducing Nano-Films of Interlath Austenite10.1007/s11661-015-3009-y ↗
10. The mechanism of hydrogen embrittlement in intecritically annealed medium Mn TRIP steel10.1016/j.actamat.2016.04.038 ↗
11. Effect of gaseous hydrogen charging on the tensile properties of standard and medium Mn X70 pipeline steels
12. Hydrogen embrittlement of intercritically annealed medium-Mn steel (0.1C–5Mn) under different rolling conditions
13. Effect of intercritical annealing time on hydrogen embrittlement of warm-rolled medium Mn steel10.1016/j.msea.2018.04.100 ↗
14. Austenite morphology and resistance to hydrogen embrittlement in medium Mn transformation-induced plasticity steel10.1016/j.scriptamat.2019.05.011 ↗
15. Effect of reverted austenite fraction on hydrogen embrittlement of TRIP-aided medium Mn steel (0.1C–5Mn)10.1016/j.engfailanal.2019.01.018 ↗
16. Enhancing the resistance to hydrogen embrittlement of Al-containing medium-Mn steel through heavy warm rolling10.1016/j.scriptamat.2019.02.009 ↗
17. Research progress and prospect of medium manganese steel
18. Hydrogen embrittlement behavior of high strength low carbon medium manganese steel under different heat treatments10.1016/j.ijhydene.2019.10.103 ↗
19. Hydrogen embrittlement susceptibility of 0.1C–5Mn medium-Mn steel under different treatment conditions
20. Influence of Microstructural Morphology on Hydrogen Embrittlement in a Medium-Mn Steel Fe-12Mn-3Al-0.05C
21. Insight into hydrogen effect on a duplex medium-Mn steel revealed by in-situ nanoindentation test10.1016/j.ijhydene.2019.04.290 ↗
22. Intercritical annealing temperature dependence of hydrogen embrittlement behavior of cold-rolled Al-containing medium-Mn steel10.1016/j.ijhydene.2019.06.204 ↗
23. Impact of precipitates on the hydrogen embrittlement behavior of a V-alloyed medium-manganese austenitic stainless steel10.1016/j.jmrt.2020.09.085 ↗
24. A review of research status of hydrogen embrittlement for automotive advanced high-strength steels
25. Homogeneous elasto-plastic deformation and improved strain compatibility between austenite and ferrite in a co-precipitation hardened medium Mn steel with enhanced hydrogen embrittlement resistance10.1016/j.ijplas.2020.102805 ↗
26. J. Wang, W. Hui, Z. Xie, Z. Wang, Y. Zhang, X. Zhao, Hydrogen embrittlement of a cold-rolled Al-containing medium-Mn steel: Effect of pre-strain, 45, 2020: 22080–22093. http://doi.org/10.1016/j.jihydene.2020.05.239.10.1016/j.ijhydene.2020.05.239 ↗
27. Influence of hydrogen and annealing process on the microstructural evolution and fracture micromechanisms of medium Mn steel: An in-situ TEM investigation10.1016/j.ijhydene.2020.05.142 ↗
28. Effect of relative humidity on mechanical degradation of medium mn steels
29. Effect of prestrain on hydrogen-induced delayed cracking for medium mn steels10.1007/s11665-020-04706-z ↗
30. Dependence of hydrogen embrittlement mechanisms on microstructure-driven hydrogen distribution in medium Mn steels10.1016/j.actamat.2019.11.029 ↗
31. Effect of heat treatment processes on hydrogen embrittlement in hot-rolled medium Mn steels10.1016/j.ijhydene.2020.04.241 ↗
32. Influence of microstructure on hydrogen embrittlement in hot-rolled medium Mn steels10.1016/j.msea.2020.139147 ↗
33. The possibility of enhanced hydrogen embrittlement resistance of medium-Mn steels by addition of micro-alloying elements10.1016/j.matchar.2020.110386 ↗
34. Critical role of Lüders banding in hydrogen embrittlement susceptibility of medium Mn steels10.1016/j.scriptamat.2020.08.025 ↗
35. Evaluation of hydrogen effect on the fatigue crack growth behavior of medium-Mn steels via in-situ hydrogen plasma charging in an environmental scanning electron microscope10.1016/j.jmst.2020.12.069 ↗
36. Hydrogen embrittlement of medium Mn steels
37. Vanadium or copper alloyed duplex lightweight steel with enhanced hydrogen embrittlement resistance at room temperature10.1016/j.msea.2021.141347 ↗
38. Current Challenges and Opportunities Toward Understanding Hydrogen Embrittlement Mechanisms in Advanced High-Strength Steels: A Review
39. The potential significance of tempering treatment in alleviating the hydrogen embrittlement susceptibility of a hot-rolled and intercritically annealed medium-Mn steel10.1016/j.engfailanal.2020.104969 ↗
40. Dependence of hydrogen embrittlement on annealing time in medium-Mn steels10.1108/ACMM-07-2021-2521 ↗
41. Effects of rolling and heat treatment on hydrogen embrittlement in medium-Mn steel10.1016/j.matlet.2021.130784 ↗
42. New Insights to Understand the Influence of Nb/Mo on Hydrogen Embrittlement Resistance of Warm-Rolled Medium-Mn Steels10.1007/s11665-021-06405-9 ↗
43. Interactions of nanoprecipitates, metastable austenite, and Lüders banding in an ultra-low carbon medium Mn steel with abnormal strength dependence of hydrogen embrittlement10.1016/j.mtla.2022.101380 ↗
44. Effect of Mo and Nb on mechanical properties and hydrogen embrittlement of hot-rolled medium-Mn steels10.1016/j.msea.2022.143108 ↗
45. Corrosion resistance of different metallic coatings on press-hardened steels for automotive10.1002/srin.201000291 ↗
46. Hot stamping of ultra-high strength steel parts10.1016/j.cirp.2017.05.007 ↗
47. Faderl · 2009 · 283
48. State-of-the-knowledge on coating systems for hot stamped parts10.1002/srin.201100292 ↗
49. Effects of Al-Si coating and Zn coating on the hydrogen uptake and embrittlement of ultra-high strength press-hardened steel10.1016/j.surfcoat.2019.06.047 ↗
50. Surface oxide formation during rapid heating of Zn-coated press hardening Steel10.2355/isijinternational.54.2364 ↗
51. Effects of alloying elements on surface oxides of hot–dip galvanized press hardened steel10.1016/j.surfcoat.2020.126466 ↗
52. A review on hot stamping10.1016/j.jmatprotec.2010.07.019 ↗
53. A review of the physical metallurgy related to the hot press forming of advanced high strength steel
54. Microstructure of liquid metal embrittlement cracks on Zn-coated 22MnB5 press-hardened steel10.1016/j.scriptamat.2014.07.008 ↗
55. Diffusion and cracking behavior involved in hot press forming of Zn coated 22MnB510.1016/j.jallcom.2019.07.232 ↗
56. Continuous Hot-Dip Galvanizing of Medium-Manganese Third-Generation Advanced High-Strength Steels10.1002/srin.202200898 ↗
57. The effect of Zn-Al coating on the hydrogen embrittlement of twinning-induced plasticity steels with and without Al10.1016/j.jallcom.2018.10.199 ↗
58. Experimental determination of phase diagram in the Zn-Fe binary system10.1016/j.jallcom.2017.11.320 ↗
59. Consideration of hydrogen transport in press-hardened 22MnB510.3139/120.110808 ↗
60. Hydrogen absorption and embrittlement of ultra-high strength aluminized press hardening steel10.1016/j.msea.2018.08.003 ↗
61. Hydrogen permeation through iron, nickel, and resisting alloys at elevated temperatures10.2355/isijinternational1966.19.547 ↗
62. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interface of nanoprecipitates in martensitic steels
63. Absorption/desorption of diffusible hydrogen in aluminized boron steel10.2355/isijinternational.53.1295 ↗